CC331G-GC and CC331G-SR are two conditions of the same copper alloy grade, CC331G: GC (continuous cast bar/tube) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. CC331G-GC is the stronger of the two: yield strength 240 MPa (34.8 ksi) against 190 MPa (27.6 ksi) for CC331G-SR, about 26% more; tensile strength follows at 600 MPa (87 ksi) vs 530 MPa (76.9 ksi). In exchange, CC331G-SR is the more ductile: elongation 28% versus 20% for CC331G-GC, and CC331G-GC is harder (135 HB vs 115 HB).

CC331G-GCChoose it when strength drives the design.

CC331G-SRChoose it when the part is bent, formed or impact-loaded.

CC331G-GC vs CC331G-SR: properties

CC331G-GCCC331G-SR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

112 GPa16.2 Msi
110 GPa16 Msi

Tensile Strength (Ultimate)

600 MPa87 ksi
530 MPa76.9 ksi

Yield Strength (0.2% offset)

240 MPa34.8 ksi
190 MPa27.6 ksi

Elongation at Break

20%
28%

Compressive Strength

265 MPa38.4 ksi
235 MPa34.1 ksi

Shear Strength

350 MPa50.8 ksi
320 MPa46.4 ksi

Fatigue Strength (Endurance Limit)

180 MPa26.1 ksi
160 MPa23.2 ksi

Charpy V-Notch Impact (RT)

19 J14 ft·lbf
26 J19.2 ft·lbf

Hardness, Brinell

135 HB
115 HB

Hardness, Rockwell B

75 HRB
66 HRB

Hardness, Vickers

142 HV
120 HV

Same in both: Shear Modulus 41 GPa5.9 Msi · Bulk Modulus 115 GPa16.7 Msi · Poisson's Ratio 0.33

Physical

Density and transition temperatures.

Same in both: Density 7.64 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,040°C1,904 °F · Liquidus Temperature 1,045°C1,913 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

59 W/m·K34.1 BTU/hr·ft·°F
60 W/m·K34.7 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 375 J/kg·K0.09 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 16.2 µm/m·K9 µin/in·°F · Latent Heat of Fusion 220 J/g94.6 BTU/lb · Max Service Temperature (continuous) 300°C572 °F · Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

15 % IACS
16 % IACS

Electrical Resistivity

1.15×10⁻⁷ Ω·m4.53 µΩ·in
1.08×10⁻⁷ Ω·m4.25 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

73 / 100
74 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.28 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

45 / 100
48 / 100

Machinability Rating (AISI 1212 = 100 %)

50%
52%

Weldability

63 / 100
68 / 100

Formability (cold)

18 / 100
24 / 100

Same in both: Castability 78 / 100 · Brazeability / Solderability 30 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 55 MJ/kg23,646 BTU/lb · Embodied Carbon (primary production) 3.8 kg CO₂/kg · Embodied Water 400 L/kg47.9 gal/lb · Typical Recycled Content 50%

Strength versus weight

Yield strength against density for every copper alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005001,0007.588.599.5Density (g/cm³)Yield strength (MPa) — log scaleCC331G

CC331G-GC vs CC331G-SR — frequently asked

Is CC331G-GC stronger than CC331G-SR?

Yes. CC331G-GC has a typical yield strength of 240 MPa (34.8 ksi) against 190 MPa (27.6 ksi) for CC331G-SR — about 26% more. Tensile strength is 600 MPa (87 ksi) vs 530 MPa (76.9 ksi).

Which condition does FabDigit quote by default, GC or SR?

GS is the default CC331G condition in the FabDigit quote flow (neither GC nor SR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, CC331G-GC or CC331G-SR?

CC331G-SR. Its weldability rates good (68/100) against good (63/100) for CC331G-GC.