C93400-M02 and C93400-M07 are two conditions of the same copper alloy grade, C93400: M02 (as centrifugally cast) versus M07 (as continuous cast). The chemistry is identical, so every difference below comes from the condition. C93400-M07 is the stronger of the two: yield strength 138 MPa (20 ksi) against 128 MPa (18.6 ksi) for C93400-M02, about 8% more.

C93400-M07Choose it when strength drives the design.

C93400-M02 vs C93400-M07: properties

C93400-M02C93400-M07

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

234 MPa33.9 ksi
241 MPa35 ksi

Yield Strength (0.2% offset)

128 MPa18.6 ksi
138 MPa20 ksi

Elongation at Break

16%
15%

Reduction in Area

15%
14%

Compressive Strength

285 MPa41.3 ksi
295 MPa42.8 ksi

Shear Strength

152 MPa22 ksi
155 MPa22.5 ksi

Fatigue Strength (Endurance Limit)

72 MPa10.4 ksi
75 MPa10.9 ksi

Charpy V-Notch Impact (RT)

12 J8.9 ft·lbf
13 J9.6 ft·lbf

Hardness, Brinell

62 HB
65 HB

Hardness, Vickers

65 HV
68 HV

Same in both: Elastic (Young's) Modulus 97 GPa14.1 Msi · Shear Modulus 37 GPa5.4 Msi · Bulk Modulus 105 GPa15.2 Msi · Poisson's Ratio 0.34

Physical

Density and transition temperatures.

Same in both: Density 8.95 g/cm³0.32 lb/in³ · Melting Point (Solidus) 854°C1,569 °F · Liquidus Temperature 977°C1,791 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 47 W/m·K27.2 BTU/hr·ft·°F · Specific Heat Capacity 377 J/kg·K0.09 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 18 µm/m·K10 µin/in·°F · Latent Heat of Fusion 170 J/g73.1 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -200°C-328 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 12 % IACS · Electrical Resistivity 1.44×10⁻⁷ Ω·m5.67 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.28 V · Corrosion Resistance 66 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Same in both: Machinability 88 / 100 · Machinability Rating (AISI 1212 = 100 %) 80% · Weldability 20 / 100 · Formability (cold) 10 / 100 · Castability 85 / 100 · Brazeability / Solderability 55 / 100 · Polishability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 50 MJ/kg21,496 BTU/lb · Embodied Carbon (primary production) 3.6 kg CO₂/kg · Embodied Water 300 L/kg35.9 gal/lb · Typical Recycled Content 75%

Strength versus weight

Yield strength against density for every copper alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005001,0007.588.599.5Density (g/cm³)Yield strength (MPa) — log scaleC93400

C93400-M02 vs C93400-M07 — frequently asked

Is C93400-M07 stronger than C93400-M02?

Yes. C93400-M07 has a typical yield strength of 138 MPa (20 ksi) against 128 MPa (18.6 ksi) for C93400-M02 — about 8% more. Tensile strength is 241 MPa (35 ksi) vs 234 MPa (33.9 ksi).

Which condition does FabDigit quote by default, M02 or M07?

M07 is the default C93400 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose C93400-M02 over C93400-M07?

Pick C93400-M07 when strength drives the design.

Ready to make it?

Upload a CAD file and FabDigit prices the part in C93400-M02 and C93400-M07 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.