FabDigitFabDigit

Copper Alloy C87700-M05 vs C87700-M06

Copper Alloy · C87700 temper comparison

C87700-M05 and C87700-M06 are two conditions of the same copper alloy grade, C87700: M05 (as plaster cast) versus M06 (as investment cast). The chemistry is identical, so every difference below comes from the condition. C87700-M05 is the stronger of the two: tensile strength 450 MPa (65.3 ksi) against 425 MPa (61.6 ksi) for C87700-M06, about 6% more. C87700-M05 is harder — 110 HB against 102 HB for C87700-M06 — which matters for wear surfaces and threads.

C87700-M05Choose it when strength drives the design, or when surface hardness matters.

C87700-M05 vs C87700-M06: properties

C87700-M05C87700-M06

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

105 GPa15.2 Msi
103 GPa14.9 Msi

Tensile Strength (Ultimate)

450 MPa65.3 ksi
425 MPa61.6 ksi

Yield Strength (0.2% offset)

205 MPa29.7 ksi
195 MPa28.3 ksi

Elongation at Break

22%
24%

Reduction in Area

26%
27%

Compressive Strength

320 MPa46.4 ksi
305 MPa44.2 ksi

Shear Strength

295 MPa42.8 ksi
280 MPa40.6 ksi

Fatigue Strength (Endurance Limit)

150 MPa21.8 ksi
138 MPa20 ksi

Charpy V-Notch Impact (RT)

24 J17.7 ft·lbf
25 J18.4 ft·lbf

Hardness, Brinell

110 HB
102 HB

Hardness, Rockwell B

68 HRB
63 HRB

Hardness, Vickers

115 HV
107 HV

Same in both: Shear Modulus 39 GPa5.7 Msi · Bulk Modulus 108 GPa15.7 Msi · Poisson's Ratio 0.34

Physical

Density and transition temperatures.

Same in both: Density 8.3 g/cm³0.3 lb/in³ · Melting Point (Solidus) 820°C1,508 °F · Liquidus Temperature 915°C1,679 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 28 W/m·K16.2 BTU/hr·ft·°F · Specific Heat Capacity 380 J/kg·K0.09 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 18 µm/m·K10 µin/in·°F · Latent Heat of Fusion 210 J/g90.3 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

6.8 % IACS
6.7 % IACS

Electrical Resistivity

2.55×10⁻⁷ Ω·m10 µΩ·in
2.6×10⁻⁷ Ω·m10.2 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

73 / 100
72 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.27 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability Rating (AISI 1212 = 100 %)

42%
40%

Formability (cold)

26 / 100
28 / 100

Same in both: Machinability 45 / 100 · Weldability 80 / 100 · Castability 85 / 100 · Brazeability / Solderability 70 / 100 · Polishability 80 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 50 MJ/kg21,496 BTU/lb · Embodied Carbon (primary production) 3.4 kg CO₂/kg · Embodied Water 250 L/kg30 gal/lb · Typical Recycled Content 75%

Strength versus weight

Yield strength against density for every copper alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005001,0007.588.599.5Density (g/cm³)Yield strength (MPa) — log scaleC87700

C87700-M05 vs C87700-M06 — frequently asked

Is C87700-M05 stronger than C87700-M06?

Yes. C87700-M05 has a typical tensile strength of 450 MPa (65.3 ksi) against 425 MPa (61.6 ksi) for C87700-M06 — about 6% more.

Which condition does FabDigit quote by default, M05 or M06?

M01 is the default C87700 condition in the FabDigit quote flow (neither M05 nor M06). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose C87700-M05 over C87700-M06?

Pick C87700-M05 when strength drives the design, or when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in C87700-M05 and C87700-M06 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.