Copper Alloy C74500 vs C76200

Copper Alloy · grade comparison

Copper Alloy C74500 and C76200 are both copper alloy grades. C76200 is the stronger of the two: yield strength 448 MPa (65 ksi) against 400 MPa (58 ksi) for C74500, about 12% more. In exchange, C74500 is the more ductile: elongation 12% versus 10% for C76200. C74500 conducts heat better (45 W/m·K vs 29 W/m·K). On the shop floor, C76200 welds better (50 vs 40 out of 100).

C74500Choose it when the part is bent, formed or impact-loaded.

C76200Choose it when strength drives the design, or when it will be welded.

C74500 vs C76200: properties

C74500C76200

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

127 GPa18.4 Msi
124 GPa18 Msi

Shear Modulus

48 GPa7 Msi
46 GPa6.7 Msi

Bulk Modulus

128 GPa18.6 Msi
129 GPa18.7 Msi

Poisson's Ratio

0.33
0.34

Tensile Strength (Ultimate)

510 MPa74 ksi
517 MPa75 ksi

Yield Strength (0.2% offset)

400 MPa58 ksi
448 MPa65 ksi

Elongation at Break

12%
10%

Fatigue Strength (Endurance Limit)

180 MPa26.1 ksi
215 MPa31.2 ksi

Hardness, Brinell

150 HB
155 HB

Hardness, Rockwell B

80 HRB
82 HRB

Hardness, Vickers

158 HV
165 HV

Same in both: Shear Strength 330 MPa47.9 ksi

Physical

Density and transition temperatures.

Density

8.73 g/cm³0.32 lb/in³
8.7 g/cm³0.31 lb/in³

Melting Point (Solidus)

954°C1,749 °F
1,010°C1,850 °F

Liquidus Temperature

1,021°C1,870 °F
1,050°C1,922 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

45 W/m·K26 BTU/hr·ft·°F
29 W/m·K16.8 BTU/hr·ft·°F

Latent Heat of Fusion

195 J/g83.8 BTU/lb
175 J/g75.2 BTU/lb

Max Service Temperature (continuous)

180°C356 °F
175°C347 °F

Same in both: Specific Heat Capacity 377 J/kg·K0.09 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 16.2 µm/m·K9 µin/in·°F · Min Service Temperature -200°C-328 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

9 % IACS
5.5 % IACS

Electrical Resistivity

1.92×10⁻⁷ Ω·m7.56 µΩ·in
3.13×10⁻⁷ Ω·m12.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.26 V
-0.19 V

Same in both: Corrosion Resistance 62 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Weldability

40 / 100
50 / 100

Brazeability / Solderability

88 / 100
85 / 100

Same in both: Machinability 30 / 100 · Machinability Rating (AISI 1212 = 100 %) 20% · Formability (cold) 60 / 100 · Polishability 90 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

78 MJ/kg33,534 BTU/lb
72 MJ/kg30,954 BTU/lb

Embodied Carbon (primary production)

5.2 kg CO₂/kg
5 kg CO₂/kg

Embodied Water

260 L/kg31.2 gal/lb
320 L/kg38.3 gal/lb

Same in both: Typical Recycled Content 40%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

58 kN·m/kg
59 kN·m/kg

Specific Stiffness (E / density)

14.5 MN·m/kg
14.3 MN·m/kg

Modulus of Resilience

630 kJ/m³
809 kJ/m³

Thermal Diffusivity

13.7 mm²/s
8.8 mm²/s

Thermal Shock Resistance Index

11
7

Strength versus weight

Yield strength against density for every copper alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005001,0007.588.599.5Density (g/cm³)Yield strength (MPa) — log scaleC74500C76200

Manufacturing and finishing

CapabilityC74500C76200
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

Both take the same 4 finishes: Copper Plating, Electroless Nickel (EN), Gold Plating, Silver Plating.

C74500 vs C76200 — frequently asked

Is C76200 stronger than C74500?

Yes. C76200 has a typical yield strength of 448 MPa (65 ksi) against 400 MPa (58 ksi) for C74500 — about 12% more. Tensile strength is 517 MPa (75 ksi) vs 510 MPa (74 ksi).

Which is cheaper, C74500 or C76200?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

Which welds better, C74500 or C76200?

C76200. Its weldability rates fair (50/100) against fair (40/100) for C74500.

Ready to make it?

Upload a CAD file and FabDigit prices the part in C74500 and C76200 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.