Elastic (Young's) Modulus

217 GPa31.5 Msi
222 GPa32.2 Msi
220 GPa31.9 Msi
220 GPa31.9 Msi

Shear Modulus

84 GPa12.2 Msi
86 GPa12.5 Msi
85 GPa12.3 Msi
84 GPa12.2 Msi

Bulk Modulus

165 GPa23.9 Msi
165 GPa23.9 Msi
170 GPa24.7 Msi
165 GPa23.9 Msi

Poisson's Ratio

0.28
0.28
0.29
0.28

Tensile Strength (Ultimate)

850 MPa123 ksi
900 MPa131 ksi
900 MPa131 ksi
860 MPa125 ksi

Yield Strength (0.2% offset)

570 MPa82.7 ksi
620 MPa89.9 ksi
570 MPa82.7 ksi
560 MPa81.2 ksi

Elongation at Break

12%
12%
15%
20%

Reduction in Area

20%
20%
25%
32%

Compressive Strength

1,100 MPa160 ksi
680 MPa98.6 ksi
1,200 MPa174 ksi
1,400 MPa203 ksi

Shear Strength

550 MPa79.8 ksi
545 MPa79 ksi
550 MPa79.8 ksi

Fatigue Strength (Endurance Limit)

380 MPa55.1 ksi
400 MPa58 ksi

Fracture Toughness (K_IC)

45 MPa·√m41 ksi·√in
33 MPa·√m30 ksi·√in

Charpy V-Notch Impact (RT)

20 J14.8 ft·lbf
9 J6.6 ft·lbf
25 J18.4 ft·lbf
25 J18.4 ft·lbf

Hardness, Brinell

240 HB
255 HB
240 HB
235 HB

Hardness, Rockwell B

99 HRB
101 HRB
99 HRB
99 HRB

Hardness, Rockwell C

23 HRC
25 HRC

Hardness, Vickers

250 HV
270 HV
250 HV
245 HV

Physical

Density and transition temperatures.

Density

8.16 g/cm³0.29 lb/in³
7.98 g/cm³0.29 lb/in³
8.6 g/cm³0.31 lb/in³
8.7 g/cm³0.31 lb/in³

Melting Point (Solidus)

1,250°C2,282 °F
1,290°C2,354 °F
1,400°C2,552 °F
1,340°C2,444 °F

Liquidus Temperature

1,430°C2,606 °F
1,420°C2,588 °F
1,460°C2,660 °F
1,440°C2,624 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

24 W/m·K13.9 BTU/hr·ft·°F
22 W/m·K12.7 BTU/hr·ft·°F
22 W/m·K12.7 BTU/hr·ft·°F
21 W/m·K12.1 BTU/hr·ft·°F

Thermal Expansion (CTE, 20–100 °C)

10.1 µm/m·K5.6 µin/in·°F
10.8 µm/m·K6 µin/in·°F
11.2 µm/m·K6.2 µin/in·°F
11 µm/m·K6.1 µin/in·°F

Latent Heat of Fusion

260 J/g112 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

500°C932 °F
400°C752 °F
400°C752 °F
400°C752 °F

Min Service Temperature

-60°C-76 °F
-60°C-76 °F
-40°C-40 °F
-60°C-76 °F

Same in both: Specific Heat Capacity 420 J/kg·K0.1 BTU/lb·°F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 3.1 % IACS · Electrical Resistivity 5.5×10⁻⁷ Ω·m21.7 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

18 / 100
18 / 100
18 / 100
22 / 100

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.55 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

40 / 100
38 / 100
35 / 100
35 / 100

Machinability Rating (AISI 1212 = 100 %)

45%
42%
40%
30%

Weldability

18 / 100
20 / 100
15 / 100
15 / 100

Formability (cold)

15 / 100
10 / 100
12 / 100
15 / 100

Castability

30 / 100
20 / 100
25 / 100

Polishability

70 / 100
80 / 100
70 / 100
60 / 100

Same in both: Brazeability / Solderability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

55 MJ/kg23,646 BTU/lb
62 MJ/kg26,655 BTU/lb
60 MJ/kg25,795 BTU/lb
52 MJ/kg22,356 BTU/lb

Embodied Carbon (primary production)

3.6 kg CO₂/kg
4.4 kg CO₂/kg
4.2 kg CO₂/kg
3.6 kg CO₂/kg

Typical Recycled Content

40%
30%
35%
45%

Same in both: Embodied Water 90 L/kg10.8 gal/lb

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

104 kN·m/kg
113 kN·m/kg
105 kN·m/kg
99 kN·m/kg

Specific Stiffness (E / density)

26.6 MN·m/kg
27.8 MN·m/kg
25.6 MN·m/kg
25.3 MN·m/kg

Modulus of Resilience

749 kJ/m³
866 kJ/m³
738 kJ/m³
713 kJ/m³

Thermal Diffusivity

7 mm²/s
6.6 mm²/s
6.1 mm²/s
5.7 mm²/s

Thermal Shock Resistance Index

9
8
8
7

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleM42T8T1W6Mo5Cr4V2

Manufacturing and finishing

CapabilityW6Mo5Cr4V2M42T8T1
Default conditionAnnealedAnnealedAnnealedAnnealed
Relative cost$$$ Premium$$$$$ Specialty$$$ Premium$$$ Premium
Min. machined wall0.8 mm0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µmRa 1.6 µm

Both are offered for CNC machining. Both take the same 38 finishes: AlCrN, AlTiN, Black Oxide, CVD Al2O3, CVD TiCN, CVD TiN, Cerakote, Chrome Plating, Copper Plating, CrN, DLC, E-Coating and 26 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in W6Mo5Cr4V2 and M42 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.