T13ASK5T10AT12A

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

210 GPa30.5 Msi
205 GPa29.7 Msi
207 GPa30 Msi
210 GPa30.5 Msi

Shear Modulus

81 GPa11.7 Msi
80 GPa11.6 Msi
80 GPa11.6 Msi
81 GPa11.7 Msi

Bulk Modulus

160 GPa23.2 Msi
160 GPa23.2 Msi
160 GPa23.2 Msi
165 GPa23.9 Msi

Tensile Strength (Ultimate)

700 MPa102 ksi
710 MPa103 ksi
700 MPa102 ksi
720 MPa104 ksi

Yield Strength (0.2% offset)

420 MPa60.9 ksi
400 MPa58 ksi
400 MPa58 ksi
420 MPa60.9 ksi

Elongation at Break

18%
12%
22%
20%

Reduction in Area

35%
20%
45%
40%

Compressive Strength

480 MPa69.6 ksi
720 MPa104 ksi
800 MPa116 ksi
430 MPa62.4 ksi

Shear Strength

450 MPa65.3 ksi
460 MPa66.7 ksi
480 MPa69.6 ksi
450 MPa65.3 ksi

Charpy V-Notch Impact (RT)

20 J14.8 ft·lbf
10 J7.4 ft·lbf
25 J18.4 ft·lbf
12 J8.9 ft·lbf

Hardness, Brinell

197 HB
200 HB
187 HB
200 HB

Hardness, Rockwell B

92 HRB
93 HRB
90 HRB
93 HRB

Hardness, Vickers

207 HV
210 HV
195 HV
210 HV

Fracture Toughness (K_IC)

45 MPa·√m41 ksi·√in
50 MPa·√m45.5 ksi·√in

Same in both: Poisson's Ratio 0.29 · Fatigue Strength (Endurance Limit) 320 MPa46.4 ksi

Physical

Density and transition temperatures.

Density

7.81 g/cm³0.28 lb/in³
7.82 g/cm³0.28 lb/in³
7.81 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,260°C2,300 °F
1,425°C2,597 °F
1,400°C2,552 °F
1,300°C2,372 °F

Liquidus Temperature

1,440°C2,624 °F
1,470°C2,678 °F
1,470°C2,678 °F
1,440°C2,624 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

48 W/m·K27.7 BTU/hr·ft·°F
48 W/m·K27.7 BTU/hr·ft·°F
47 W/m·K27.2 BTU/hr·ft·°F
47 W/m·K27.2 BTU/hr·ft·°F

Specific Heat Capacity

470 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.3 µm/m·K6.3 µin/in·°F
11.5 µm/m·K6.4 µin/in·°F
11.5 µm/m·K6.4 µin/in·°F
11.8 µm/m·K6.6 µin/in·°F

Max Service Temperature (continuous)

300°C572 °F
350°C662 °F
300°C572 °F
400°C752 °F

Same in both: Latent Heat of Fusion 250 J/g107 BTU/lb · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 9.5 % IACS · Electrical Resistivity 1.8×10⁻⁷ Ω·m7.09 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.61 V
-0.6 V
-0.62 V

Corrosion Resistance

10 / 100
10 / 100
10 / 100
9 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

40 / 100
36 / 100
55 / 100
45 / 100

Machinability Rating (AISI 1212 = 100 %)

30%
40%
65%
45%

Weldability

12 / 100
18 / 100
15 / 100
12 / 100

Formability (cold)

35 / 100
30 / 100
40 / 100
40 / 100

Brazeability / Solderability

50 / 100
45 / 100
50 / 100
50 / 100

Polishability

80 / 100
70 / 100
70 / 100
70 / 100

Castability

30 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

30 MJ/kg12,898 BTU/lb
27 MJ/kg11,608 BTU/lb
30 MJ/kg12,898 BTU/lb
28 MJ/kg12,038 BTU/lb

Embodied Carbon (primary production)

2.3 kg CO₂/kg
2.1 kg CO₂/kg
2.3 kg CO₂/kg
2.1 kg CO₂/kg

Embodied Water

60 L/kg7.2 gal/lb
45 L/kg5.4 gal/lb
60 L/kg7.2 gal/lb
60 L/kg7.2 gal/lb

Same in both: Typical Recycled Content 30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

90 kN·m/kg
91 kN·m/kg
90 kN·m/kg
92 kN·m/kg

Specific Stiffness (E / density)

26.9 MN·m/kg
26.2 MN·m/kg
26.5 MN·m/kg
26.8 MN·m/kg

Modulus of Resilience

420 kJ/m³
390 kJ/m³
386 kJ/m³
420 kJ/m³

Thermal Diffusivity

13.1 mm²/s
12.9 mm²/s
12.8 mm²/s
12.7 mm²/s

Same in both: Thermal Shock Resistance Index 14

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSK5T10AT12AT13A

Manufacturing and finishing

CapabilityT13ASK5T10AT12A
CNC machiningYes
Sheet metalYes
Default conditionHR
Relative cost$ Budget$$ Standard$ Budget$ Budget
Min. machined wall0.8 mm
Best machined surfaceRa 1.6 µm
AlCrNYes
AlTiNYes
Black OxideYes
CVD Al2O3Yes
CVD TiCNYes
CVD TiNYes
CerakoteYes
Chrome PlatingYes
CrNYes
DLCYes
E-CoatingYes
HVOF CoatingYes
Hot-Dip GalvanizingYes
MoS2Yes
Multilayer CVDYes
Nickel PlatingYes
PTFE CoatingYes
PaintingYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in T13A and SK5 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.