FabDigit

SKD11 vs A11 and 2 more: properties

SKD11A11A2A3

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

210 GPa30.5 Msi
221 GPa32.1 Msi
203 GPa29.4 Msi
203 GPa29.4 Msi

Shear Modulus

80 GPa11.6 Msi
85 GPa12.3 Msi
78 GPa11.3 Msi
79 GPa11.5 Msi

Bulk Modulus

160 GPa23.2 Msi
160 GPa23.2 Msi
160 GPa23.2 Msi

Poisson's Ratio

0.29
0.29
0.28
0.29

Tensile Strength (Ultimate)

820 MPa119 ksi
900 MPa131 ksi
740 MPa107 ksi
760 MPa110 ksi

Yield Strength (0.2% offset)

500 MPa72.5 ksi
600 MPa87 ksi
470 MPa68.2 ksi
430 MPa62.4 ksi

Elongation at Break

12%
8%
22%
20%

Reduction in Area

20%
20%
45%
35%

Compressive Strength

900 MPa131 ksi
950 MPa138 ksi
500 MPa72.5 ksi
900 MPa131 ksi

Shear Strength

550 MPa79.8 ksi
550 MPa79.8 ksi
450 MPa65.3 ksi
460 MPa66.7 ksi

Fatigue Strength (Endurance Limit)

380 MPa55.1 ksi
390 MPa56.6 ksi
330 MPa47.9 ksi

Fracture Toughness (K_IC)

30 MPa·√m27.3 ksi·√in
32 MPa·√m29.1 ksi·√in

Charpy V-Notch Impact (RT)

20 J14.8 ft·lbf
12 J8.9 ft·lbf
30 J22.1 ft·lbf
25 J18.4 ft·lbf

Hardness, Brinell

225 HB
269 HB
217 HB
217 HB

Hardness, Rockwell B

98 HRB
103 HRB
96 HRB
96 HRB

Hardness, Rockwell C

20 HRC
26 HRC
19 HRC

Hardness, Vickers

235 HV
283 HV
230 HV
228 HV

Physical

Density and transition temperatures.

Density

7.7 g/cm³0.28 lb/in³
7.41 g/cm³0.27 lb/in³
7.86 g/cm³0.28 lb/in³
7.86 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,250°C2,282 °F
1,420°C2,588 °F
1,420°C2,588 °F

Liquidus Temperature

1,420°C2,588 °F
1,465°C2,669 °F
1,470°C2,678 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

20 W/m·K11.6 BTU/hr·ft·°F
21 W/m·K12.1 BTU/hr·ft·°F
26 W/m·K15 BTU/hr·ft·°F
24 W/m·K13.9 BTU/hr·ft·°F

Thermal Expansion (CTE, 20–100 °C)

10.9 µm/m·K6.1 µin/in·°F
10.6 µm/m·K5.9 µin/in·°F
10.7 µm/m·K5.9 µin/in·°F
10.7 µm/m·K5.9 µin/in·°F

Latent Heat of Fusion

250 J/g107 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

250°C482 °F
425°C797 °F
425°C797 °F
200°C392 °F

Min Service Temperature

-30°C-22 °F
-50°C-58 °F
-30°C-22 °F
-30°C-22 °F

Same in both: Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 2.7 % IACS · Electrical Resistivity 6.5×10⁻⁷ Ω·m25.6 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.35 V
-0.6 V

Corrosion Resistance

25 / 100
20 / 100
20 / 100
16 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

32 / 100
20 / 100
45 / 100
38 / 100

Machinability Rating (AISI 1212 = 100 %)

30%
25%
60%
42%

Weldability

20 / 100
15 / 100
20 / 100
15 / 100

Formability (cold)

25 / 100
12 / 100
35 / 100
20 / 100

Castability

25 / 100
20 / 100
25 / 100

Brazeability / Solderability

40 / 100
40 / 100
35 / 100

Polishability

80 / 100
65 / 100
70 / 100
70 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

36 MJ/kg15,477 BTU/lb
55 MJ/kg23,646 BTU/lb
36 MJ/kg15,477 BTU/lb
36 MJ/kg15,477 BTU/lb

Embodied Carbon (primary production)

2.6 kg CO₂/kg
4.5 kg CO₂/kg
2.6 kg CO₂/kg
2.6 kg CO₂/kg

Embodied Water

70 L/kg8.4 gal/lb
65 L/kg7.8 gal/lb
60 L/kg7.2 gal/lb

Typical Recycled Content

40%
25%
35%
30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

106 kN·m/kg
121 kN·m/kg
94 kN·m/kg
97 kN·m/kg

Specific Stiffness (E / density)

27.3 MN·m/kg
29.8 MN·m/kg
25.8 MN·m/kg
25.8 MN·m/kg

Modulus of Resilience

595 kJ/m³
814 kJ/m³
544 kJ/m³
455 kJ/m³

Thermal Diffusivity

5.6 mm²/s
6.2 mm²/s
7.2 mm²/s
6.6 mm²/s

Thermal Shock Resistance Index

7
8
9
8

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleA11A2A3SKD11

Manufacturing and finishing

CapabilitySKD11A11A2A3
Default conditionAnnealedAnnealedAnnealed
Relative cost$$$ Premium$$$$$ Specialty$$$ Premium$$$ Premium
Min. machined wall0.8 mm0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µmRa 1.6 µm

Both are offered for CNC machining. Both take the same 38 finishes: AlCrN, AlTiN, Black Oxide, CVD Al2O3, CVD TiCN, CVD TiN, Cerakote, Chrome Plating, Copper Plating, CrN, DLC, E-Coating and 26 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in SKD11 and A11 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.