FabDigit

S960QL vs 4140 and 2 more: properties

S960QL414041504340

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

210 GPa30.5 Msi
205 GPa29.7 Msi
205 GPa29.7 Msi
205 GPa29.7 Msi

Shear Modulus

81 GPa11.7 Msi
80 GPa11.6 Msi
80 GPa11.6 Msi
80 GPa11.6 Msi

Bulk Modulus

165 GPa23.9 Msi
160 GPa23.2 Msi
160 GPa23.2 Msi
160 GPa23.2 Msi

Poisson's Ratio

0.3
0.29
0.29
0.29

Tensile Strength (Ultimate)

1,050 MPa152 ksi
690 MPa100 ksi
860 MPa125 ksi
950 MPa138 ksi

Yield Strength (0.2% offset)

1,010 MPa146 ksi
480 MPa69.6 ksi
520 MPa75.4 ksi
620 MPa89.9 ksi

Elongation at Break

12%
22%
16%
18%

Reduction in Area

55%
50%
40%
45%

Compressive Strength

1,000 MPa145 ksi
480 MPa69.6 ksi
640 MPa92.8 ksi

Shear Strength

640 MPa92.8 ksi
420 MPa60.9 ksi
560 MPa81.2 ksi
580 MPa84.1 ksi

Fatigue Strength (Endurance Limit)

470 MPa68.2 ksi
345 MPa50 ksi
390 MPa56.6 ksi
430 MPa62.4 ksi

Fracture Toughness (K_IC)

100 MPa·√m91 ksi·√in
110 MPa·√m100 ksi·√in
95 MPa·√m86.5 ksi·√in

Charpy V-Notch Impact (RT)

70 J51.6 ft·lbf
40 J29.5 ft·lbf
25 J18.4 ft·lbf
30 J22.1 ft·lbf

Hardness, Brinell

320 HB
210 HB
235 HB
285 HB

Hardness, Rockwell C

34 HRC
21 HRC
29 HRC

Hardness, Vickers

340 HV
220 HV
245 HV
300 HV

Hardness, Rockwell B

94 HRB
100 HRB

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,460°C2,660 °F
1,416°C2,581 °F
1,416°C2,581 °F
1,416°C2,581 °F

Liquidus Temperature

1,510°C2,750 °F
1,483°C2,701 °F
1,490°C2,714 °F
1,454°C2,649 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

34 W/m·K19.6 BTU/hr·ft·°F
42.6 W/m·K24.6 BTU/hr·ft·°F
42.6 W/m·K24.6 BTU/hr·ft·°F
44.5 W/m·K25.7 BTU/hr·ft·°F

Specific Heat Capacity

460 J/kg·K0.11 BTU/lb·°F
473 J/kg·K0.11 BTU/lb·°F
473 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

12 µm/m·K6.7 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F

Latent Heat of Fusion

270 J/g116 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

350°C662 °F
425°C797 °F
400°C752 °F
400°C752 °F

Same in both: Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

7 % IACS
7.8 % IACS
7.8 % IACS
7 % IACS

Electrical Resistivity

2.5×10⁻⁷ Ω·m9.84 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.48×10⁻⁷ Ω·m9.76 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.61 V
-0.6 V
-0.62 V

Same in both: Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

35 / 100
60 / 100
45 / 100
48 / 100

Machinability Rating (AISI 1212 = 100 %)

38%
62%
50%
50%

Weldability

55 / 100
40 / 100
25 / 100
33 / 100

Formability (cold)

40 / 100
40 / 100
25 / 100
35 / 100

Castability

0 / 100
35 / 100
45 / 100

Brazeability / Solderability

30 / 100
55 / 100
55 / 100
55 / 100

Polishability

55 / 100
60 / 100
60 / 100
70 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

30 MJ/kg12,898 BTU/lb
32 MJ/kg13,758 BTU/lb
31 MJ/kg13,328 BTU/lb
32 MJ/kg13,758 BTU/lb

Embodied Carbon (primary production)

2.3 kg CO₂/kg
2.2 kg CO₂/kg
2.3 kg CO₂/kg
2.3 kg CO₂/kg

Embodied Water

60 L/kg7.2 gal/lb
55 L/kg6.6 gal/lb
60 L/kg7.2 gal/lb
60 L/kg7.2 gal/lb

Typical Recycled Content

25%
30%
30%
30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

134 kN·m/kg
88 kN·m/kg
110 kN·m/kg
121 kN·m/kg

Specific Stiffness (E / density)

26.8 MN·m/kg
26.1 MN·m/kg
26.1 MN·m/kg
26.1 MN·m/kg

Modulus of Resilience

2,429 kJ/m³
562 kJ/m³
660 kJ/m³
938 kJ/m³

Thermal Diffusivity

9.4 mm²/s
11.5 mm²/s
11.5 mm²/s
11.9 mm²/s

Thermal Shock Resistance Index

14
12
15
17

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale414041504340S960QL

Manufacturing and finishing

CapabilityS960QL414041504340
Casting & forgingYes
Default conditionQ&THRHRHR
Relative cost$$ Standard$$ Standard$$$ Premium$$$ Premium
Min. machined wall0.8 mm0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µmRa 1.6 µm

Both are offered for CNC machining and Sheet metal. Both take the same 38 finishes: AlCrN, AlTiN, Black Oxide, CVD Al2O3, CVD TiCN, CVD TiN, Cerakote, Chrome Plating, Copper Plating, CrN, DLC, E-Coating and 26 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in S960QL and 4140 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.