S1 vs S2 and 2 more: properties

S1S2S5S4

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

690 MPa100 ksi
760 MPa110 ksi
725 MPa105 ksi
720 MPa104 ksi

Yield Strength (0.2% offset)

415 MPa60.2 ksi
460 MPa66.7 ksi
440 MPa63.8 ksi
430 MPa62.4 ksi

Elongation at Break

25%
20%
25%
25%

Reduction in Area

45%
45%
45%
50%

Compressive Strength

450 MPa65.3 ksi
480 MPa69.6 ksi
460 MPa66.7 ksi

Shear Strength

450 MPa65.3 ksi
460 MPa66.7 ksi
440 MPa63.8 ksi
450 MPa65.3 ksi

Fatigue Strength (Endurance Limit)

310 MPa45 ksi
340 MPa49.3 ksi
340 MPa49.3 ksi
330 MPa47.9 ksi

Charpy V-Notch Impact (RT)

60 J44.3 ft·lbf
100 J73.8 ft·lbf
60 J44.3 ft·lbf
60 J44.3 ft·lbf

Hardness, Brinell

200 HB
200 HB
215 HB
210 HB

Hardness, Rockwell B

94 HRB
94 HRB
95 HRB
95 HRB

Hardness, Vickers

210 HV
210 HV
225 HV

Fracture Toughness (K_IC)

70 MPa·√m63.7 ksi·√in

Same in both: Elastic (Young's) Modulus 207 GPa30 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Density

7.85 g/cm³0.28 lb/in³
7.79 g/cm³0.28 lb/in³
7.76 g/cm³0.28 lb/in³
7.79 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,420°C2,588 °F
1,425°C2,597 °F
1,420°C2,588 °F
1,420°C2,588 °F

Liquidus Temperature

1,470°C2,678 °F
1,500°C2,732 °F
1,480°C2,696 °F
1,480°C2,696 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

25 W/m·K14.4 BTU/hr·ft·°F
25.5 W/m·K14.7 BTU/hr·ft·°F
24 W/m·K13.9 BTU/hr·ft·°F
25 W/m·K14.4 BTU/hr·ft·°F

Specific Heat Capacity

460 J/kg·K0.11 BTU/lb·°F
477 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

12.4 µm/m·K6.9 µin/in·°F
12.5 µm/m·K6.9 µin/in·°F
12.4 µm/m·K6.9 µin/in·°F
12.4 µm/m·K6.9 µin/in·°F

Latent Heat of Fusion

260 J/g112 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

200°C392 °F
400°C752 °F
400°C752 °F
400°C752 °F

Min Service Temperature

-30°C-22 °F
-50°C-58 °F
-50°C-58 °F
-40°C-40 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

7.5 % IACS
5.5 % IACS
4 % IACS
3.1 % IACS

Electrical Resistivity

2.3×10⁻⁷ Ω·m9.06 µΩ·in
3.1×10⁻⁷ Ω·m12.2 µΩ·in
4.5×10⁻⁷ Ω·m17.7 µΩ·in
5.5×10⁻⁷ Ω·m21.7 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.6 V
-0.55 V

Same in both: Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

45 / 100
45 / 100
50 / 100
48 / 100

Machinability Rating (AISI 1212 = 100 %)

55%
65%
55%
60%

Weldability

20 / 100
15 / 100
25 / 100
22 / 100

Formability (cold)

25 / 100
35 / 100
30 / 100
35 / 100

Brazeability / Solderability

40 / 100
35 / 100
35 / 100
45 / 100

Polishability

60 / 100
60 / 100
60 / 100
55 / 100

Castability

25 / 100
30 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

34 MJ/kg14,617 BTU/lb
34 MJ/kg14,617 BTU/lb
36 MJ/kg15,477 BTU/lb
33 MJ/kg14,187 BTU/lb

Embodied Carbon (primary production)

2.5 kg CO₂/kg
2.4 kg CO₂/kg
2.6 kg CO₂/kg
2.4 kg CO₂/kg

Embodied Water

60 L/kg7.2 gal/lb
65 L/kg7.8 gal/lb
65 L/kg7.8 gal/lb
65 L/kg7.8 gal/lb

Typical Recycled Content

30%
45%
40%
35%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

88 kN·m/kg
98 kN·m/kg
93 kN·m/kg
92 kN·m/kg

Specific Stiffness (E / density)

26.4 MN·m/kg
26.6 MN·m/kg
26.7 MN·m/kg
26.6 MN·m/kg

Modulus of Resilience

416 kJ/m³
511 kJ/m³
468 kJ/m³
447 kJ/m³

Thermal Diffusivity

6.9 mm²/s
6.9 mm²/s
6.7 mm²/s
6.8 mm²/s

Same in both: Thermal Shock Resistance Index 7

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleS2S1S5S4

Manufacturing and finishing

CapabilityS1S2S5S4
CNC machiningYesYesYes
Default conditionAnnealedAnnealedAnnealed
Relative cost$$$ Premium$$$$ High$$$ Premium$$$ Premium
Min. machined wall0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µm
AlCrNYesYesYes
AlTiNYesYesYes
Black OxideYesYesYes
CVD Al2O3YesYesYes
CVD TiCNYesYesYes
CVD TiNYesYesYes
CerakoteYesYesYes
Chrome PlatingYesYesYes
CrNYesYesYes
DLCYesYesYes
E-CoatingYesYesYes
HVOF CoatingYesYesYes
Hot-Dip GalvanizingYesYesYes
MoS2YesYesYes
Multilayer CVDYesYesYes
Nickel PlatingYesYesYes
PTFE CoatingYesYesYes
PaintingYesYesYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in S1 and S2 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.