Q345R vs 17Mn4 and 2 more: properties

Q345R17Mn4P265GHA516 Gr 60

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

206 GPa29.9 Msi
210 GPa30.5 Msi
211 GPa30.6 Msi
203 GPa29.4 Msi

Shear Modulus

79 GPa11.5 Msi
81 GPa11.7 Msi
81 GPa11.7 Msi
79 GPa11.5 Msi

Poisson's Ratio

0.29
0.29
0.3
0.29

Tensile Strength (Ultimate)

550 MPa79.8 ksi
520 MPa75.4 ksi
465 MPa67.4 ksi
460 MPa66.7 ksi

Yield Strength (0.2% offset)

370 MPa53.7 ksi
330 MPa47.9 ksi
295 MPa42.8 ksi
265 MPa38.4 ksi

Elongation at Break

24%
22%
26%
27%

Reduction in Area

50%
48%
52%
55%

Compressive Strength

370 MPa53.7 ksi
330 MPa47.9 ksi
295 MPa42.8 ksi
265 MPa38.4 ksi

Shear Strength

330 MPa47.9 ksi
335 MPa48.6 ksi
280 MPa40.6 ksi
290 MPa42.1 ksi

Fatigue Strength (Endurance Limit)

240 MPa34.8 ksi
235 MPa34.1 ksi
205 MPa29.7 ksi
200 MPa29 ksi

Fracture Toughness (K_IC)

100 MPa·√m91 ksi·√in
110 MPa·√m100 ksi·√in
100 MPa·√m91 ksi·√in
130 MPa·√m118 ksi·√in

Charpy V-Notch Impact (RT)

90 J66.4 ft·lbf
45 J33.2 ft·lbf
70 J51.6 ft·lbf
45 J33.2 ft·lbf

Hardness, Brinell

160 HB
155 HB
140 HB
130 HB

Hardness, Rockwell B

84 HRB
82 HRB
76 HRB
72 HRB

Hardness, Vickers

168 HV
163 HV
147 HV
137 HV

Same in both: Bulk Modulus 160 GPa23.2 Msi

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,440°C2,624 °F
1,450°C2,642 °F
1,495°C2,723 °F
1,490°C2,714 °F

Liquidus Temperature

1,510°C2,750 °F
1,510°C2,750 °F
1,520°C2,768 °F
1,520°C2,768 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

48 W/m·K27.7 BTU/hr·ft·°F
48 W/m·K27.7 BTU/hr·ft·°F
50 W/m·K28.9 BTU/hr·ft·°F
52 W/m·K30 BTU/hr·ft·°F

Specific Heat Capacity

480 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F
461 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.8 µm/m·K6.6 µin/in·°F
12 µm/m·K6.7 µin/in·°F
12 µm/m·K6.7 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F

Max Service Temperature (continuous)

400°C752 °F
400°C752 °F
400°C752 °F
425°C797 °F

Min Service Temperature

-20°C-4 °F
-20°C-4 °F
-10°C14 °F
-29°C-20 °F

Same in both: Latent Heat of Fusion 270 J/g116 BTU/lb

Electrical

Conductivity and insulation.

Electrical Conductivity

8.6 % IACS
9 % IACS
10 % IACS
10 % IACS

Electrical Resistivity

2×10⁻⁷ Ω·m7.87 µΩ·in
1.9×10⁻⁷ Ω·m7.48 µΩ·in
1.7×10⁻⁷ Ω·m6.69 µΩ·in
1.7×10⁻⁷ Ω·m6.69 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.62 V
-0.62 V
-0.62 V
-0.65 V

Corrosion Resistance

12 / 100
12 / 100
12 / 100
10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

62 / 100
58 / 100
66 / 100
65 / 100

Machinability Rating (AISI 1212 = 100 %)

65%
62%
63%
70%

Weldability

85 / 100
85 / 100
90 / 100
92 / 100

Formability (cold)

70 / 100
65 / 100
76 / 100
78 / 100

Castability

45 / 100

Brazeability / Solderability

60 / 100
60 / 100
70 / 100
60 / 100

Polishability

45 / 100
45 / 100
50 / 100
40 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Carbon (primary production)

2.1 kg CO₂/kg
2 kg CO₂/kg
2 kg CO₂/kg
1.9 kg CO₂/kg

Embodied Water

35 L/kg4.2 gal/lb
45 L/kg5.4 gal/lb
40 L/kg4.8 gal/lb
40 L/kg4.8 gal/lb

Typical Recycled Content

22%
30%
25%
25%

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

70 kN·m/kg
66 kN·m/kg
59 kN·m/kg
59 kN·m/kg

Specific Stiffness (E / density)

26.2 MN·m/kg
26.8 MN·m/kg
26.9 MN·m/kg
25.9 MN·m/kg

Modulus of Resilience

332 kJ/m³
259 kJ/m³
206 kJ/m³
173 kJ/m³

Thermal Diffusivity

12.7 mm²/s
13.3 mm²/s
13.8 mm²/s
14.1 mm²/s

Thermal Shock Resistance Index

11
10
9
10

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale17Mn4Q345RP265GHA516 Gr 60

Manufacturing and finishing

CapabilityQ345R17Mn4P265GHA516 Gr 60
Default conditionHRHRHRHR
Relative cost$$ Standard$$ Standard$$ Standard$$ Standard
Min. machined wall0.8 mm0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µmRa 1.6 µm

Both are offered for CNC machining and Sheet metal. Both take the same 38 finishes: AlCrN, AlTiN, Black Oxide, CVD Al2O3, CVD TiCN, CVD TiN, Cerakote, Chrome Plating, Copper Plating, CrN, DLC, E-Coating and 26 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Q345R and 17Mn4 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.