MS1500 vs 4140 and 2 more: properties

MS1500414041504340

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

210 GPa30.5 Msi
205 GPa29.7 Msi
205 GPa29.7 Msi
205 GPa29.7 Msi

Poisson's Ratio

0.3
0.29
0.29
0.29

Tensile Strength (Ultimate)

1,550 MPa225 ksi
690 MPa100 ksi
860 MPa125 ksi
950 MPa138 ksi

Yield Strength (0.2% offset)

1,250 MPa181 ksi
480 MPa69.6 ksi
520 MPa75.4 ksi
620 MPa89.9 ksi

Elongation at Break

5%
22%
16%
18%

Shear Strength

930 MPa135 ksi
420 MPa60.9 ksi
560 MPa81.2 ksi
580 MPa84.1 ksi

Fatigue Strength (Endurance Limit)

650 MPa94.3 ksi
345 MPa50 ksi
390 MPa56.6 ksi
430 MPa62.4 ksi

Fracture Toughness (K_IC)

50 MPa·√m45.5 ksi·√in
110 MPa·√m100 ksi·√in
95 MPa·√m86.5 ksi·√in

Hardness, Rockwell C

46 HRC
21 HRC
29 HRC

Hardness, Vickers

470 HV
220 HV
245 HV
300 HV

Reduction in Area

50%
40%
45%

Compressive Strength

480 MPa69.6 ksi
640 MPa92.8 ksi

Charpy V-Notch Impact (RT)

40 J29.5 ft·lbf
25 J18.4 ft·lbf
30 J22.1 ft·lbf

Hardness, Brinell

210 HB
235 HB
285 HB

Hardness, Rockwell B

94 HRB
100 HRB

Same in both: Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,425°C2,597 °F
1,416°C2,581 °F
1,416°C2,581 °F
1,416°C2,581 °F

Liquidus Temperature

1,500°C2,732 °F
1,483°C2,701 °F
1,490°C2,714 °F
1,454°C2,649 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

30 W/m·K17.3 BTU/hr·ft·°F
42.6 W/m·K24.6 BTU/hr·ft·°F
42.6 W/m·K24.6 BTU/hr·ft·°F
44.5 W/m·K25.7 BTU/hr·ft·°F

Specific Heat Capacity

470 J/kg·K0.11 BTU/lb·°F
473 J/kg·K0.11 BTU/lb·°F
473 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

12 µm/m·K6.7 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F

Max Service Temperature (continuous)

200°C392 °F
425°C797 °F
400°C752 °F
400°C752 °F

Same in both: Latent Heat of Fusion 250 J/g107 BTU/lb · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

8 % IACS
7.8 % IACS
7.8 % IACS
7 % IACS

Electrical Resistivity

2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.48×10⁻⁷ Ω·m9.76 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.61 V
-0.6 V
-0.62 V

Same in both: Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

22 / 100
60 / 100
45 / 100
48 / 100

Machinability Rating (AISI 1212 = 100 %)

15%
62%
50%
50%

Weldability

50 / 100
40 / 100
25 / 100
33 / 100

Formability (cold)

18 / 100
40 / 100
25 / 100
35 / 100

Polishability

60 / 100
60 / 100
60 / 100
70 / 100

Brazeability / Solderability

55 / 100
55 / 100
55 / 100

Castability

35 / 100
45 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

30 MJ/kg12,898 BTU/lb
32 MJ/kg13,758 BTU/lb
31 MJ/kg13,328 BTU/lb
32 MJ/kg13,758 BTU/lb

Embodied Carbon (primary production)

2.3 kg CO₂/kg
2.2 kg CO₂/kg
2.3 kg CO₂/kg
2.3 kg CO₂/kg

Embodied Water

40 L/kg4.8 gal/lb
55 L/kg6.6 gal/lb
60 L/kg7.2 gal/lb
60 L/kg7.2 gal/lb

Typical Recycled Content

25%
30%
30%
30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

197 kN·m/kg
88 kN·m/kg
110 kN·m/kg
121 kN·m/kg

Specific Stiffness (E / density)

26.8 MN·m/kg
26.1 MN·m/kg
26.1 MN·m/kg
26.1 MN·m/kg

Modulus of Resilience

3,720 kJ/m³
562 kJ/m³
660 kJ/m³
938 kJ/m³

Thermal Diffusivity

8.1 mm²/s
11.5 mm²/s
11.5 mm²/s
11.9 mm²/s

Thermal Shock Resistance Index

18
12
15
17

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale414041504340MS1500

Manufacturing and finishing

CapabilityMS1500414041504340
CNC machiningYesYesYes
Casting & forgingYes
Default conditionCRHRHRHR
Relative cost$$ Standard$$ Standard$$$ Premium$$$ Premium
Min. machined wall0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µm
AlCrNYesYesYes
AlTiNYesYesYes
CVD Al2O3YesYesYes
CVD TiCNYesYesYes
CVD TiNYesYesYes
CrNYesYesYes
DLCYesYesYes
HVOF CoatingYesYesYes
MoS2YesYesYes
Multilayer CVDYesYesYes
TiAlNYesYesYes
TiB2YesYesYes
TiCNYesYesYes
TiNYesYesYes
WC/CYesYesYes
ZrNYesYesYes

Both are offered for Sheet metal. They share 22 finishes: Black Oxide, Cerakote, Chrome Plating, Copper Plating, E-Coating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Hot-Dip Galvanizing, Manganese Phosphate, Nickel Plating and 10 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in MS1500 and 4140 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.