FabDigit

M50 vs 52100 and 2 more: properties

M5052100SUJ2100Cr6

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

207 GPa30 Msi
205 GPa29.7 Msi
210 GPa30.5 Msi
210 GPa30.5 Msi

Bulk Modulus

165 GPa23.9 Msi
166 GPa24.1 Msi
160 GPa23.2 Msi
160 GPa23.2 Msi

Poisson's Ratio

0.29
0.3
0.29
0.29

Tensile Strength (Ultimate)

860 MPa125 ksi
690 MPa100 ksi
660 MPa95.7 ksi
660 MPa95.7 ksi

Yield Strength (0.2% offset)

570 MPa82.7 ksi
415 MPa60.2 ksi
420 MPa60.9 ksi
420 MPa60.9 ksi

Elongation at Break

12%
25%
25%
22%

Reduction in Area

25%
45%
45%
48%

Compressive Strength

620 MPa89.9 ksi
430 MPa62.4 ksi
450 MPa65.3 ksi

Shear Strength

560 MPa81.2 ksi
420 MPa60.9 ksi
400 MPa58 ksi
400 MPa58 ksi

Fatigue Strength (Endurance Limit)

390 MPa56.6 ksi
320 MPa46.4 ksi
320 MPa46.4 ksi
300 MPa43.5 ksi

Fracture Toughness (K_IC)

60 MPa·√m54.6 ksi·√in

Charpy V-Notch Impact (RT)

20 J14.8 ft·lbf
15 J11.1 ft·lbf
30 J22.1 ft·lbf
25 J18.4 ft·lbf

Hardness, Brinell

240 HB
195 HB
192 HB
200 HB

Hardness, Rockwell B

99 HRB
93 HRB
92 HRB
94 HRB

Hardness, Rockwell C

22 HRC

Hardness, Vickers

250 HV
205 HV
200 HV
210 HV

Same in both: Shear Modulus 80 GPa11.6 Msi

Physical

Density and transition temperatures.

Density

8 g/cm³0.29 lb/in³
7.81 g/cm³0.28 lb/in³
7.81 g/cm³0.28 lb/in³
7.81 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,400°C2,552 °F
1,424°C2,595 °F
1,425°C2,597 °F
1,424°C2,595 °F

Liquidus Temperature

1,450°C2,642 °F
1,455°C2,651 °F
1,460°C2,660 °F
1,455°C2,651 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

26 W/m·K15 BTU/hr·ft·°F
46 W/m·K26.6 BTU/hr·ft·°F
46 W/m·K26.6 BTU/hr·ft·°F
45 W/m·K26 BTU/hr·ft·°F

Specific Heat Capacity

460 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.3 µm/m·K6.3 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F

Latent Heat of Fusion

250 J/g107 BTU/lb
247 J/g106 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

200°C392 °F
400°C752 °F
200°C392 °F
200°C392 °F

Min Service Temperature

-73°C-99 °F
-40°C-40 °F
-40°C-40 °F
-40°C-40 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

2.9 % IACS
7 % IACS
7 % IACS
8 % IACS

Electrical Resistivity

6×10⁻⁷ Ω·m23.6 µΩ·in
2.5×10⁻⁷ Ω·m9.84 µΩ·in
2.5×10⁻⁷ Ω·m9.84 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.62 V
-0.61 V
-0.6 V

Corrosion Resistance

15 / 100
12 / 100
12 / 100
12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

35 / 100
40 / 100
45 / 100
45 / 100

Machinability Rating (AISI 1212 = 100 %)

45%
40%
40%
40%

Weldability

10 / 100
12 / 100
12 / 100
12 / 100

Formability (cold)

12 / 100
35 / 100
35 / 100
35 / 100

Castability

20 / 100
25 / 100
30 / 100
30 / 100

Brazeability / Solderability

30 / 100
35 / 100
35 / 100
45 / 100

Polishability

85 / 100
85 / 100
85 / 100
88 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

50 MJ/kg21,496 BTU/lb
30 MJ/kg12,898 BTU/lb
30 MJ/kg12,898 BTU/lb
32 MJ/kg13,758 BTU/lb

Embodied Carbon (primary production)

3.6 kg CO₂/kg
2.2 kg CO₂/kg
2.3 kg CO₂/kg
2.3 kg CO₂/kg

Embodied Water

70 L/kg8.4 gal/lb
55 L/kg6.6 gal/lb
55 L/kg6.6 gal/lb
65 L/kg7.8 gal/lb

Typical Recycled Content

15%
30%
30%
30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

108 kN·m/kg
88 kN·m/kg
85 kN·m/kg
85 kN·m/kg

Specific Stiffness (E / density)

25.9 MN·m/kg
26.2 MN·m/kg
26.9 MN·m/kg
26.9 MN·m/kg

Modulus of Resilience

785 kJ/m³
420 kJ/m³
420 kJ/m³
420 kJ/m³

Thermal Diffusivity

7.1 mm²/s
12.4 mm²/s
12.8 mm²/s
12.3 mm²/s

Thermal Shock Resistance Index

10
13
12
12

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale52100SUJ2100Cr6M50

Manufacturing and finishing

CapabilityM5052100SUJ2100Cr6
Sheet metalYesYesYes
Default conditionAnnealedAnnealedAnnealedAnnealed
Relative cost$$$ Premium$$$ Premium$$ Standard$$ Standard
Min. machined wall0.8 mm0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µmRa 1.6 µm

Both are offered for CNC machining. Both take the same 38 finishes: AlCrN, AlTiN, Black Oxide, CVD Al2O3, CVD TiCN, CVD TiN, Cerakote, Chrome Plating, Copper Plating, CrN, DLC, E-Coating and 26 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in M50 and 52100 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.