M19M435W250M36

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

200 GPa29 Msi
217 GPa31.5 Msi
195 GPa28.3 Msi
217 GPa31.5 Msi

Shear Modulus

78 GPa11.3 Msi
84 GPa12.2 Msi
76 GPa11 Msi
84 GPa12.2 Msi

Bulk Modulus

160 GPa23.2 Msi
165 GPa23.9 Msi
160 GPa23.2 Msi
160 GPa23.2 Msi

Poisson's Ratio

0.29
0.28
0.3
0.28

Tensile Strength (Ultimate)

460 MPa66.7 ksi
880 MPa128 ksi
480 MPa69.6 ksi
880 MPa128 ksi

Yield Strength (0.2% offset)

340 MPa49.3 ksi
550 MPa79.8 ksi
360 MPa52.2 ksi
550 MPa79.8 ksi

Elongation at Break

25%
12%
12%
14%

Reduction in Area

45%
25%
22%

Shear Strength

320 MPa46.4 ksi
600 MPa87 ksi
330 MPa47.9 ksi
570 MPa82.7 ksi

Fatigue Strength (Endurance Limit)

230 MPa33.4 ksi
210 MPa30.5 ksi

Hardness, Rockwell B

72 HRB
82 HRB
100 HRB

Hardness, Vickers

150 HV
265 HV
190 HV
260 HV

Compressive Strength

1,600 MPa232 ksi
360 MPa52.2 ksi
1,900 MPa276 ksi

Fracture Toughness (K_IC)

22 MPa·√m20 ksi·√in

Hardness, Brinell

250 HB
180 HB
248 HB

Hardness, Rockwell C

24 HRC

Charpy V-Notch Impact (RT)

5 J3.7 ft·lbf
20 J14.8 ft·lbf

Physical

Density and transition temperatures.

Density

7.65 g/cm³0.28 lb/in³
7.97 g/cm³0.29 lb/in³
7.65 g/cm³0.28 lb/in³
8.19 g/cm³0.3 lb/in³

Melting Point (Solidus)

1,480°C2,696 °F
1,250°C2,282 °F
1,490°C2,714 °F
1,400°C2,552 °F

Liquidus Temperature

1,520°C2,768 °F
1,420°C2,588 °F
1,510°C2,750 °F
1,455°C2,651 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

25 W/m·K14.4 BTU/hr·ft·°F
22 W/m·K12.7 BTU/hr·ft·°F
24 W/m·K13.9 BTU/hr·ft·°F
22 W/m·K12.7 BTU/hr·ft·°F

Specific Heat Capacity

480 J/kg·K0.11 BTU/lb·°F
420 J/kg·K0.1 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F
420 J/kg·K0.1 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.5 µm/m·K6.4 µin/in·°F
11 µm/m·K6.1 µin/in·°F
11.5 µm/m·K6.4 µin/in·°F
11 µm/m·K6.1 µin/in·°F

Latent Heat of Fusion

260 J/g112 BTU/lb
250 J/g107 BTU/lb
260 J/g112 BTU/lb
260 J/g112 BTU/lb

Max Service Temperature (continuous)

200°C392 °F
400°C752 °F
180°C356 °F
500°C932 °F

Min Service Temperature

-60°C-76 °F
-60°C-76 °F
-60°C-76 °F
-50°C-58 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

3.3 % IACS
2.9 % IACS
3.1 % IACS

Electrical Resistivity

5.2×10⁻⁷ Ω·m20.5 µΩ·in
6×10⁻⁷ Ω·m23.6 µΩ·in
5.5×10⁻⁷ Ω·m21.7 µΩ·in
6×10⁻⁷ Ω·m23.6 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.58 V

Corrosion Resistance

15 / 100
18 / 100
18 / 100
18 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

45 / 100
25 / 100
45 / 100
26 / 100

Machinability Rating (AISI 1212 = 100 %)

45%
25%
45%
30%

Weldability

50 / 100
15 / 100
35 / 100
15 / 100

Formability (cold)

65 / 100
12 / 100
45 / 100
12 / 100

Brazeability / Solderability

50 / 100
45 / 100
30 / 100
55 / 100

Polishability

50 / 100
50 / 100
40 / 100
65 / 100

Castability

20 / 100
25 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

32 MJ/kg13,758 BTU/lb
58 MJ/kg24,936 BTU/lb
32 MJ/kg13,758 BTU/lb
70 MJ/kg30,095 BTU/lb

Embodied Carbon (primary production)

2.4 kg CO₂/kg
4.2 kg CO₂/kg
2.4 kg CO₂/kg
4.6 kg CO₂/kg

Embodied Water

55 L/kg6.6 gal/lb
110 L/kg13.2 gal/lb
45 L/kg5.4 gal/lb
90 L/kg10.8 gal/lb

Typical Recycled Content

25%
35%
15%
30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

60 kN·m/kg
110 kN·m/kg
63 kN·m/kg
107 kN·m/kg

Specific Stiffness (E / density)

26.1 MN·m/kg
27.2 MN·m/kg
25.5 MN·m/kg
26.5 MN·m/kg

Modulus of Resilience

289 kJ/m³
697 kJ/m³
332 kJ/m³
697 kJ/m³

Thermal Diffusivity

6.8 mm²/s
6.6 mm²/s
6.7 mm²/s
6.4 mm²/s

Thermal Shock Resistance Index

5
8
5
8

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleM435W250M19M36

Manufacturing and finishing

CapabilityM19M435W250M36
Sheet metalYesYesYes
CNC machiningYes
Default conditionAnnealedAnnealedFinal AnnealedAnnealed
Relative cost$$ Standard$$$$$ Specialty$$ Standard$$ Standard
Min. machined wall0.8 mm
Best machined surfaceRa 1.6 µm
AlCrNYes
AlTiNYes
CVD Al2O3Yes
CVD TiCNYes
CVD TiNYes
CrNYes
DLCYes
HVOF CoatingYes
MoS2Yes
Multilayer CVDYes
TiAlNYes
TiB2Yes
TiCNYes
TiNYes
WC/CYes
ZrNYes

They share 22 finishes: Black Oxide, Cerakote, Chrome Plating, Copper Plating, E-Coating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Hot-Dip Galvanizing, Manganese Phosphate, Nickel Plating and 10 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in M19 and M4 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.