FabDigit

Steel F1 vs A2

Benchmark · 2 materials

Steel F1 and A2 are both steel grades. A2 is the stronger of the two: yield strength 470 MPa (68.2 ksi) against 420 MPa (60.9 ksi) for F1, about 12% more; tensile strength follows at 740 MPa (107 ksi) vs 700 MPa (102 ksi). A2 is harder — 217 HB against 197 HB for F1 — which matters for wear surfaces and threads. A2 runs hotter in service (425°C vs 300°C continuous) and F1 conducts heat better (44 W/m·K vs 26 W/m·K). On the shop floor, F1 machines more easily (good vs fair), A2 forms better (fair vs poor), and F1 sits in a lower cost tier (standard, $$) than A2 (premium, $$$).

F1Choose it when the part is machined in volume, or when cost is the deciding factor.

A2Choose it when strength drives the design, or when surface hardness matters.

F1 vs A2: properties

F1A2

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

205 GPa29.7 Msi
203 GPa29.4 Msi

Shear Modulus

80 GPa11.6 Msi
78 GPa11.3 Msi

Poisson's Ratio

0.29
0.28

Tensile Strength (Ultimate)

700 MPa102 ksi
740 MPa107 ksi

Yield Strength (0.2% offset)

420 MPa60.9 ksi
470 MPa68.2 ksi

Elongation at Break

20%
22%

Reduction in Area

40%
45%

Compressive Strength

430 MPa62.4 ksi
500 MPa72.5 ksi

Charpy V-Notch Impact (RT)

20 J14.8 ft·lbf
30 J22.1 ft·lbf

Hardness, Brinell

197 HB
217 HB

Hardness, Rockwell B

93 HRB
96 HRB

Hardness, Vickers

207 HV
230 HV

Same in both: Bulk Modulus 160 GPa23.2 Msi · Shear Strength 450 MPa65.3 ksi · Fatigue Strength (Endurance Limit) 330 MPa47.9 ksi

Physical

Density and transition temperatures.

Density

7.8 g/cm³0.28 lb/in³
7.86 g/cm³0.28 lb/in³

Liquidus Temperature

1,470°C2,678 °F
1,465°C2,669 °F

Same in both: Melting Point (Solidus) 1,420°C2,588 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

44 W/m·K25.4 BTU/hr·ft·°F
26 W/m·K15 BTU/hr·ft·°F

Thermal Expansion (CTE, 20–100 °C)

11.5 µm/m·K6.4 µin/in·°F
10.7 µm/m·K5.9 µin/in·°F

Max Service Temperature (continuous)

300°C572 °F
425°C797 °F

Same in both: Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Min Service Temperature -30°C-22 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

9.5 % IACS
2.7 % IACS

Electrical Resistivity

1.8×10⁻⁷ Ω·m7.09 µΩ·in
6.5×10⁻⁷ Ω·m25.6 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V

Corrosion Resistance

10 / 100
20 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
45 / 100

Machinability Rating (AISI 1212 = 100 %)

75%
60%

Weldability

12 / 100
20 / 100

Formability (cold)

25 / 100
35 / 100

Castability

25 / 100
20 / 100

Brazeability / Solderability

45 / 100
40 / 100

Polishability

75 / 100
70 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

33 MJ/kg14,187 BTU/lb
36 MJ/kg15,477 BTU/lb

Embodied Carbon (primary production)

2.3 kg CO₂/kg
2.6 kg CO₂/kg

Embodied Water

60 L/kg7.2 gal/lb
65 L/kg7.8 gal/lb

Typical Recycled Content

30%
35%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

90 kN·m/kg
94 kN·m/kg

Specific Stiffness (E / density)

26.3 MN·m/kg
25.8 MN·m/kg

Modulus of Resilience

430 kJ/m³
544 kJ/m³

Thermal Diffusivity

12.3 mm²/s
7.2 mm²/s

Thermal Shock Resistance Index

13
9

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleA2F1

Manufacturing and finishing

CapabilityF1A2
CNC machiningYes
Default conditionAnnealed
Relative cost$$ Standard$$$ Premium
Min. machined wall0.8 mm
Best machined surfaceRa 1.6 µm
AlCrNYes
AlTiNYes
Black OxideYes
CVD Al2O3Yes
CVD TiCNYes
CVD TiNYes
CerakoteYes
Chrome PlatingYes
CrNYes
DLCYes
E-CoatingYes
HVOF CoatingYes
Hot-Dip GalvanizingYes
MoS2Yes
Multilayer CVDYes
Nickel PlatingYes
PTFE CoatingYes
PaintingYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

F1 vs A2 — frequently asked

Is A2 stronger than F1?

Yes. A2 has a typical yield strength of 470 MPa (68.2 ksi) against 420 MPa (60.9 ksi) for F1 — about 12% more. Tensile strength is 740 MPa (107 ksi) vs 700 MPa (102 ksi).

Which is cheaper, F1 or A2?

F1 is the lower-cost material: it sits in the standard tier ($$) while A2 is premium ($$$). Part price depends far more on geometry, tolerance and quantity than on raw stock — upload a CAD file for a live quote.

Which is easier to machine, F1 or A2?

F1. Its machinability rates good (55/100) against fair (45/100) for A2; for welding the order is A2 first (poor, 20/100) then F1 (not recommended, 12/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in F1 and A2 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.