FabDigit

E355M vs 55Cr3 and 2 more: properties

E355M55Cr342CrMo434MnB5

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

210 GPa30.5 Msi
206 GPa29.9 Msi
210 GPa30.5 Msi
210 GPa30.5 Msi

Shear Modulus

81 GPa11.7 Msi
79.5 GPa11.5 Msi
80 GPa11.6 Msi
80 GPa11.6 Msi

Bulk Modulus

166 GPa24.1 Msi
160 GPa23.2 Msi
160 GPa23.2 Msi
160 GPa23.2 Msi

Poisson's Ratio

0.3
0.29
0.29
0.29

Tensile Strength (Ultimate)

520 MPa75.4 ksi
800 MPa116 ksi
850 MPa123 ksi
620 MPa89.9 ksi

Yield Strength (0.2% offset)

400 MPa58 ksi
480 MPa69.6 ksi
550 MPa79.8 ksi
420 MPa60.9 ksi

Elongation at Break

26%
16%
14%
14%

Reduction in Area

60%
40%
40%
45%

Compressive Strength

400 MPa58 ksi
480 MPa69.6 ksi
560 MPa81.2 ksi

Shear Strength

320 MPa46.4 ksi
500 MPa72.5 ksi
510 MPa74 ksi
400 MPa58 ksi

Fatigue Strength (Endurance Limit)

240 MPa34.8 ksi
360 MPa52.2 ksi
400 MPa58 ksi
280 MPa40.6 ksi

Fracture Toughness (K_IC)

150 MPa·√m137 ksi·√in
85 MPa·√m77.4 ksi·√in
75 MPa·√m68.3 ksi·√in
55 MPa·√m50.1 ksi·√in

Charpy V-Notch Impact (RT)

120 J88.5 ft·lbf
30 J22.1 ft·lbf
30 J22.1 ft·lbf
40 J29.5 ft·lbf

Hardness, Brinell

160 HB
225 HB
245 HB
185 HB

Hardness, Rockwell B

83 HRB
98 HRB
89 HRB

Hardness, Vickers

168 HV
236 HV
258 HV
195 HV

Hardness, Rockwell C

20 HRC
23 HRC

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,460°C2,660 °F
1,420°C2,588 °F
1,420°C2,588 °F
1,420°C2,588 °F

Liquidus Temperature

1,515°C2,759 °F
1,490°C2,714 °F
1,495°C2,723 °F
1,495°C2,723 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

45 W/m·K26 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F
42.6 W/m·K24.6 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F

Specific Heat Capacity

460 J/kg·K0.11 BTU/lb·°F
465 J/kg·K0.11 BTU/lb·°F
473 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

12 µm/m·K6.7 µin/in·°F
12.5 µm/m·K6.9 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F
12.5 µm/m·K6.9 µin/in·°F

Latent Heat of Fusion

247 J/g106 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb

Min Service Temperature

-20°C-4 °F
-40°C-40 °F
-40°C-40 °F
-40°C-40 °F

Same in both: Max Service Temperature (continuous) 400°C752 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

9 % IACS
7.8 % IACS
7.8 % IACS
8 % IACS

Electrical Resistivity

1.9×10⁻⁷ Ω·m7.48 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.65 V
-0.6 V
-0.6 V

Corrosion Resistance

12 / 100
10 / 100
12 / 100
11 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
50 / 100
50 / 100
55 / 100

Machinability Rating (AISI 1212 = 100 %)

60%
55%
55%
60%

Weldability

88 / 100
25 / 100
35 / 100
55 / 100

Formability (cold)

72 / 100
45 / 100
35 / 100
60 / 100

Castability

0 / 100

Brazeability / Solderability

60 / 100
40 / 100
50 / 100
45 / 100

Polishability

45 / 100
60 / 100
70 / 100
55 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

25 MJ/kg10,748 BTU/lb
26 MJ/kg11,178 BTU/lb
30 MJ/kg12,898 BTU/lb
25 MJ/kg10,748 BTU/lb

Embodied Carbon (primary production)

2 kg CO₂/kg
2 kg CO₂/kg
2.2 kg CO₂/kg
2 kg CO₂/kg

Embodied Water

40 L/kg4.8 gal/lb
45 L/kg5.4 gal/lb
60 L/kg7.2 gal/lb
40 L/kg4.8 gal/lb

Typical Recycled Content

30%
30%
30%
25%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

66 kN·m/kg
102 kN·m/kg
108 kN·m/kg
79 kN·m/kg

Specific Stiffness (E / density)

26.8 MN·m/kg
26.2 MN·m/kg
26.8 MN·m/kg
26.8 MN·m/kg

Modulus of Resilience

381 kJ/m³
559 kJ/m³
720 kJ/m³
420 kJ/m³

Thermal Diffusivity

12.5 mm²/s
12.1 mm²/s
11.5 mm²/s
11.9 mm²/s

Thermal Shock Resistance Index

9
14
14
10

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale55Cr342CrMo434MnB5E355M

Manufacturing and finishing

CapabilityE355M55Cr342CrMo434MnB5
CNC machiningYesYes
Sheet metalYesYesYes
Default conditionAnnealedHRCR
Relative cost$ Budget$$ Standard$$ Standard$$ Standard
Min. machined wall0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µm
AlCrNYesYes
AlTiNYesYes
Black OxideYesYesYes
CVD Al2O3YesYes
CVD TiCNYesYes
CVD TiNYesYes
CerakoteYesYesYes
Chrome PlatingYesYesYes
CrNYesYes
DLCYesYes
E-CoatingYesYesYes
HVOF CoatingYesYes
Hot-Dip GalvanizingYesYesYes
MoS2YesYes
Multilayer CVDYesYes
Nickel PlatingYesYesYes
PTFE CoatingYesYesYes
PaintingYesYesYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in E355M and 55Cr3 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.