CRS vs SPCC and 2 more: properties

CRSSPCCHRSMild Steel

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

200 GPa29 Msi
205 GPa29.7 Msi
200 GPa29 Msi
200 GPa29 Msi

Shear Modulus

79 GPa11.5 Msi
80 GPa11.6 Msi
79 GPa11.5 Msi
79 GPa11.5 Msi

Tensile Strength (Ultimate)

365 MPa52.9 ksi
320 MPa46.4 ksi
450 MPa65.3 ksi
400 MPa58 ksi

Yield Strength (0.2% offset)

250 MPa36.3 ksi
220 MPa31.9 ksi
285 MPa41.3 ksi
250 MPa36.3 ksi

Elongation at Break

32%
33%
23%
24%

Reduction in Area

65%
60%
50%
45%

Compressive Strength

220 MPa31.9 ksi
220 MPa31.9 ksi
285 MPa41.3 ksi
250 MPa36.3 ksi

Shear Strength

230 MPa33.4 ksi
235 MPa34.1 ksi
270 MPa39.2 ksi
250 MPa36.3 ksi

Fatigue Strength (Endurance Limit)

180 MPa26.1 ksi
160 MPa23.2 ksi
200 MPa29 ksi
200 MPa29 ksi

Fracture Toughness (K_IC)

120 MPa·√m109 ksi·√in
110 MPa·√m100 ksi·√in
80 MPa·√m72.8 ksi·√in
110 MPa·√m100 ksi·√in

Charpy V-Notch Impact (RT)

90 J66.4 ft·lbf
60 J44.3 ft·lbf
40 J29.5 ft·lbf
50 J36.9 ft·lbf

Hardness, Brinell

110 HB
110 HB
130 HB
120 HB

Hardness, Rockwell B

62 HRB
55 HRB
71 HRB
67 HRB

Hardness, Vickers

100 HV
118 HV
137 HV
126 HV

Same in both: Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Density

7.87 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³

Liquidus Temperature

1,528°C2,782 °F
1,530°C2,786 °F
1,525°C2,777 °F
1,520°C2,768 °F

Same in both: Melting Point (Solidus) 1,495°C2,723 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

52 W/m·K30 BTU/hr·ft·°F
51 W/m·K29.5 BTU/hr·ft·°F
51.9 W/m·K30 BTU/hr·ft·°F
51 W/m·K29.5 BTU/hr·ft·°F

Thermal Expansion (CTE, 20–100 °C)

12.2 µm/m·K6.8 µin/in·°F
12 µm/m·K6.7 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F
12 µm/m·K6.7 µin/in·°F

Latent Heat of Fusion

272 J/g117 BTU/lb
272 J/g117 BTU/lb
247 J/g106 BTU/lb
247 J/g106 BTU/lb

Max Service Temperature (continuous)

400°C752 °F
350°C662 °F
400°C752 °F
400°C752 °F

Same in both: Specific Heat Capacity 480 J/kg·K0.11 BTU/lb·°F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

12 % IACS
11 % IACS
10.8 % IACS
10.8 % IACS

Electrical Resistivity

1.43×10⁻⁷ Ω·m5.63 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.62 V
-0.65 V
-0.65 V
-0.65 V

Corrosion Resistance

10 / 100
8 / 100
10 / 100
10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

52 / 100
62 / 100
60 / 100
60 / 100

Machinability Rating (AISI 1212 = 100 %)

50%
66%
60%
60%

Formability (cold)

78 / 100
75 / 100
65 / 100
80 / 100

Brazeability / Solderability

75 / 100
75 / 100
70 / 100
80 / 100

Polishability

35 / 100
30 / 100
40 / 100
55 / 100

Castability

45 / 100

Same in both: Weldability 95 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

25 MJ/kg10,748 BTU/lb
30 MJ/kg12,898 BTU/lb
25 MJ/kg10,748 BTU/lb
25 MJ/kg10,748 BTU/lb

Embodied Carbon (primary production)

2.1 kg CO₂/kg
2.3 kg CO₂/kg
2.1 kg CO₂/kg
2.1 kg CO₂/kg

Embodied Water

50 L/kg6 gal/lb
60 L/kg7.2 gal/lb
40 L/kg4.8 gal/lb
40 L/kg4.8 gal/lb

Typical Recycled Content

25%
25%
25%
30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

46 kN·m/kg
41 kN·m/kg
57 kN·m/kg
51 kN·m/kg

Specific Stiffness (E / density)

25.4 MN·m/kg
26.1 MN·m/kg
25.5 MN·m/kg
25.5 MN·m/kg

Modulus of Resilience

156 kJ/m³
118 kJ/m³
203 kJ/m³
156 kJ/m³

Thermal Diffusivity

13.8 mm²/s
13.5 mm²/s
13.8 mm²/s
13.5 mm²/s

Thermal Shock Resistance Index

8
7
10
9

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSPCCCRSHRSMild Steel

Manufacturing and finishing

CapabilityCRSSPCCHRSMild Steel
CNC machiningYesYesYes
Default conditionHRHRHRHR
Relative cost$$ Standard$ Budget$$ Standard$$ Standard
Min. machined wall0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µm
AlCrNYesYesYes
AlTiNYesYesYes
CVD Al2O3YesYesYes
CVD TiCNYesYesYes
CVD TiNYesYesYes
CrNYesYesYes
DLCYesYesYes
HVOF CoatingYesYesYes
MoS2YesYesYes
Multilayer CVDYesYesYes
TiAlNYesYesYes
TiB2YesYesYes
TiCNYesYesYes
TiNYesYesYes
WC/CYesYesYes
ZrNYesYesYes

Both are offered for Sheet metal. They share 22 finishes: Black Oxide, Cerakote, Chrome Plating, Copper Plating, E-Coating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Hot-Dip Galvanizing, Manganese Phosphate, Nickel Plating and 10 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in CRS and SPCC side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.