FabDigit

C12A vs 35# and 2 more: properties

C12A35#WC1WC4

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

218 GPa31.6 Msi
207 GPa30 Msi
205 GPa29.7 Msi
200 GPa29 Msi

Shear Modulus

84 GPa12.2 Msi
80 GPa11.6 Msi
80 GPa11.6 Msi
78 GPa11.3 Msi

Poisson's Ratio

0.3
0.29
0.29
0.29

Tensile Strength (Ultimate)

650 MPa94.3 ksi
560 MPa81.2 ksi
520 MPa75.4 ksi
545 MPa79 ksi

Yield Strength (0.2% offset)

470 MPa68.2 ksi
330 MPa47.9 ksi
305 MPa44.2 ksi
335 MPa48.6 ksi

Elongation at Break

21%
22%
28%
24%

Reduction in Area

58%
50%
48%
50%

Compressive Strength

470 MPa68.2 ksi
300 MPa43.5 ksi
340 MPa49.3 ksi

Shear Strength

400 MPa58 ksi
400 MPa58 ksi
340 MPa49.3 ksi
340 MPa49.3 ksi

Fatigue Strength (Endurance Limit)

295 MPa42.8 ksi
250 MPa36.3 ksi
210 MPa30.5 ksi
235 MPa34.1 ksi

Fracture Toughness (K_IC)

130 MPa·√m118 ksi·√in
55 MPa·√m50.1 ksi·√in
130 MPa·√m118 ksi·√in
120 MPa·√m109 ksi·√in

Charpy V-Notch Impact (RT)

55 J40.6 ft·lbf
60 J44.3 ft·lbf
50 J36.9 ft·lbf
48 J35.4 ft·lbf

Hardness, Brinell

215 HB
160 HB
160 HB
163 HB

Hardness, Rockwell C

19 HRC

Hardness, Vickers

225 HV
168 HV
168 HV

Hardness, Rockwell B

83 HRB
84 HRB
85 HRB

Same in both: Bulk Modulus 160 GPa23.2 Msi

Physical

Density and transition temperatures.

Density

7.77 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³
7.83 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,420°C2,588 °F
1,425°C2,597 °F
1,425°C2,597 °F
1,425°C2,597 °F

Liquidus Temperature

1,490°C2,714 °F
1,500°C2,732 °F
1,505°C2,741 °F
1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

26 W/m·K15 BTU/hr·ft·°F
49 W/m·K28.3 BTU/hr·ft·°F
42 W/m·K24.3 BTU/hr·ft·°F
42 W/m·K24.3 BTU/hr·ft·°F

Specific Heat Capacity

460 J/kg·K0.11 BTU/lb·°F
477 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

10.8 µm/m·K6 µin/in·°F
11.6 µm/m·K6.4 µin/in·°F
12.2 µm/m·K6.8 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F

Latent Heat of Fusion

270 J/g116 BTU/lb
250 J/g107 BTU/lb
270 J/g116 BTU/lb
270 J/g116 BTU/lb

Max Service Temperature (continuous)

600°C1,112 °F
400°C752 °F
455°C851 °F
540°C1,004 °F

Min Service Temperature

-30°C-22 °F
-20°C-4 °F
-29°C-20 °F
-29°C-20 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

2.9 % IACS
10 % IACS
8.5 % IACS
7.8 % IACS

Electrical Resistivity

6×10⁻⁷ Ω·m23.6 µΩ·in
1.7×10⁻⁷ Ω·m6.69 µΩ·in
2×10⁻⁷ Ω·m7.87 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.52 V
-0.65 V
-0.61 V
-0.62 V

Corrosion Resistance

33 / 100
11 / 100
12 / 100
14 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

42 / 100
60 / 100
58 / 100
58 / 100

Machinability Rating (AISI 1212 = 100 %)

45%
65%
60%
60%

Weldability

38 / 100
55 / 100
70 / 100
55 / 100

Formability (cold)

10 / 100
45 / 100
20 / 100
20 / 100

Castability

55 / 100
35 / 100
70 / 100
70 / 100

Brazeability / Solderability

25 / 100
65 / 100
55 / 100
45 / 100

Polishability

60 / 100
55 / 100
50 / 100
45 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

33 MJ/kg14,187 BTU/lb
25 MJ/kg10,748 BTU/lb
26 MJ/kg11,178 BTU/lb
26 MJ/kg11,178 BTU/lb

Embodied Carbon (primary production)

2.4 kg CO₂/kg
1.9 kg CO₂/kg
2.1 kg CO₂/kg
2 kg CO₂/kg

Embodied Water

45 L/kg5.4 gal/lb
40 L/kg4.8 gal/lb
55 L/kg6.6 gal/lb
55 L/kg6.6 gal/lb

Typical Recycled Content

80%
25%
80%
75%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

84 kN·m/kg
71 kN·m/kg
66 kN·m/kg
70 kN·m/kg

Specific Stiffness (E / density)

28.1 MN·m/kg
26.4 MN·m/kg
26.1 MN·m/kg
25.5 MN·m/kg

Modulus of Resilience

507 kJ/m³
263 kJ/m³
227 kJ/m³
281 kJ/m³

Thermal Diffusivity

7.3 mm²/s
13.1 mm²/s
11.4 mm²/s
11.4 mm²/s

Thermal Shock Resistance Index

7
11
9
9

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale35#WC1WC4C12A

Manufacturing and finishing

CapabilityC12A35#WC1WC4
CNC machiningYes
Sheet metalYes
Default conditionHR
Relative cost$$$ Premium$ Budget$$ Standard$$ Standard
Min. machined wall0.8 mm
Best machined surfaceRa 1.6 µm
AlCrNYes
AlTiNYes
Black OxideYes
CVD Al2O3Yes
CVD TiCNYes
CVD TiNYes
CerakoteYes
Chrome PlatingYes
CrNYes
DLCYes
E-CoatingYes
HVOF CoatingYes
Hot-Dip GalvanizingYes
MoS2Yes
Multilayer CVDYes
Nickel PlatingYes
PTFE CoatingYes
PaintingYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in C12A and 35# side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.