Alloy 4950W470Alloy 7930Q130

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

150 GPa21.8 Msi
190 GPa27.6 Msi
205 GPa29.7 Msi
120 GPa17.4 Msi

Shear Modulus

58 GPa8.4 Msi
74 GPa10.7 Msi
78 GPa11.3 Msi
47 GPa6.8 Msi

Bulk Modulus

155 GPa22.5 Msi
160 GPa23.2 Msi
172 GPa24.9 Msi
160 GPa23.2 Msi

Poisson's Ratio

0.3
0.29
0.3
0.3

Tensile Strength (Ultimate)

530 MPa76.9 ksi
440 MPa63.8 ksi
550 MPa79.8 ksi
345 MPa50 ksi

Yield Strength (0.2% offset)

220 MPa31.9 ksi
310 MPa45 ksi
270 MPa39.2 ksi
315 MPa45.7 ksi

Elongation at Break

38%
30%
40%
8%

Reduction in Area

65%
60%

Shear Strength

350 MPa50.8 ksi
265 MPa38.4 ksi
370 MPa53.7 ksi
230 MPa33.4 ksi

Fatigue Strength (Endurance Limit)

240 MPa34.8 ksi
200 MPa29 ksi
220 MPa31.9 ksi
160 MPa23.2 ksi

Charpy V-Notch Impact (RT)

100 J73.8 ft·lbf
160 J118 ft·lbf

Hardness, Brinell

120 HB
152 HB
120 HB
160 HB

Hardness, Rockwell B

70 HRB
82 HRB
65 HRB

Hardness, Vickers

125 HV
160 HV
125 HV
170 HV

Physical

Density and transition temperatures.

Density

8.25 g/cm³0.3 lb/in³
7.7 g/cm³0.28 lb/in³
8.74 g/cm³0.32 lb/in³
7.65 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,425°C2,597 °F
1,480°C2,696 °F
1,425°C2,597 °F
1,470°C2,678 °F

Liquidus Temperature

1,450°C2,642 °F
1,520°C2,768 °F
1,450°C2,642 °F
1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

13.5 W/m·K7.8 BTU/hr·ft·°F
28 W/m·K16.2 BTU/hr·ft·°F
30 W/m·K17.3 BTU/hr·ft·°F
22 W/m·K12.7 BTU/hr·ft·°F

Specific Heat Capacity

500 J/kg·K0.12 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F
480 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

9.5 µm/m·K5.3 µin/in·°F
12 µm/m·K6.7 µin/in·°F
12.7 µm/m·K7.1 µin/in·°F
11.6 µm/m·K6.4 µin/in·°F

Max Service Temperature (continuous)

480°C896 °F
180°C356 °F
400°C752 °F
200°C392 °F

Min Service Temperature

-196°C-321 °F
-60°C-76 °F
-196°C-321 °F
-60°C-76 °F

Latent Heat of Fusion

290 J/g125 BTU/lb
270 J/g116 BTU/lb

Electrical

Conductivity and insulation.

Electrical Conductivity

3.6 % IACS
4.1 % IACS
3 % IACS
3.6 % IACS

Electrical Resistivity

4.8×10⁻⁷ Ω·m18.9 µΩ·in
4.2×10⁻⁷ Ω·m16.5 µΩ·in
5.7×10⁻⁷ Ω·m22.4 µΩ·in
4.8×10⁻⁷ Ω·m18.9 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.35 V
-0.2 V

Corrosion Resistance

32 / 100
20 / 100
50 / 100
18 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

35 / 100
45 / 100
32 / 100
40 / 100

Machinability Rating (AISI 1212 = 100 %)

35%
50%
30%
45%

Weldability

70 / 100
55 / 100
60 / 100
35 / 100

Formability (cold)

85 / 100
70 / 100
85 / 100
35 / 100

Castability

40 / 100

Brazeability / Solderability

70 / 100
70 / 100
40 / 100

Polishability

70 / 100
50 / 100
75 / 100
45 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

120 MJ/kg51,591 BTU/lb
32 MJ/kg13,758 BTU/lb
115 MJ/kg49,441 BTU/lb
34 MJ/kg14,617 BTU/lb

Embodied Carbon (primary production)

8.5 kg CO₂/kg
2.3 kg CO₂/kg
11 kg CO₂/kg
2.6 kg CO₂/kg

Embodied Water

300 L/kg35.9 gal/lb
60 L/kg7.2 gal/lb
400 L/kg47.9 gal/lb
60 L/kg7.2 gal/lb

Typical Recycled Content

30%
25%
25%
15%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

64 kN·m/kg
57 kN·m/kg
63 kN·m/kg
45 kN·m/kg

Specific Stiffness (E / density)

18.2 MN·m/kg
24.7 MN·m/kg
23.5 MN·m/kg
15.7 MN·m/kg

Modulus of Resilience

161 kJ/m³
253 kJ/m³
178 kJ/m³
413 kJ/m³

Thermal Diffusivity

3.3 mm²/s
7.7 mm²/s
7.5 mm²/s
6 mm²/s

Thermal Shock Resistance Index

5
5
6
5

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale50W470Alloy 49Alloy 7930Q130

Manufacturing and finishing

CapabilityAlloy 4950W470Alloy 7930Q130
Sheet metalYes
Default conditionFinal Annealed
Relative cost$$$$ High$$ Standard$$$$ High$$ Standard
Min. machined wall
Best machined surface
Black OxideYes
CerakoteYes
Chrome PlatingYes
E-CoatingYes
Hot-Dip GalvanizingYes
Nickel PlatingYes
PTFE CoatingYes
PaintingYes
Powder CoatingYes
Tin PlatingYes
Zinc PlatingYes
Zinc-Flake (Dip-Spin) CoatingYes
Zinc-Nickel PlatingYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Alloy 49 and 50W470 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.