FabDigit

A656 vs A283 and 2 more: properties

A656A283SPHCA36

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

200 GPa29 Msi
200 GPa29 Msi
205 GPa29.7 Msi
200 GPa29 Msi

Shear Modulus

79 GPa11.5 Msi
79 GPa11.5 Msi
79 GPa11.5 Msi
79.3 GPa11.5 Msi

Tensile Strength (Ultimate)

660 MPa95.7 ksi
420 MPa60.9 ksi
310 MPa45 ksi
450 MPa65.3 ksi

Yield Strength (0.2% offset)

580 MPa84.1 ksi
230 MPa33.4 ksi
240 MPa34.8 ksi
260 MPa37.7 ksi

Elongation at Break

16%
25%
38%
22%

Reduction in Area

50%
45%
60%
50%

Compressive Strength

580 MPa84.1 ksi
230 MPa33.4 ksi
260 MPa37.7 ksi

Shear Strength

420 MPa60.9 ksi
270 MPa39.2 ksi
210 MPa30.5 ksi
275 MPa39.9 ksi

Fatigue Strength (Endurance Limit)

290 MPa42.1 ksi
190 MPa27.6 ksi
155 MPa22.5 ksi
200 MPa29 ksi

Fracture Toughness (K_IC)

100 MPa·√m91 ksi·√in
90 MPa·√m81.9 ksi·√in
120 MPa·√m109 ksi·√in
100 MPa·√m91 ksi·√in

Charpy V-Notch Impact (RT)

80 J59 ft·lbf
27 J19.9 ft·lbf
45 J33.2 ft·lbf
55 J40.6 ft·lbf

Hardness, Brinell

215 HB
120 HB
110 HB
120 HB

Hardness, Rockwell B

96 HRB
68 HRB
64 HRB
67 HRB

Hardness, Rockwell C

18 HRC

Hardness, Vickers

225 HV
126 HV
115 HV
126 HV

Same in both: Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,425°C2,597 °F
1,425°C2,597 °F
1,495°C2,723 °F
1,470°C2,678 °F

Liquidus Temperature

1,510°C2,750 °F
1,510°C2,750 °F
1,530°C2,786 °F
1,520°C2,768 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

46 W/m·K26.6 BTU/hr·ft·°F
51 W/m·K29.5 BTU/hr·ft·°F
52 W/m·K30 BTU/hr·ft·°F
51.9 W/m·K30 BTU/hr·ft·°F

Specific Heat Capacity

480 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F
480 J/kg·K0.11 BTU/lb·°F
486 J/kg·K0.12 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

12 µm/m·K6.7 µin/in·°F
11.7 µm/m·K6.5 µin/in·°F
12 µm/m·K6.7 µin/in·°F
11.7 µm/m·K6.5 µin/in·°F

Latent Heat of Fusion

270 J/g116 BTU/lb
247 J/g106 BTU/lb
247 J/g106 BTU/lb
247 J/g106 BTU/lb

Max Service Temperature (continuous)

350°C662 °F
400°C752 °F
400°C752 °F
400°C752 °F

Min Service Temperature

-40°C-40 °F
-20°C-4 °F
-20°C-4 °F
-20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

9 % IACS
10.8 % IACS
10.5 % IACS
11 % IACS

Electrical Resistivity

1.9×10⁻⁷ Ω·m7.48 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in
1.65×10⁻⁷ Ω·m6.5 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.62 V
-0.65 V
-0.62 V
-0.65 V

Corrosion Resistance

12 / 100
10 / 100
10 / 100
10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

50 / 100
65 / 100
68 / 100
65 / 100

Machinability Rating (AISI 1212 = 100 %)

50%
70%
68%
72%

Weldability

75 / 100
95 / 100
95 / 100
95 / 100

Formability (cold)

65 / 100
78 / 100
80 / 100
80 / 100

Brazeability / Solderability

45 / 100
70 / 100
70 / 100
70 / 100

Polishability

45 / 100
45 / 100
40 / 100
40 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

25 MJ/kg10,748 BTU/lb
25 MJ/kg10,748 BTU/lb
26 MJ/kg11,178 BTU/lb
25 MJ/kg10,748 BTU/lb

Embodied Carbon (primary production)

2 kg CO₂/kg
1.9 kg CO₂/kg
2.1 kg CO₂/kg
2 kg CO₂/kg

Embodied Water

40 L/kg4.8 gal/lb
40 L/kg4.8 gal/lb
45 L/kg5.4 gal/lb
40 L/kg4.8 gal/lb

Typical Recycled Content

30%
30%
25%
40%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

84 kN·m/kg
54 kN·m/kg
39 kN·m/kg
57 kN·m/kg

Specific Stiffness (E / density)

25.5 MN·m/kg
25.5 MN·m/kg
26.1 MN·m/kg
25.5 MN·m/kg

Modulus of Resilience

841 kJ/m³
132 kJ/m³
140 kJ/m³
169 kJ/m³

Thermal Diffusivity

12.2 mm²/s
13.8 mm²/s
13.8 mm²/s
13.6 mm²/s

Thermal Shock Resistance Index

13
9
7
10

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleA283A656SPHCA36

Manufacturing and finishing

CapabilityA656A283SPHCA36
CNC machiningYesYesYes
Default conditionHRHRHRHR
Relative cost$ Budget$ Budget$ Budget$ Budget
Min. machined wall0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µm
AlCrNYesYesYes
AlTiNYesYesYes
CVD Al2O3YesYesYes
CVD TiCNYesYesYes
CVD TiNYesYesYes
CrNYesYesYes
DLCYesYesYes
HVOF CoatingYesYesYes
MoS2YesYesYes
Multilayer CVDYesYesYes
TiAlNYesYesYes
TiB2YesYesYes
TiCNYesYesYes
TiNYesYesYes
WC/CYesYesYes
ZrNYesYesYes

Both are offered for Sheet metal. They share 22 finishes: Black Oxide, Cerakote, Chrome Plating, Copper Plating, E-Coating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Hot-Dip Galvanizing, Manganese Phosphate, Nickel Plating and 10 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in A656 and A283 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.