FabDigit

A372 Grade A vs P265GH and 2 more: properties

A372 Grade AP265GHA285P355GH

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

200 GPa29 Msi
211 GPa30.6 Msi
200 GPa29 Msi
210 GPa30.5 Msi

Shear Modulus

79 GPa11.5 Msi
81 GPa11.7 Msi
79 GPa11.5 Msi
81 GPa11.7 Msi

Poisson's Ratio

0.29
0.3
0.29
0.29

Tensile Strength (Ultimate)

530 MPa76.9 ksi
465 MPa67.4 ksi
450 MPa65.3 ksi
550 MPa79.8 ksi

Yield Strength (0.2% offset)

300 MPa43.5 ksi
295 MPa42.8 ksi
250 MPa36.3 ksi
385 MPa55.8 ksi

Elongation at Break

26%
26%
30%
24%

Reduction in Area

50%
52%
55%
50%

Compressive Strength

300 MPa43.5 ksi
295 MPa42.8 ksi
250 MPa36.3 ksi
385 MPa55.8 ksi

Shear Strength

330 MPa47.9 ksi
280 MPa40.6 ksi
290 MPa42.1 ksi
340 MPa49.3 ksi

Fatigue Strength (Endurance Limit)

230 MPa33.4 ksi
205 MPa29.7 ksi
200 MPa29 ksi
245 MPa35.5 ksi

Fracture Toughness (K_IC)

85 MPa·√m77.4 ksi·√in
100 MPa·√m91 ksi·√in
100 MPa·√m91 ksi·√in
100 MPa·√m91 ksi·√in

Charpy V-Notch Impact (RT)

45 J33.2 ft·lbf
70 J51.6 ft·lbf
40 J29.5 ft·lbf
70 J51.6 ft·lbf

Hardness, Brinell

155 HB
140 HB
130 HB
165 HB

Hardness, Rockwell B

82 HRB
76 HRB
72 HRB
85 HRB

Hardness, Vickers

162 HV
147 HV
173 HV

Same in both: Bulk Modulus 160 GPa23.2 Msi

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,425°C2,597 °F
1,495°C2,723 °F
1,460°C2,660 °F
1,460°C2,660 °F

Liquidus Temperature

1,510°C2,750 °F
1,520°C2,768 °F
1,515°C2,759 °F
1,510°C2,750 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

50 W/m·K28.9 BTU/hr·ft·°F
50 W/m·K28.9 BTU/hr·ft·°F
51 W/m·K29.5 BTU/hr·ft·°F
48 W/m·K27.7 BTU/hr·ft·°F

Specific Heat Capacity

470 J/kg·K0.11 BTU/lb·°F
461 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F
461 J/kg·K0.11 BTU/lb·°F

Latent Heat of Fusion

250 J/g107 BTU/lb
270 J/g116 BTU/lb
250 J/g107 BTU/lb
260 J/g112 BTU/lb

Max Service Temperature (continuous)

425°C797 °F
400°C752 °F
425°C797 °F
380°C716 °F

Min Service Temperature

-29°C-20 °F
-10°C14 °F
-29°C-20 °F
-10°C14 °F

Same in both: Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F

Electrical

Conductivity and insulation.

Electrical Conductivity

10 % IACS
10 % IACS
10.8 % IACS
8.2 % IACS

Electrical Resistivity

1.7×10⁻⁷ Ω·m6.69 µΩ·in
1.7×10⁻⁷ Ω·m6.69 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in
2.1×10⁻⁷ Ω·m8.27 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.61 V
-0.62 V
-0.62 V
-0.62 V

Corrosion Resistance

12 / 100
12 / 100
10 / 100
12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

62 / 100
66 / 100
68 / 100
58 / 100

Machinability Rating (AISI 1212 = 100 %)

62%
63%
65%
62%

Weldability

75 / 100
90 / 100
92 / 100
85 / 100

Formability (cold)

60 / 100
76 / 100
82 / 100
64 / 100

Castability

50 / 100

Brazeability / Solderability

65 / 100
70 / 100
60 / 100
50 / 100

Polishability

55 / 100
50 / 100
40 / 100
45 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

26 MJ/kg11,178 BTU/lb
25 MJ/kg10,748 BTU/lb
25 MJ/kg10,748 BTU/lb
25 MJ/kg10,748 BTU/lb

Embodied Carbon (primary production)

2 kg CO₂/kg
2 kg CO₂/kg
1.9 kg CO₂/kg
1.9 kg CO₂/kg

Embodied Water

45 L/kg5.4 gal/lb
40 L/kg4.8 gal/lb
30 L/kg3.6 gal/lb
40 L/kg4.8 gal/lb

Typical Recycled Content

30%
25%
25%
25%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

68 kN·m/kg
59 kN·m/kg
57 kN·m/kg
70 kN·m/kg

Specific Stiffness (E / density)

25.5 MN·m/kg
26.9 MN·m/kg
25.5 MN·m/kg
26.8 MN·m/kg

Modulus of Resilience

225 kJ/m³
206 kJ/m³
156 kJ/m³
353 kJ/m³

Thermal Diffusivity

13.6 mm²/s
13.8 mm²/s
13.8 mm²/s
13.3 mm²/s

Thermal Shock Resistance Index

11
9
10
10

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleP265GHA285P355GHA372 Grade A

Manufacturing and finishing

CapabilityA372 Grade AP265GHA285P355GH
CNC machiningYesYesYes
Sheet metalYesYesYes
Default conditionHRHRHR
Relative cost$ Budget$$ Standard$$ Standard$$ Standard
Min. machined wall0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µm
AlCrNYesYesYes
AlTiNYesYesYes
Black OxideYesYesYes
CVD Al2O3YesYesYes
CVD TiCNYesYesYes
CVD TiNYesYesYes
CerakoteYesYesYes
Chrome PlatingYesYesYes
CrNYesYesYes
DLCYesYesYes
E-CoatingYesYesYes
HVOF CoatingYesYesYes
Hot-Dip GalvanizingYesYesYes
MoS2YesYesYes
Multilayer CVDYesYesYes
Nickel PlatingYesYesYes
PTFE CoatingYesYesYes
PaintingYesYesYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in A372 Grade A and P265GH side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.