FabDigit

A283 vs A36 and 2 more: properties

A283A36Q235BS235JR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

200 GPa29 Msi
200 GPa29 Msi
206 GPa29.9 Msi
210 GPa30.5 Msi

Shear Modulus

79 GPa11.5 Msi
79.3 GPa11.5 Msi
79 GPa11.5 Msi
81 GPa11.7 Msi

Poisson's Ratio

0.29
0.29
0.3
0.3

Tensile Strength (Ultimate)

420 MPa60.9 ksi
450 MPa65.3 ksi
420 MPa60.9 ksi
420 MPa60.9 ksi

Yield Strength (0.2% offset)

230 MPa33.4 ksi
260 MPa37.7 ksi
250 MPa36.3 ksi
260 MPa37.7 ksi

Elongation at Break

25%
22%
28%
26%

Reduction in Area

45%
50%
55%
55%

Compressive Strength

230 MPa33.4 ksi
260 MPa37.7 ksi
250 MPa36.3 ksi
255 MPa37 ksi

Shear Strength

270 MPa39.2 ksi
275 MPa39.9 ksi
260 MPa37.7 ksi
260 MPa37.7 ksi

Fatigue Strength (Endurance Limit)

190 MPa27.6 ksi
200 MPa29 ksi
190 MPa27.6 ksi
170 MPa24.7 ksi

Fracture Toughness (K_IC)

90 MPa·√m81.9 ksi·√in
100 MPa·√m91 ksi·√in
110 MPa·√m100 ksi·√in
80 MPa·√m72.8 ksi·√in

Charpy V-Notch Impact (RT)

27 J19.9 ft·lbf
55 J40.6 ft·lbf
45 J33.2 ft·lbf
40 J29.5 ft·lbf

Hardness, Rockwell B

68 HRB
67 HRB
67 HRB
67 HRB

Hardness, Vickers

126 HV
126 HV
126 HV
125 HV

Same in both: Bulk Modulus 160 GPa23.2 Msi · Hardness, Brinell 120 HB

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,425°C2,597 °F
1,470°C2,678 °F
1,495°C2,723 °F
1,425°C2,597 °F

Liquidus Temperature

1,510°C2,750 °F
1,520°C2,768 °F
1,520°C2,768 °F
1,520°C2,768 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

51 W/m·K29.5 BTU/hr·ft·°F
51.9 W/m·K30 BTU/hr·ft·°F
50 W/m·K28.9 BTU/hr·ft·°F
50 W/m·K28.9 BTU/hr·ft·°F

Specific Heat Capacity

470 J/kg·K0.11 BTU/lb·°F
486 J/kg·K0.12 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.7 µm/m·K6.5 µin/in·°F
11.7 µm/m·K6.5 µin/in·°F
12 µm/m·K6.7 µin/in·°F
12 µm/m·K6.7 µin/in·°F

Latent Heat of Fusion

247 J/g106 BTU/lb
247 J/g106 BTU/lb
270 J/g116 BTU/lb
270 J/g116 BTU/lb

Max Service Temperature (continuous)

400°C752 °F
400°C752 °F
350°C662 °F
350°C662 °F

Min Service Temperature

-20°C-4 °F
-20°C-4 °F
-20°C-4 °F
0°C32 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

10.8 % IACS
11 % IACS
10.8 % IACS
11 % IACS

Same in both: Electrical Resistivity 1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.65 V
-0.65 V
-0.63 V
-0.61 V

Same in both: Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

65 / 100
65 / 100
65 / 100
66 / 100

Machinability Rating (AISI 1212 = 100 %)

70%
72%
70%
65%

Formability (cold)

78 / 100
80 / 100
85 / 100
85 / 100

Brazeability / Solderability

70 / 100
70 / 100
65 / 100
80 / 100

Polishability

45 / 100
40 / 100
40 / 100
55 / 100

Castability

40 / 100
40 / 100

Same in both: Weldability 95 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Carbon (primary production)

1.9 kg CO₂/kg
2 kg CO₂/kg
2 kg CO₂/kg
2 kg CO₂/kg

Embodied Water

40 L/kg4.8 gal/lb
40 L/kg4.8 gal/lb
30 L/kg3.6 gal/lb
40 L/kg4.8 gal/lb

Typical Recycled Content

30%
40%
25%
30%

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

54 kN·m/kg
57 kN·m/kg
54 kN·m/kg
54 kN·m/kg

Specific Stiffness (E / density)

25.5 MN·m/kg
25.5 MN·m/kg
26.2 MN·m/kg
26.8 MN·m/kg

Modulus of Resilience

132 kJ/m³
169 kJ/m³
152 kJ/m³
161 kJ/m³

Thermal Diffusivity

13.8 mm²/s
13.6 mm²/s
13.6 mm²/s
13.8 mm²/s

Thermal Shock Resistance Index

9
10
8
8

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleA283A36Q235BS235JR

Manufacturing and finishing

CapabilityA283A36Q235BS235JR
Default conditionHRHRHRHR
Relative cost$ Budget$ Budget$ Budget$ Budget
Min. machined wall0.8 mm0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µmRa 1.6 µm

Both are offered for CNC machining and Sheet metal. Both take the same 38 finishes: AlCrN, AlTiN, Black Oxide, CVD Al2O3, CVD TiCN, CVD TiN, Cerakote, Chrome Plating, Copper Plating, CrN, DLC, E-Coating and 26 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in A283 and A36 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.