8620 vs 4130 and 2 more: properties

8620413043409310

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

635 MPa92.1 ksi
700 MPa102 ksi
950 MPa138 ksi
950 MPa138 ksi

Yield Strength (0.2% offset)

385 MPa55.8 ksi
440 MPa63.8 ksi
620 MPa89.9 ksi
600 MPa87 ksi

Elongation at Break

28%
22%
18%
15%

Reduction in Area

60%
50%
45%
45%

Shear Strength

390 MPa56.6 ksi
440 MPa63.8 ksi
580 MPa84.1 ksi
590 MPa85.6 ksi

Fatigue Strength (Endurance Limit)

295 MPa42.8 ksi
330 MPa47.9 ksi
430 MPa62.4 ksi
430 MPa62.4 ksi

Fracture Toughness (K_IC)

85 MPa·√m77.4 ksi·√in
110 MPa·√m100 ksi·√in
95 MPa·√m86.5 ksi·√in
95 MPa·√m86.5 ksi·√in

Charpy V-Notch Impact (RT)

90 J66.4 ft·lbf
55 J40.6 ft·lbf
30 J22.1 ft·lbf
60 J44.3 ft·lbf

Hardness, Brinell

183 HB
210 HB
285 HB
270 HB

Hardness, Rockwell B

90 HRB
95 HRB
100 HRB
98 HRB

Compressive Strength

480 MPa69.6 ksi
640 MPa92.8 ksi
620 MPa89.9 ksi

Hardness, Vickers

228 HV
300 HV
284 HV

Hardness, Rockwell C

29 HRC
27 HRC

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,425°C2,597 °F
1,432°C2,610 °F
1,416°C2,581 °F
1,420°C2,588 °F

Liquidus Temperature

1,505°C2,741 °F
1,510°C2,750 °F
1,454°C2,649 °F
1,490°C2,714 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

46.6 W/m·K26.9 BTU/hr·ft·°F
42.7 W/m·K24.7 BTU/hr·ft·°F
44.5 W/m·K25.7 BTU/hr·ft·°F
34 W/m·K19.6 BTU/hr·ft·°F

Specific Heat Capacity

475 J/kg·K0.11 BTU/lb·°F
477 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.6 µm/m·K6.4 µin/in·°F
12.2 µm/m·K6.8 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F
11.6 µm/m·K6.4 µin/in·°F

Latent Heat of Fusion

270 J/g116 BTU/lb
272 J/g117 BTU/lb
250 J/g107 BTU/lb
270 J/g116 BTU/lb

Min Service Temperature

-40°C-40 °F
-50°C-58 °F
-40°C-40 °F
-90°C-130 °F

Same in both: Max Service Temperature (continuous) 400°C752 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

8 % IACS
7.7 % IACS
7 % IACS
6.6 % IACS

Electrical Resistivity

2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.23×10⁻⁷ Ω·m8.78 µΩ·in
2.48×10⁻⁷ Ω·m9.76 µΩ·in
2.6×10⁻⁷ Ω·m10.2 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.61 V
-0.62 V
-0.6 V

Corrosion Resistance

11 / 100
14 / 100
12 / 100
14 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

62 / 100
55 / 100
48 / 100
40 / 100

Machinability Rating (AISI 1212 = 100 %)

65%
60%
50%
40%

Weldability

60 / 100
65 / 100
33 / 100
38 / 100

Formability (cold)

55 / 100
45 / 100
35 / 100
35 / 100

Brazeability / Solderability

65 / 100
70 / 100
55 / 100
55 / 100

Polishability

70 / 100
60 / 100
70 / 100
65 / 100

Castability

45 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

30 MJ/kg12,898 BTU/lb
30 MJ/kg12,898 BTU/lb
32 MJ/kg13,758 BTU/lb
34 MJ/kg14,617 BTU/lb

Embodied Carbon (primary production)

2.1 kg CO₂/kg
2.3 kg CO₂/kg
2.3 kg CO₂/kg
2.5 kg CO₂/kg

Embodied Water

60 L/kg7.2 gal/lb
45 L/kg5.4 gal/lb
60 L/kg7.2 gal/lb
60 L/kg7.2 gal/lb

Typical Recycled Content

30%
30%
30%
25%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

81 kN·m/kg
89 kN·m/kg
121 kN·m/kg
121 kN·m/kg

Modulus of Resilience

362 kJ/m³
472 kJ/m³
938 kJ/m³
878 kJ/m³

Thermal Diffusivity

12.5 mm²/s
11.4 mm²/s
11.9 mm²/s
9.1 mm²/s

Thermal Shock Resistance Index

12
12
17
14

Same in both: Specific Stiffness (E / density) 26.1 MN·m/kg

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale4130434086209310

Manufacturing and finishing

Capability8620413043409310
Default conditionHRHRHRHR
Relative cost$$ Standard$$ Standard$$$ Premium$$$ Premium
Min. machined wall0.8 mm0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µmRa 1.6 µm

Both are offered for CNC machining and Sheet metal. Both take the same 38 finishes: AlCrN, AlTiN, Black Oxide, CVD Al2O3, CVD TiCN, CVD TiN, Cerakote, Chrome Plating, Copper Plating, CrN, DLC, E-Coating and 26 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 8620 and 4130 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.