FabDigit

5CrNiMo vs H13 and 2 more: properties

5CrNiMoH13H215CrMnMo

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Poisson's Ratio

0.3
0.3
0.29
0.29

Tensile Strength (Ultimate)

760 MPa110 ksi
760 MPa110 ksi
900 MPa131 ksi
780 MPa113 ksi

Yield Strength (0.2% offset)

450 MPa65.3 ksi
520 MPa75.4 ksi
620 MPa89.9 ksi
500 MPa72.5 ksi

Elongation at Break

18%
25%
18%
18%

Reduction in Area

45%
50%
40%
40%

Fracture Toughness (K_IC)

65 MPa·√m59.2 ksi·√in
55 MPa·√m50.1 ksi·√in
80 MPa·√m72.8 ksi·√in

Charpy V-Notch Impact (RT)

35 J25.8 ft·lbf
40 J29.5 ft·lbf
25 J18.4 ft·lbf
45 J33.2 ft·lbf

Hardness, Brinell

220 HB
205 HB
220 HB
220 HB

Hardness, Vickers

230 HV
215 HV
230 HV
230 HV

Compressive Strength

550 MPa79.8 ksi
650 MPa94.3 ksi
520 MPa75.4 ksi

Shear Strength

480 MPa69.6 ksi
550 MPa79.8 ksi
470 MPa68.2 ksi

Fatigue Strength (Endurance Limit)

360 MPa52.2 ksi
400 MPa58 ksi
350 MPa50.8 ksi

Hardness, Rockwell B

95 HRB
97 HRB
97 HRB

Hardness, Rockwell C

19 HRC
18 HRC

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 81 GPa11.7 Msi · Bulk Modulus 160 GPa23.2 Msi

Physical

Density and transition temperatures.

Density

7.83 g/cm³0.28 lb/in³
7.8 g/cm³0.28 lb/in³
8.28 g/cm³0.3 lb/in³
7.8 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,420°C2,588 °F
1,425°C2,597 °F
1,420°C2,588 °F
1,420°C2,588 °F

Liquidus Temperature

1,480°C2,696 °F
1,480°C2,696 °F
1,480°C2,696 °F
1,470°C2,678 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

33 W/m·K19.1 BTU/hr·ft·°F
24.5 W/m·K14.2 BTU/hr·ft·°F
27 W/m·K15.6 BTU/hr·ft·°F
34 W/m·K19.6 BTU/hr·ft·°F

Thermal Expansion (CTE, 20–100 °C)

12.5 µm/m·K6.9 µin/in·°F
10.9 µm/m·K6.1 µin/in·°F
11.8 µm/m·K6.6 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F

Latent Heat of Fusion

270 J/g116 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

300°C572 °F
400°C752 °F
450°C842 °F
400°C752 °F

Min Service Temperature

-30°C-22 °F
-30°C-22 °F
-20°C-4 °F
-20°C-4 °F

Same in both: Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F

Electrical

Conductivity and insulation.

Electrical Resistivity

2.6×10⁻⁷ Ω·m10.2 µΩ·in
5.2×10⁻⁷ Ω·m20.5 µΩ·in
5.5×10⁻⁷ Ω·m21.7 µΩ·in
2.4×10⁻⁷ Ω·m9.45 µΩ·in

Electrical Conductivity

3.3 % IACS
3.1 % IACS
7.2 % IACS

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

12 / 100
22 / 100
15 / 100
12 / 100

Galvanic Potential (seawater, vs SCE)

-0.58 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
45 / 100
40 / 100
55 / 100

Machinability Rating (AISI 1212 = 100 %)

55%
50%
45%
55%

Weldability

30 / 100
35 / 100
35 / 100
35 / 100

Formability (cold)

25 / 100
20 / 100
20 / 100
30 / 100

Polishability

55 / 100
78 / 100
65 / 100
55 / 100

Brazeability / Solderability

30 / 100
40 / 100
35 / 100

Castability

30 / 100
25 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

32 MJ/kg13,758 BTU/lb
34 MJ/kg14,617 BTU/lb
42 MJ/kg18,057 BTU/lb
34 MJ/kg14,617 BTU/lb

Embodied Carbon (primary production)

2.4 kg CO₂/kg
2.6 kg CO₂/kg
3 kg CO₂/kg
2.6 kg CO₂/kg

Embodied Water

60 L/kg7.2 gal/lb
75 L/kg9 gal/lb
60 L/kg7.2 gal/lb
60 L/kg7.2 gal/lb

Typical Recycled Content

30%
45%
45%
45%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

97 kN·m/kg
97 kN·m/kg
109 kN·m/kg
100 kN·m/kg

Specific Stiffness (E / density)

26.8 MN·m/kg
26.9 MN·m/kg
25.4 MN·m/kg
26.9 MN·m/kg

Modulus of Resilience

482 kJ/m³
644 kJ/m³
915 kJ/m³
595 kJ/m³

Thermal Diffusivity

9.2 mm²/s
6.8 mm²/s
7.1 mm²/s
9.5 mm²/s

Thermal Shock Resistance Index

10
8
10
10

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleH13H215CrMnMo5CrNiMo

Manufacturing and finishing

Capability5CrNiMoH13H215CrMnMo
CNC machiningYesYes
3D printingYes
Default conditionAnnealedAnnealed
Relative cost$$ Standard$$$$ High$$ Standard$ Budget
Min. machined wall0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µm
AlCrNYesYes
AlTiNYesYes
Black OxideYesYes
CVD Al2O3YesYes
CVD TiCNYesYes
CVD TiNYesYes
CerakoteYesYes
Chrome PlatingYesYes
CrNYesYes
DLCYesYes
E-CoatingYesYes
HVOF CoatingYesYes
Hot-Dip GalvanizingYesYes
MoS2YesYes
Multilayer CVDYesYes
Nickel PlatingYesYes
PTFE CoatingYesYes
PaintingYesYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 5CrNiMo and H13 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.