4820 vs SCM415 and 2 more: properties

4820SCM41543204620

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

205 GPa29.7 Msi
206 GPa29.9 Msi
205 GPa29.7 Msi
205 GPa29.7 Msi

Tensile Strength (Ultimate)

700 MPa102 ksi
640 MPa92.8 ksi
640 MPa92.8 ksi
570 MPa82.7 ksi

Yield Strength (0.2% offset)

450 MPa65.3 ksi
430 MPa62.4 ksi
415 MPa60.2 ksi
360 MPa52.2 ksi

Elongation at Break

20%
22%
22%
26%

Reduction in Area

50%
55%
50%
55%

Compressive Strength

450 MPa65.3 ksi
430 MPa62.4 ksi

Shear Strength

430 MPa62.4 ksi
400 MPa58 ksi
415 MPa60.2 ksi
380 MPa55.1 ksi

Fatigue Strength (Endurance Limit)

320 MPa46.4 ksi
290 MPa42.1 ksi
300 MPa43.5 ksi
260 MPa37.7 ksi

Fracture Toughness (K_IC)

110 MPa·√m100 ksi·√in
90 MPa·√m81.9 ksi·√in

Charpy V-Notch Impact (RT)

90 J66.4 ft·lbf
55 J40.6 ft·lbf
70 J51.6 ft·lbf
85 J62.7 ft·lbf

Hardness, Brinell

200 HB
180 HB
187 HB
163 HB

Hardness, Rockwell B

93 HRB
89 HRB
90 HRB
84 HRB

Hardness, Vickers

210 HV
190 HV

Same in both: Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Density

7.86 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,425°C2,597 °F
1,430°C2,606 °F
1,425°C2,597 °F
1,420°C2,588 °F

Liquidus Temperature

1,500°C2,732 °F
1,510°C2,750 °F
1,500°C2,732 °F
1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

34 W/m·K19.6 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F
46 W/m·K26.6 BTU/hr·ft·°F

Specific Heat Capacity

470 J/kg·K0.11 BTU/lb·°F
473 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.8 µm/m·K6.6 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F
11.7 µm/m·K6.5 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F

Latent Heat of Fusion

270 J/g116 BTU/lb
250 J/g107 BTU/lb
270 J/g116 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

250°C482 °F
400°C752 °F
350°C662 °F
400°C752 °F

Min Service Temperature

-100°C-148 °F
-50°C-58 °F
-60°C-76 °F
-50°C-58 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

6.9 % IACS
7.8 % IACS
8 % IACS

Electrical Resistivity

2.5×10⁻⁷ Ω·m9.84 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.61 V
-0.61 V
-0.6 V
-0.61 V

Corrosion Resistance

12 / 100
12 / 100
11 / 100
12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

52 / 100
58 / 100
50 / 100
57 / 100

Machinability Rating (AISI 1212 = 100 %)

55%
60%
55%
65%

Weldability

40 / 100
55 / 100
40 / 100
65 / 100

Formability (cold)

55 / 100
60 / 100
45 / 100
58 / 100

Brazeability / Solderability

60 / 100
65 / 100
55 / 100
70 / 100

Polishability

65 / 100
60 / 100
60 / 100
55 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

33 MJ/kg14,187 BTU/lb
27 MJ/kg11,608 BTU/lb
31 MJ/kg13,328 BTU/lb
29 MJ/kg12,468 BTU/lb

Embodied Carbon (primary production)

2.4 kg CO₂/kg
2.1 kg CO₂/kg
2.3 kg CO₂/kg
2.2 kg CO₂/kg

Embodied Water

60 L/kg7.2 gal/lb
50 L/kg6 gal/lb
50 L/kg6 gal/lb
55 L/kg6.6 gal/lb

Typical Recycled Content

35%
30%
30%
30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

89 kN·m/kg
82 kN·m/kg
82 kN·m/kg
73 kN·m/kg

Specific Stiffness (E / density)

26.1 MN·m/kg
26.2 MN·m/kg
26.1 MN·m/kg
26.1 MN·m/kg

Modulus of Resilience

494 kJ/m³
449 kJ/m³
420 kJ/m³
316 kJ/m³

Thermal Diffusivity

9.2 mm²/s
11.9 mm²/s
11.8 mm²/s
12.3 mm²/s

Thermal Shock Resistance Index

10
11
12
11

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSCM415432046204820

Manufacturing and finishing

Capability4820SCM41543204620
Default conditionHRHRHRHR
Relative cost$$ Standard$$ Standard$$$ Premium$$ Standard
Min. machined wall0.8 mm0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µmRa 1.6 µm

Both are offered for CNC machining and Sheet metal. Both take the same 38 finishes: AlCrN, AlTiN, Black Oxide, CVD Al2O3, CVD TiCN, CVD TiN, Cerakote, Chrome Plating, Copper Plating, CrN, DLC, E-Coating and 26 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 4820 and SCM415 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.