Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

210 GPa30.5 Msi
205 GPa29.7 Msi
210 GPa30.5 Msi
207 GPa30 Msi

Shear Modulus

80 GPa11.6 Msi
80 GPa11.6 Msi
81 GPa11.7 Msi
80 GPa11.6 Msi

Tensile Strength (Ultimate)

900 MPa131 ksi
925 MPa134 ksi
1,030 MPa149 ksi
950 MPa138 ksi

Yield Strength (0.2% offset)

600 MPa87 ksi
740 MPa107 ksi
880 MPa128 ksi
780 MPa113 ksi

Elongation at Break

14%
15%
16%
17%

Reduction in Area

30%
45%
55%
55%

Compressive Strength

620 MPa89.9 ksi
760 MPa110 ksi
900 MPa131 ksi
790 MPa115 ksi

Shear Strength

560 MPa81.2 ksi
560 MPa81.2 ksi
620 MPa89.9 ksi
570 MPa82.7 ksi

Fatigue Strength (Endurance Limit)

400 MPa58 ksi
450 MPa65.3 ksi
480 MPa69.6 ksi
430 MPa62.4 ksi

Fracture Toughness (K_IC)

55 MPa·√m50.1 ksi·√in
70 MPa·√m63.7 ksi·√in
70 MPa·√m63.7 ksi·√in
70 MPa·√m63.7 ksi·√in

Charpy V-Notch Impact (RT)

25 J18.4 ft·lbf
40 J29.5 ft·lbf
80 J59 ft·lbf
75 J55.3 ft·lbf

Hardness, Brinell

270 HB
269 HB
310 HB
270 HB

Hardness, Rockwell C

27 HRC
27 HRC
32 HRC
28 HRC

Hardness, Vickers

285 HV
285 HV
325 HV
285 HV

Same in both: Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Density

7.85 g/cm³0.28 lb/in³
7.8 g/cm³0.28 lb/in³
7.8 g/cm³0.28 lb/in³
7.8 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,420°C2,588 °F
1,420°C2,588 °F
1,450°C2,642 °F
1,425°C2,597 °F

Liquidus Temperature

1,490°C2,714 °F
1,480°C2,696 °F
1,500°C2,732 °F
1,490°C2,714 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

44 W/m·K25.4 BTU/hr·ft·°F
40 W/m·K23.1 BTU/hr·ft·°F
36 W/m·K20.8 BTU/hr·ft·°F
36 W/m·K20.8 BTU/hr·ft·°F

Specific Heat Capacity

470 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F
465 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

12.3 µm/m·K6.8 µin/in·°F
12 µm/m·K6.7 µin/in·°F
11.8 µm/m·K6.6 µin/in·°F
12.2 µm/m·K6.8 µin/in·°F

Latent Heat of Fusion

250 J/g107 BTU/lb
260 J/g112 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

350°C662 °F
450°C842 °F
500°C932 °F
450°C842 °F

Min Service Temperature

-20°C-4 °F
-40°C-40 °F
-40°C-40 °F
-40°C-40 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

8 % IACS
7.8 % IACS
7.5 % IACS

Electrical Resistivity

2.1×10⁻⁷ Ω·m8.27 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.3×10⁻⁷ Ω·m9.06 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

11 / 100
12 / 100
16 / 100
15 / 100

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.6 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

58 / 100
50 / 100
40 / 100
42 / 100

Machinability Rating (AISI 1212 = 100 %)

60%
50%
45%
45%

Weldability

30 / 100
20 / 100
18 / 100
18 / 100

Formability (cold)

25 / 100
25 / 100
20 / 100
25 / 100

Polishability

55 / 100
70 / 100
70 / 100
60 / 100

Brazeability / Solderability

40 / 100
40 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

25 MJ/kg10,748 BTU/lb
34 MJ/kg14,617 BTU/lb
34 MJ/kg14,617 BTU/lb
34 MJ/kg14,617 BTU/lb

Embodied Carbon (primary production)

2 kg CO₂/kg
2.3 kg CO₂/kg
2.4 kg CO₂/kg
2.5 kg CO₂/kg

Embodied Water

45 L/kg5.4 gal/lb
60 L/kg7.2 gal/lb
60 L/kg7.2 gal/lb
55 L/kg6.6 gal/lb

Typical Recycled Content

25%
30%
25%
28%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

115 kN·m/kg
119 kN·m/kg
132 kN·m/kg
122 kN·m/kg

Specific Stiffness (E / density)

26.8 MN·m/kg
26.3 MN·m/kg
26.9 MN·m/kg
26.5 MN·m/kg

Modulus of Resilience

857 kJ/m³
1,336 kJ/m³
1,844 kJ/m³
1,470 kJ/m³

Thermal Diffusivity

11.9 mm²/s
11.1 mm²/s
10 mm²/s
9.9 mm²/s

Thermal Shock Resistance Index

15
15
15
14

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleEN41B38CrMoAl38MnVS6SACM645

Manufacturing and finishing

Capability38MnVS6EN41B38CrMoAlSACM645
Default conditionAs ForgedQ&TQ&TQ&T
Relative cost$$ Standard$$ Standard$$ Standard$$ Standard
Min. machined wall0.8 mm0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µmRa 1.6 µm

Both are offered for CNC machining and Sheet metal. Both take the same 38 finishes: AlCrN, AlTiN, Black Oxide, CVD Al2O3, CVD TiCN, CVD TiN, Cerakote, Chrome Plating, Copper Plating, CrN, DLC, E-Coating and 26 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 38MnVS6 and EN41B side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.