FabDigit

34CrAlNi7-10 vs SACM645 and 2 more: properties

34CrAlNi7-10SACM64538CrMoAlA34CrAlMo5-10

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

210 GPa30.5 Msi
207 GPa30 Msi
210 GPa30.5 Msi
210 GPa30.5 Msi

Shear Modulus

80 GPa11.6 Msi
80 GPa11.6 Msi
80 GPa11.6 Msi
81 GPa11.7 Msi

Bulk Modulus

165 GPa23.9 Msi
160 GPa23.2 Msi
160 GPa23.2 Msi
160 GPa23.2 Msi

Tensile Strength (Ultimate)

1,000 MPa145 ksi
950 MPa138 ksi
1,030 MPa149 ksi
900 MPa131 ksi

Yield Strength (0.2% offset)

780 MPa113 ksi
780 MPa113 ksi
880 MPa128 ksi
720 MPa104 ksi

Elongation at Break

13%
17%
16%
14%

Reduction in Area

50%
55%
55%
48%

Compressive Strength

800 MPa116 ksi
790 MPa115 ksi
900 MPa131 ksi
730 MPa106 ksi

Shear Strength

620 MPa89.9 ksi
570 MPa82.7 ksi
640 MPa92.8 ksi
550 MPa79.8 ksi

Fatigue Strength (Endurance Limit)

480 MPa69.6 ksi
430 MPa62.4 ksi
470 MPa68.2 ksi
430 MPa62.4 ksi

Fracture Toughness (K_IC)

70 MPa·√m63.7 ksi·√in
70 MPa·√m63.7 ksi·√in
70 MPa·√m63.7 ksi·√in
75 MPa·√m68.3 ksi·√in

Charpy V-Notch Impact (RT)

45 J33.2 ft·lbf
75 J55.3 ft·lbf
80 J59 ft·lbf
45 J33.2 ft·lbf

Hardness, Brinell

310 HB
270 HB
310 HB
280 HB

Hardness, Rockwell C

33 HRC
28 HRC
32 HRC
29 HRC

Hardness, Vickers

325 HV
285 HV
325 HV
295 HV

Same in both: Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,400°C2,552 °F
1,425°C2,597 °F
1,420°C2,588 °F
1,420°C2,588 °F

Liquidus Temperature

1,480°C2,696 °F
1,490°C2,714 °F
1,490°C2,714 °F
1,490°C2,714 °F

Same in both: Density 7.8 g/cm³0.28 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

33 W/m·K19.1 BTU/hr·ft·°F
36 W/m·K20.8 BTU/hr·ft·°F
33 W/m·K19.1 BTU/hr·ft·°F
34 W/m·K19.6 BTU/hr·ft·°F

Specific Heat Capacity

460 J/kg·K0.11 BTU/lb·°F
465 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.6 µm/m·K6.4 µin/in·°F
12.2 µm/m·K6.8 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F

Latent Heat of Fusion

270 J/g116 BTU/lb
250 J/g107 BTU/lb
270 J/g116 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

500°C932 °F
450°C842 °F
500°C932 °F
500°C932 °F

Same in both: Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

6.6 % IACS
7.5 % IACS
7.8 % IACS
8 % IACS

Electrical Resistivity

2.6×10⁻⁷ Ω·m10.2 µΩ·in
2.3×10⁻⁷ Ω·m9.06 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

16 / 100
15 / 100
12 / 100
12 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

45 / 100
42 / 100
45 / 100
45 / 100

Machinability Rating (AISI 1212 = 100 %)

45%
45%
55%
50%

Weldability

12 / 100
18 / 100
20 / 100
20 / 100

Formability (cold)

20 / 100
25 / 100
20 / 100
25 / 100

Brazeability / Solderability

25 / 100
40 / 100
35 / 100

Polishability

70 / 100
60 / 100
70 / 100
65 / 100

Castability

25 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

31 MJ/kg13,328 BTU/lb
34 MJ/kg14,617 BTU/lb
34 MJ/kg14,617 BTU/lb
31 MJ/kg13,328 BTU/lb

Embodied Carbon (primary production)

2.2 kg CO₂/kg
2.5 kg CO₂/kg
2.3 kg CO₂/kg
2.2 kg CO₂/kg

Embodied Water

60 L/kg7.2 gal/lb
55 L/kg6.6 gal/lb
55 L/kg6.6 gal/lb
55 L/kg6.6 gal/lb

Typical Recycled Content

25%
28%
30%
30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

128 kN·m/kg
122 kN·m/kg
132 kN·m/kg
115 kN·m/kg

Specific Stiffness (E / density)

26.9 MN·m/kg
26.5 MN·m/kg
26.9 MN·m/kg
26.9 MN·m/kg

Modulus of Resilience

1,449 kJ/m³
1,470 kJ/m³
1,844 kJ/m³
1,234 kJ/m³

Thermal Diffusivity

9.2 mm²/s
9.9 mm²/s
9 mm²/s
9.5 mm²/s

Thermal Shock Resistance Index

14
14
14
12

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSACM64538CrMoAlA34CrAlMo5-1034CrAlNi7-10

Manufacturing and finishing

Capability34CrAlNi7-10SACM64538CrMoAlA34CrAlMo5-10
CNC machiningYesYes
Sheet metalYesYes
Default conditionQ&TQ&T
Relative cost$$ Standard$$ Standard$$ Standard$$ Standard
Min. machined wall0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µm
AlCrNYesYes
AlTiNYesYes
Black OxideYesYes
CVD Al2O3YesYes
CVD TiCNYesYes
CVD TiNYesYes
CerakoteYesYes
Chrome PlatingYesYes
CrNYesYes
DLCYesYes
E-CoatingYesYes
HVOF CoatingYesYes
Hot-Dip GalvanizingYesYes
MoS2YesYes
Multilayer CVDYesYes
Nickel PlatingYesYes
PTFE CoatingYesYes
PaintingYesYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 34CrAlNi7-10 and SACM645 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.