FabDigit

300M vs 9310 and 2 more: properties

300M9310Maraging 250E4340

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

200 GPa29 Msi
205 GPa29.7 Msi
181 GPa26.3 Msi
205 GPa29.7 Msi

Shear Modulus

78 GPa11.3 Msi
80 GPa11.6 Msi
70 GPa10.2 Msi
80 GPa11.6 Msi

Bulk Modulus

160 GPa23.2 Msi
160 GPa23.2 Msi
155 GPa22.5 Msi
160 GPa23.2 Msi

Poisson's Ratio

0.29
0.29
0.3
0.29

Tensile Strength (Ultimate)

1,100 MPa160 ksi
950 MPa138 ksi
1,010 MPa146 ksi
950 MPa138 ksi

Yield Strength (0.2% offset)

760 MPa110 ksi
600 MPa87 ksi
810 MPa117 ksi
620 MPa89.9 ksi

Elongation at Break

12%
15%
18%
16%

Reduction in Area

45%
45%
72%
45%

Compressive Strength

800 MPa116 ksi
620 MPa89.9 ksi
830 MPa120 ksi
640 MPa92.8 ksi

Shear Strength

660 MPa95.7 ksi
590 MPa85.6 ksi
620 MPa89.9 ksi
570 MPa82.7 ksi

Fatigue Strength (Endurance Limit)

520 MPa75.4 ksi
430 MPa62.4 ksi
450 MPa65.3 ksi
450 MPa65.3 ksi

Fracture Toughness (K_IC)

95 MPa·√m86.5 ksi·√in
95 MPa·√m86.5 ksi·√in
90 MPa·√m81.9 ksi·√in

Charpy V-Notch Impact (RT)

45 J33.2 ft·lbf
60 J44.3 ft·lbf
130 J95.9 ft·lbf
35 J25.8 ft·lbf

Hardness, Brinell

320 HB
270 HB
300 HB
285 HB

Hardness, Rockwell C

34 HRC
27 HRC
30 HRC
30 HRC

Hardness, Vickers

335 HV
284 HV
310 HV
300 HV

Hardness, Rockwell B

98 HRB

Physical

Density and transition temperatures.

Density

7.83 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³
8 g/cm³0.29 lb/in³
7.85 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,400°C2,552 °F
1,420°C2,588 °F
1,413°C2,575 °F
1,427°C2,601 °F

Liquidus Temperature

1,470°C2,678 °F
1,490°C2,714 °F
1,430°C2,606 °F
1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

40 W/m·K23.1 BTU/hr·ft·°F
34 W/m·K19.6 BTU/hr·ft·°F
25.5 W/m·K14.7 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F

Specific Heat Capacity

475 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F
450 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

12 µm/m·K6.7 µin/in·°F
11.6 µm/m·K6.4 µin/in·°F
10.1 µm/m·K5.6 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F

Latent Heat of Fusion

250 J/g107 BTU/lb
270 J/g116 BTU/lb
270 J/g116 BTU/lb
250 J/g107 BTU/lb

Min Service Temperature

-73°C-99 °F
-90°C-130 °F
-196°C-321 °F
-60°C-76 °F

Same in both: Max Service Temperature (continuous) 400°C752 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

8 % IACS
6.6 % IACS
2.7 % IACS
7 % IACS

Electrical Resistivity

2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.6×10⁻⁷ Ω·m10.2 µΩ·in
6.5×10⁻⁷ Ω·m25.6 µΩ·in
2.48×10⁻⁷ Ω·m9.76 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.6 V
-0.58 V
-0.6 V

Corrosion Resistance

12 / 100
14 / 100
25 / 100
15 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

38 / 100
40 / 100
45 / 100
42 / 100

Machinability Rating (AISI 1212 = 100 %)

35%
40%
45%
45%

Weldability

25 / 100
38 / 100
80 / 100
30 / 100

Formability (cold)

18 / 100
35 / 100
55 / 100
35 / 100

Castability

25 / 100
35 / 100
30 / 100

Brazeability / Solderability

25 / 100
55 / 100
55 / 100
50 / 100

Polishability

75 / 100
65 / 100
85 / 100
70 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

40 MJ/kg17,197 BTU/lb
34 MJ/kg14,617 BTU/lb
90 MJ/kg38,693 BTU/lb
30 MJ/kg12,898 BTU/lb

Embodied Carbon (primary production)

2.8 kg CO₂/kg
2.5 kg CO₂/kg
7 kg CO₂/kg
2.3 kg CO₂/kg

Embodied Water

70 L/kg8.4 gal/lb
60 L/kg7.2 gal/lb
130 L/kg15.6 gal/lb
55 L/kg6.6 gal/lb

Typical Recycled Content

20%
25%
30%
40%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

140 kN·m/kg
121 kN·m/kg
126 kN·m/kg
121 kN·m/kg

Specific Stiffness (E / density)

25.5 MN·m/kg
26.1 MN·m/kg
22.6 MN·m/kg
26.1 MN·m/kg

Modulus of Resilience

1,444 kJ/m³
878 kJ/m³
1,812 kJ/m³
938 kJ/m³

Thermal Diffusivity

10.8 mm²/s
9.1 mm²/s
7.1 mm²/s
11.8 mm²/s

Thermal Shock Resistance Index

18
14
14
17

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale300M9310Maraging 250E4340

Manufacturing and finishing

Capability300M9310Maraging 250E4340
3D printingYes
Default conditionHRHRAnnealedHR
Relative cost$$$$$ Specialty$$$ Premium$$ Standard$$ Standard
Min. machined wall0.8 mm0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µmRa 1.6 µm
Passivated (Metal AM)Yes
Plated (Metal AM)Yes

Both are offered for CNC machining and Sheet metal. They share 38 finishes: AlCrN, AlTiN, Black Oxide, CVD Al2O3, CVD TiCN, CVD TiN, Cerakote, Chrome Plating, Copper Plating, CrN, DLC, E-Coating and 26 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 300M and 9310 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.