FabDigitFabDigit

25KhGT vs SCM415 and 2 more: properties

25KhGTSCM41543204620

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

212 GPa30.7 Msi
206 GPa29.9 Msi
205 GPa29.7 Msi
205 GPa29.7 Msi

Shear Modulus

82 GPa11.9 Msi
80 GPa11.6 Msi
80 GPa11.6 Msi
80 GPa11.6 Msi

Bulk Modulus

165 GPa23.9 Msi
160 GPa23.2 Msi
160 GPa23.2 Msi
160 GPa23.2 Msi

Tensile Strength (Ultimate)

620 MPa89.9 ksi
640 MPa92.8 ksi
640 MPa92.8 ksi
570 MPa82.7 ksi

Yield Strength (0.2% offset)

400 MPa58 ksi
430 MPa62.4 ksi
415 MPa60.2 ksi
360 MPa52.2 ksi

Elongation at Break

18%
22%
22%
26%

Reduction in Area

45%
55%
50%
55%

Compressive Strength

400 MPa58 ksi
430 MPa62.4 ksi
—
—

Shear Strength

380 MPa55.1 ksi
400 MPa58 ksi
415 MPa60.2 ksi
380 MPa55.1 ksi

Fatigue Strength (Endurance Limit)

290 MPa42.1 ksi
290 MPa42.1 ksi
300 MPa43.5 ksi
260 MPa37.7 ksi

Fracture Toughness (K_IC)

80 MPa·√m72.8 ksi·√in
90 MPa·√m81.9 ksi·√in
—
—

Charpy V-Notch Impact (RT)

60 J44.3 ft·lbf
55 J40.6 ft·lbf
70 J51.6 ft·lbf
85 J62.7 ft·lbf

Hardness, Brinell

197 HB
180 HB
187 HB
163 HB

Hardness, Rockwell B

92 HRB
89 HRB
90 HRB
84 HRB

Hardness, Vickers

207 HV
190 HV
—
—

Same in both: Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Density

7.8 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,425°C2,597 °F
1,430°C2,606 °F
1,425°C2,597 °F
1,420°C2,588 °F

Liquidus Temperature

1,500°C2,732 °F
1,510°C2,750 °F
1,500°C2,732 °F
1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

40 W/m·K23.1 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F
46 W/m·K26.6 BTU/hr·ft·°F

Specific Heat Capacity

470 J/kg·K0.11 BTU/lb·°F
473 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.8 µm/m·K6.6 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F
11.7 µm/m·K6.5 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F

Latent Heat of Fusion

250 J/g107 BTU/lb
250 J/g107 BTU/lb
270 J/g116 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

350°C662 °F
400°C752 °F
350°C662 °F
400°C752 °F

Min Service Temperature

-40°C-40 °F
-50°C-58 °F
-60°C-76 °F
-50°C-58 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

7.5 % IACS
7.8 % IACS
—
8 % IACS

Electrical Resistivity

2.3×10⁻⁷ Ω·m9.06 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.61 V
-0.6 V
-0.61 V

Corrosion Resistance

11 / 100
12 / 100
11 / 100
12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

60 / 100
58 / 100
50 / 100
57 / 100

Machinability Rating (AISI 1212 = 100 %)

60%
60%
55%
65%

Weldability

30 / 100
55 / 100
40 / 100
65 / 100

Formability (cold)

48 / 100
60 / 100
45 / 100
58 / 100

Brazeability / Solderability

55 / 100
65 / 100
55 / 100
70 / 100

Polishability

60 / 100
60 / 100
60 / 100
55 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

30 MJ/kg12,898 BTU/lb
27 MJ/kg11,608 BTU/lb
31 MJ/kg13,328 BTU/lb
29 MJ/kg12,468 BTU/lb

Embodied Carbon (primary production)

2.2 kg CO₂/kg
2.1 kg CO₂/kg
2.3 kg CO₂/kg
2.2 kg CO₂/kg

Embodied Water

60 L/kg7.2 gal/lb
50 L/kg6 gal/lb
50 L/kg6 gal/lb
55 L/kg6.6 gal/lb

Same in both: Typical Recycled Content 30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

79 kN·m/kg
82 kN·m/kg
82 kN·m/kg
73 kN·m/kg

Specific Stiffness (E / density)

27.2 MN·m/kg
26.2 MN·m/kg
26.1 MN·m/kg
26.1 MN·m/kg

Modulus of Resilience

377 kJ/m³
449 kJ/m³
420 kJ/m³
316 kJ/m³

Thermal Diffusivity

10.9 mm²/s
11.9 mm²/s
11.8 mm²/s
12.3 mm²/s

Thermal Shock Resistance Index

10
11
12
11

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSCM4154320462025KhGT

Manufacturing and finishing

Capability25KhGTSCM41543204620
CNC machining—YesYesYes
Sheet metal—YesYesYes
Default condition—HRHRHR
Relative cost$ Budget$$ Standard$$$ Premium$$ Standard
Min. machined wall—0.8 mm0.8 mm0.8 mm
Best machined surface—Ra 1.6 µmRa 1.6 µmRa 1.6 µm
AlCrN—YesYesYes
AlTiN—YesYesYes
Black Oxide—YesYesYes
CVD Al2O3—YesYesYes
CVD TiCN—YesYesYes
CVD TiN—YesYesYes
Cerakote—YesYesYes
Chrome Plating—YesYesYes
CrN—YesYesYes
DLC—YesYesYes
E-Coating—YesYesYes
HVOF Coating—YesYesYes
Hot-Dip Galvanizing—YesYesYes
MoS2—YesYesYes
Multilayer CVD—YesYesYes
Nickel Plating—YesYesYes
PTFE Coating—YesYesYes
Painting—YesYesYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 25KhGT and SCM415 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.