15B3510B2110B2215B41

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

730 MPa106 ksi
430 MPa62.4 ksi
620 MPa89.9 ksi
1,160 MPa168 ksi

Yield Strength (0.2% offset)

620 MPa89.9 ksi
290 MPa42.1 ksi
525 MPa76.1 ksi
1,030 MPa149 ksi

Elongation at Break

13%
30%
13%
13%

Reduction in Area

40%
55%
48%
45%

Compressive Strength

620 MPa89.9 ksi
1,080 MPa157 ksi

Shear Strength

440 MPa63.8 ksi
275 MPa39.9 ksi
375 MPa54.4 ksi
700 MPa102 ksi

Fatigue Strength (Endurance Limit)

330 MPa47.9 ksi
200 MPa29 ksi
280 MPa40.6 ksi
520 MPa75.4 ksi

Charpy V-Notch Impact (RT)

25 J18.4 ft·lbf
65 J47.9 ft·lbf
45 J33.2 ft·lbf
40 J29.5 ft·lbf

Hardness, Brinell

217 HB
126 HB
180 HB
336 HB

Hardness, Rockwell B

96 HRB
71 HRB
89 HRB

Fracture Toughness (K_IC)

90 MPa·√m81.9 ksi·√in
75 MPa·√m68.3 ksi·√in
60 MPa·√m54.6 ksi·√in

Hardness, Rockwell C

36 HRC

Hardness, Vickers

350 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,425°C2,597 °F
1,465°C2,669 °F
1,450°C2,642 °F
1,420°C2,588 °F

Liquidus Temperature

1,495°C2,723 °F
1,510°C2,750 °F
1,510°C2,750 °F
1,490°C2,714 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

46 W/m·K26.6 BTU/hr·ft·°F
51.9 W/m·K30 BTU/hr·ft·°F
49 W/m·K28.3 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F

Specific Heat Capacity

475 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.9 µm/m·K6.6 µin/in·°F
11.7 µm/m·K6.5 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F
11.7 µm/m·K6.5 µin/in·°F

Latent Heat of Fusion

247 J/g106 BTU/lb
247 J/g106 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

350°C662 °F
400°C752 °F
350°C662 °F
300°C572 °F

Min Service Temperature

-30°C-22 °F
-30°C-22 °F
-30°C-22 °F
-40°C-40 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

9.5 % IACS
10.8 % IACS
10 % IACS
8.6 % IACS

Electrical Resistivity

1.8×10⁻⁷ Ω·m7.09 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in
1.7×10⁻⁷ Ω·m6.69 µΩ·in
2×10⁻⁷ Ω·m7.87 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.61 V
-0.61 V
-0.6 V
-0.6 V

Same in both: Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
62 / 100
55 / 100
40 / 100

Machinability Rating (AISI 1212 = 100 %)

65%
65%
65%
40%

Weldability

40 / 100
85 / 100
72 / 100
25 / 100

Formability (cold)

55 / 100
82 / 100
85 / 100
20 / 100

Brazeability / Solderability

60 / 100
70 / 100
65 / 100
45 / 100

Polishability

55 / 100
45 / 100
50 / 100
60 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

25 MJ/kg10,748 BTU/lb
25 MJ/kg10,748 BTU/lb
25 MJ/kg10,748 BTU/lb
26 MJ/kg11,178 BTU/lb

Embodied Carbon (primary production)

1.9 kg CO₂/kg
1.9 kg CO₂/kg
1.9 kg CO₂/kg
2 kg CO₂/kg

Embodied Water

40 L/kg4.8 gal/lb
40 L/kg4.8 gal/lb
40 L/kg4.8 gal/lb
45 L/kg5.4 gal/lb

Same in both: Typical Recycled Content 30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

93 kN·m/kg
55 kN·m/kg
79 kN·m/kg
148 kN·m/kg

Modulus of Resilience

938 kJ/m³
205 kJ/m³
672 kJ/m³
2,588 kJ/m³

Thermal Diffusivity

12.3 mm²/s
14.1 mm²/s
13.3 mm²/s
11.9 mm²/s

Thermal Shock Resistance Index

14
9
12
21

Same in both: Specific Stiffness (E / density) 26.1 MN·m/kg

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale10B2110B2215B3515B41

Manufacturing and finishing

Capability15B3510B2110B2215B41
CNC machiningYes
Sheet metalYes
Default conditionHR
Relative cost$ Budget$ Budget$ Budget$ Budget
Min. machined wall0.8 mm
Best machined surfaceRa 1.6 µm
AlCrNYes
AlTiNYes
Black OxideYes
CVD Al2O3Yes
CVD TiCNYes
CVD TiNYes
CerakoteYes
Chrome PlatingYes
CrNYes
DLCYes
E-CoatingYes
HVOF CoatingYes
Hot-Dip GalvanizingYes
MoS2Yes
Multilayer CVDYes
Nickel PlatingYes
PTFE CoatingYes
PaintingYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.