Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

201 GPa29.2 Msi
206 GPa29.9 Msi
210 GPa30.5 Msi
210 GPa30.5 Msi

Shear Modulus

78 GPa11.3 Msi
79.5 GPa11.5 Msi
80 GPa11.6 Msi
80 GPa11.6 Msi

Tensile Strength (Ultimate)

860 MPa125 ksi
800 MPa116 ksi
850 MPa123 ksi
620 MPa89.9 ksi

Yield Strength (0.2% offset)

560 MPa81.2 ksi
480 MPa69.6 ksi
550 MPa79.8 ksi
420 MPa60.9 ksi

Elongation at Break

18%
16%
14%
14%

Reduction in Area

45%
40%
40%
45%

Compressive Strength

600 MPa87 ksi
480 MPa69.6 ksi
560 MPa81.2 ksi

Shear Strength

520 MPa75.4 ksi
500 MPa72.5 ksi
510 MPa74 ksi
400 MPa58 ksi

Fatigue Strength (Endurance Limit)

390 MPa56.6 ksi
360 MPa52.2 ksi
400 MPa58 ksi
280 MPa40.6 ksi

Charpy V-Notch Impact (RT)

60 J44.3 ft·lbf
30 J22.1 ft·lbf
30 J22.1 ft·lbf
40 J29.5 ft·lbf

Hardness, Brinell

220 HB
225 HB
245 HB
185 HB

Hardness, Rockwell B

97 HRB
98 HRB
89 HRB

Hardness, Vickers

232 HV
236 HV
258 HV
195 HV

Fracture Toughness (K_IC)

85 MPa·√m77.4 ksi·√in
75 MPa·√m68.3 ksi·√in
55 MPa·√m50.1 ksi·√in

Hardness, Rockwell C

20 HRC
23 HRC

Same in both: Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Density

7.78 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,400°C2,552 °F
1,420°C2,588 °F
1,420°C2,588 °F
1,420°C2,588 °F

Liquidus Temperature

1,460°C2,660 °F
1,490°C2,714 °F
1,495°C2,723 °F
1,495°C2,723 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

23 W/m·K13.3 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F
42.6 W/m·K24.6 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F

Specific Heat Capacity

460 J/kg·K0.11 BTU/lb·°F
465 J/kg·K0.11 BTU/lb·°F
473 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.3 µm/m·K6.3 µin/in·°F
12.5 µm/m·K6.9 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F
12.5 µm/m·K6.9 µin/in·°F

Latent Heat of Fusion

265 J/g114 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

200°C392 °F
400°C752 °F
400°C752 °F
400°C752 °F

Min Service Temperature

-60°C-76 °F
-40°C-40 °F
-40°C-40 °F
-40°C-40 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

2.9 % IACS
7.8 % IACS
7.8 % IACS
8 % IACS

Electrical Resistivity

6×10⁻⁷ Ω·m23.6 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.6 V
-0.6 V

Corrosion Resistance

16 / 100
10 / 100
12 / 100
11 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

32 / 100
50 / 100
50 / 100
55 / 100

Machinability Rating (AISI 1212 = 100 %)

30%
55%
55%
60%

Weldability

15 / 100
25 / 100
35 / 100
55 / 100

Formability (cold)

20 / 100
45 / 100
35 / 100
60 / 100

Castability

25 / 100

Brazeability / Solderability

30 / 100
40 / 100
50 / 100
45 / 100

Polishability

85 / 100
60 / 100
70 / 100
55 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

48 MJ/kg20,636 BTU/lb
26 MJ/kg11,178 BTU/lb
30 MJ/kg12,898 BTU/lb
25 MJ/kg10,748 BTU/lb

Embodied Carbon (primary production)

3.6 kg CO₂/kg
2 kg CO₂/kg
2.2 kg CO₂/kg
2 kg CO₂/kg

Embodied Water

70 L/kg8.4 gal/lb
45 L/kg5.4 gal/lb
60 L/kg7.2 gal/lb
40 L/kg4.8 gal/lb

Typical Recycled Content

15%
30%
30%
25%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

111 kN·m/kg
102 kN·m/kg
108 kN·m/kg
79 kN·m/kg

Specific Stiffness (E / density)

25.8 MN·m/kg
26.2 MN·m/kg
26.8 MN·m/kg
26.8 MN·m/kg

Modulus of Resilience

780 kJ/m³
559 kJ/m³
720 kJ/m³
420 kJ/m³

Thermal Diffusivity

6.4 mm²/s
12.1 mm²/s
11.5 mm²/s
11.9 mm²/s

Thermal Shock Resistance Index

9
14
14
10

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale55Cr342CrMo434MnB513MoCrNi42-16-14

Manufacturing and finishing

Capability13MoCrNi42-16-1455Cr342CrMo434MnB5
CNC machiningYesYes
Sheet metalYesYesYes
Default conditionAnnealedHRCR
Relative cost$$$$ High$$ Standard$$ Standard$$ Standard
Min. machined wall0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µm
AlCrNYesYes
AlTiNYesYes
Black OxideYesYesYes
CVD Al2O3YesYes
CVD TiCNYesYes
CVD TiNYesYes
CerakoteYesYesYes
Chrome PlatingYesYesYes
CrNYesYes
DLCYesYes
E-CoatingYesYesYes
HVOF CoatingYesYes
Hot-Dip GalvanizingYesYesYes
MoS2YesYes
Multilayer CVDYesYes
Nickel PlatingYesYesYes
PTFE CoatingYesYesYes
PaintingYesYesYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 13MoCrNi42-16-14 and 55Cr3 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.