100Cr6 vs 52100 and 2 more: properties

100Cr652100SUJ2M50

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

210 GPa30.5 Msi
205 GPa29.7 Msi
210 GPa30.5 Msi
207 GPa30 Msi

Bulk Modulus

160 GPa23.2 Msi
166 GPa24.1 Msi
160 GPa23.2 Msi
165 GPa23.9 Msi

Poisson's Ratio

0.29
0.3
0.29
0.29

Tensile Strength (Ultimate)

660 MPa95.7 ksi
690 MPa100 ksi
660 MPa95.7 ksi
860 MPa125 ksi

Yield Strength (0.2% offset)

420 MPa60.9 ksi
415 MPa60.2 ksi
420 MPa60.9 ksi
570 MPa82.7 ksi

Elongation at Break

22%
25%
25%
12%

Reduction in Area

48%
45%
45%
25%

Shear Strength

400 MPa58 ksi
420 MPa60.9 ksi
400 MPa58 ksi
560 MPa81.2 ksi

Fatigue Strength (Endurance Limit)

300 MPa43.5 ksi
320 MPa46.4 ksi
320 MPa46.4 ksi
390 MPa56.6 ksi

Charpy V-Notch Impact (RT)

25 J18.4 ft·lbf
15 J11.1 ft·lbf
30 J22.1 ft·lbf
20 J14.8 ft·lbf

Hardness, Brinell

200 HB
195 HB
192 HB
240 HB

Hardness, Rockwell B

94 HRB
93 HRB
92 HRB
99 HRB

Hardness, Vickers

210 HV
205 HV
200 HV
250 HV

Compressive Strength

430 MPa62.4 ksi
450 MPa65.3 ksi
620 MPa89.9 ksi

Fracture Toughness (K_IC)

60 MPa·√m54.6 ksi·√in

Hardness, Rockwell C

22 HRC

Same in both: Shear Modulus 80 GPa11.6 Msi

Physical

Density and transition temperatures.

Density

7.81 g/cm³0.28 lb/in³
7.81 g/cm³0.28 lb/in³
7.81 g/cm³0.28 lb/in³
8 g/cm³0.29 lb/in³

Melting Point (Solidus)

1,424°C2,595 °F
1,424°C2,595 °F
1,425°C2,597 °F
1,400°C2,552 °F

Liquidus Temperature

1,455°C2,651 °F
1,455°C2,651 °F
1,460°C2,660 °F
1,450°C2,642 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

45 W/m·K26 BTU/hr·ft·°F
46 W/m·K26.6 BTU/hr·ft·°F
46 W/m·K26.6 BTU/hr·ft·°F
26 W/m·K15 BTU/hr·ft·°F

Specific Heat Capacity

470 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.9 µm/m·K6.6 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F
11.3 µm/m·K6.3 µin/in·°F

Latent Heat of Fusion

250 J/g107 BTU/lb
247 J/g106 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

200°C392 °F
400°C752 °F
200°C392 °F
200°C392 °F

Min Service Temperature

-40°C-40 °F
-40°C-40 °F
-40°C-40 °F
-73°C-99 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

8 % IACS
7 % IACS
7 % IACS
2.9 % IACS

Electrical Resistivity

2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.5×10⁻⁷ Ω·m9.84 µΩ·in
2.5×10⁻⁷ Ω·m9.84 µΩ·in
6×10⁻⁷ Ω·m23.6 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.62 V
-0.61 V
-0.6 V

Corrosion Resistance

12 / 100
12 / 100
12 / 100
15 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

45 / 100
40 / 100
45 / 100
35 / 100

Machinability Rating (AISI 1212 = 100 %)

40%
40%
40%
45%

Weldability

12 / 100
12 / 100
12 / 100
10 / 100

Formability (cold)

35 / 100
35 / 100
35 / 100
12 / 100

Castability

30 / 100
25 / 100
30 / 100
20 / 100

Brazeability / Solderability

45 / 100
35 / 100
35 / 100
30 / 100

Polishability

88 / 100
85 / 100
85 / 100
85 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

32 MJ/kg13,758 BTU/lb
30 MJ/kg12,898 BTU/lb
30 MJ/kg12,898 BTU/lb
50 MJ/kg21,496 BTU/lb

Embodied Carbon (primary production)

2.3 kg CO₂/kg
2.2 kg CO₂/kg
2.3 kg CO₂/kg
3.6 kg CO₂/kg

Embodied Water

65 L/kg7.8 gal/lb
55 L/kg6.6 gal/lb
55 L/kg6.6 gal/lb
70 L/kg8.4 gal/lb

Typical Recycled Content

30%
30%
30%
15%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

85 kN·m/kg
88 kN·m/kg
85 kN·m/kg
108 kN·m/kg

Specific Stiffness (E / density)

26.9 MN·m/kg
26.2 MN·m/kg
26.9 MN·m/kg
25.9 MN·m/kg

Modulus of Resilience

420 kJ/m³
420 kJ/m³
420 kJ/m³
785 kJ/m³

Thermal Diffusivity

12.3 mm²/s
12.4 mm²/s
12.8 mm²/s
7.1 mm²/s

Thermal Shock Resistance Index

12
13
12
10

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale52100SUJ2100Cr6M50

Manufacturing and finishing

Capability100Cr652100SUJ2M50
Sheet metalYesYesYes
Default conditionAnnealedAnnealedAnnealedAnnealed
Relative cost$$ Standard$$$ Premium$$ Standard$$$ Premium
Min. machined wall0.8 mm0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µmRa 1.6 µm

Both are offered for CNC machining. Both take the same 38 finishes: AlCrN, AlTiN, Black Oxide, CVD Al2O3, CVD TiCN, CVD TiN, Cerakote, Chrome Plating, Copper Plating, CrN, DLC, E-Coating and 26 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 100Cr6 and 52100 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.