Side-by-side benchmark of 4 polymer grades.

TPS vs PLLA and 2 more: properties

TPSPLLAPDLAPDLLA

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

0.25 GPa0.04 Msi
3.5 GPa0.51 Msi
3.3 GPa0.48 Msi
3 GPa0.44 Msi

Poisson's Ratio

0.42
0.36
0.36
0.36

Tensile Strength (Ultimate)

8 MPa1.2 ksi
62 MPa9 ksi
60 MPa8.7 ksi
50 MPa7.3 ksi

Yield Strength (0.2% offset)

6 MPa0.87 ksi
60 MPa8.7 ksi
58 MPa8.4 ksi
48 MPa7 ksi

Elongation at Break

60%
4%
4%
5%

Compressive Strength

15 MPa2.2 ksi
92 MPa13.3 ksi
80 MPa11.6 ksi
90 MPa13.1 ksi

Flexural Strength

10 MPa1.5 ksi
100 MPa14.5 ksi
90 MPa13.1 ksi
80 MPa11.6 ksi

Flexural Modulus

0.3 GPa0.04 Msi
3.7 GPa0.54 Msi
3.6 GPa0.52 Msi
3.3 GPa0.48 Msi

Izod Impact, Notched

40 J/m0.75 ft·lbf/in
25 J/m0.47 ft·lbf/in
20 J/m0.37 ft·lbf/in
20 J/m0.37 ft·lbf/in

Hardness, Shore A

92 Shore A

Hardness, Shore D

48 Shore D
83 Shore D
83 Shore D
82 Shore D

Tear Strength

30 kN/m171 lbf/in

Shear Modulus

1.3 GPa0.19 Msi
1.2 GPa0.17 Msi

Bulk Modulus

4 GPa0.59 Msi
4 GPa0.57 Msi

Compressive Modulus

3.3 GPa0.48 Msi
3 GPa0.44 Msi
2.8 GPa0.41 Msi

Fracture Toughness (K_IC)

2.2 MPa·√m2 ksi·√in
2.5 MPa·√m2.3 ksi·√in
1.6 MPa·√m1.5 ksi·√in

Hardness, Rockwell R

85 HRR
105 HRR
95 HRR

Shear Strength

48 MPa7 ksi
40 MPa5.8 ksi

Physical

Density and transition temperatures.

Density

1.32 g/cm³0.05 lb/in³
1.26 g/cm³0.05 lb/in³
1.25 g/cm³0.05 lb/in³
1.25 g/cm³0.05 lb/in³

Melting Temperature (Tm)

150°C302 °F
175°C347 °F
178°C352 °F

Glass Transition (Tg)

10°C50 °F
61°C142 °F
58°C136 °F
55°C131 °F

Water Absorption (24 h)

35%
0.4%
0.4%
0.5%

Water Absorption (Saturation)

60%
1%
1%
1.2%

Refractive Index

1.5
1.46
1.455
1.46

Light Transmission

82%
88%
90%
90%

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.25 W/m·K0.14 BTU/hr·ft·°F
0.16 W/m·K0.09 BTU/hr·ft·°F
0.16 W/m·K0.09 BTU/hr·ft·°F
0.15 W/m·K0.09 BTU/hr·ft·°F

Specific Heat Capacity

1,700 J/kg·K0.41 BTU/lb·°F
1,500 J/kg·K0.36 BTU/lb·°F
1,590 J/kg·K0.38 BTU/lb·°F
1,500 J/kg·K0.36 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

150 µm/m·K83.3 µin/in·°F
75 µm/m·K41.7 µin/in·°F
80 µm/m·K44.4 µin/in·°F
85 µm/m·K47.2 µin/in·°F

Max Service Temperature (continuous)

50°C122 °F
55°C131 °F
50°C122 °F
45°C113 °F

Heat Deflection Temp. @ 0.45 MPa

55°C131 °F
65°C149 °F
62°C144 °F
55°C131 °F

Heat Deflection Temp. @ 1.8 MPa

45°C113 °F
55°C131 °F
53°C127 °F
50°C122 °F

Vicat Softening Point (B50)

60°C140 °F
60°C140 °F
59°C138 °F
57°C135 °F

Limiting Oxygen Index

22%
20%
20%
22%

Max Service Temperature (short-term)

90°C194 °F
80°C176 °F
70°C158 °F
60°C140 °F

Same in both: Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1×10⁹ Ω·m3.94×10¹⁶ µΩ·in
1×10¹⁴ Ω·m3.94×10²¹ µΩ·in
1×10¹⁴ Ω·m3.94×10²¹ µΩ·in
1×10¹⁴ Ω·m3.94×10²¹ µΩ·in

Dielectric Strength

15 kV/mm381 V/mil
18 kV/mm457 V/mil
20 kV/mm508 V/mil
17 kV/mm432 V/mil

Dielectric Constant (1 MHz)

6
3
3
3

Volume Resistivity

1×10¹¹ Ω·cm
1×10¹⁶ Ω·cm
1×10¹⁶ Ω·cm
1×10¹⁶ Ω·cm

Surface Resistivity

1×10¹¹ Ω
1×10¹⁶ Ω
1×10¹⁶ Ω

Dissipation Factor (1 MHz)

0.015
0.02
0.013

Comparative Tracking Index (CTI)

600 V

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

20 / 100
55 / 100
45 / 100
30 / 100

UV / Weathering Resistance

35 / 100
45 / 100
35 / 100
40 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

40 / 100
60 / 100
60 / 100
60 / 100

Weldability

65 / 100
75 / 100
60 / 100
55 / 100

Formability (cold)

70 / 100
55 / 100
40 / 100
45 / 100

Polishability

25 / 100
70 / 100
70 / 100
70 / 100

Mold Shrinkage

1.6%
0.4%
0.4%
0.3%

Melt Flow Rate

8 g/10 min
8 g/10 min
15 g/10 min
10 g/10 min

Processing Melt Temperature (typ.)

140°C284 °F
205°C401 °F
210°C410 °F
180°C356 °F

Same in both: Mold Temperature (typ.) 30°C86 °F

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

25 MJ/kg10,748 BTU/lb
50 MJ/kg21,496 BTU/lb
55 MJ/kg23,646 BTU/lb
55 MJ/kg23,646 BTU/lb

Embodied Carbon (primary production)

1.4 kg CO₂/kg
1.3 kg CO₂/kg
2.6 kg CO₂/kg
2.2 kg CO₂/kg

Embodied Water

500 L/kg59.9 gal/lb
400 L/kg47.9 gal/lb

Same in both: Typical Recycled Content 0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

6 kN·m/kg
49 kN·m/kg
48 kN·m/kg
40 kN·m/kg

Specific Stiffness (E / density)

0.2 MN·m/kg
2.8 MN·m/kg
2.6 MN·m/kg
2.4 MN·m/kg

Modulus of Resilience

72 kJ/m³
514 kJ/m³
510 kJ/m³
384 kJ/m³

Same in both: Thermal Diffusivity 0.1 mm²/s · Thermal Shock Resistance Index 0

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scalePLLAPDLAPDLLATPS

Manufacturing and finishing

CapabilityTPSPLLAPDLAPDLLA
Default condition
Relative cost$$ Standard$$$ Premium$$$$ High$$$$ High
Min. machined wall
Best machined surface

Ready to make it?

Upload a CAD file and FabDigit prices the part in TPS and PLLA side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.