FabDigit

TPO vs PP-H vs PP-C vs PP-R

Benchmark · 4 materials

Side-by-side benchmark of 4 polymer grades.

TPO vs PP-H and 2 more: properties

TPOPP-HPP-CPP-R

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

0.6 GPa0.09 Msi
1.5 GPa0.22 Msi
1.1 GPa0.16 Msi
0.85 GPa0.12 Msi

Shear Modulus

0.21 GPa0.03 Msi
0.5 GPa0.07 Msi
0.4 GPa0.06 Msi
0.3 GPa0.04 Msi

Poisson's Ratio

0.42
0.42
0.43
0.43

Tensile Strength (Ultimate)

15 MPa2.2 ksi
35 MPa5.1 ksi
26 MPa3.8 ksi
26 MPa3.8 ksi

Yield Strength (0.2% offset)

12 MPa1.7 ksi
34 MPa4.9 ksi
25 MPa3.6 ksi
25 MPa3.6 ksi

Elongation at Break

400%
300%
350%
600%

Compressive Strength

18 MPa2.6 ksi
45 MPa6.5 ksi
32 MPa4.6 ksi
40 MPa5.8 ksi

Flexural Strength

15 MPa2.2 ksi
45 MPa6.5 ksi
30 MPa4.4 ksi
30 MPa4.4 ksi

Flexural Modulus

0.55 GPa0.08 Msi
1.5 GPa0.22 Msi
1.1 GPa0.16 Msi
0.85 GPa0.12 Msi

Shear Strength

12 MPa1.7 ksi
25 MPa3.6 ksi
20 MPa2.9 ksi
18 MPa2.6 ksi

Izod Impact, Notched

600 J/m11.2 ft·lbf/in
30 J/m0.56 ft·lbf/in
250 J/m4.7 ft·lbf/in
80 J/m1.5 ft·lbf/in

Hardness, Shore A

92 Shore A

Hardness, Shore D

45 Shore D
72 Shore D
67 Shore D
65 Shore D

Hardness, Rockwell R

60 HRR
96 HRR
88 HRR
85 HRR

Tear Strength

60 kN/m343 lbf/in

Compression Set (22 h, 70 °C)

55%

Bulk Modulus

4 GPa0.51 Msi
3 GPa0.48 Msi
3 GPa0.42 Msi

Compressive Modulus

1.5 GPa0.22 Msi
1 GPa0.15 Msi
0.9 GPa0.13 Msi

Fracture Toughness (K_IC)

3 MPa·√m2.7 ksi·√in
3.8 MPa·√m3.5 ksi·√in

Hardness, Rockwell M

68 HRM

Physical

Density and transition temperatures.

Density

0.89 g/cm³0.03 lb/in³
0.91 g/cm³0.03 lb/in³
0.9 g/cm³0.03 lb/in³
0.91 g/cm³0.03 lb/in³

Melting Temperature (Tm)

163°C325 °F
165°C329 °F
164°C327 °F
148°C298 °F

Glass Transition (Tg)

-50°C-58 °F
-10°C14 °F
-18°C-0.4 °F
-12°C10 °F

Water Absorption (24 h)

0.02%
0.01%
0.02%
0.02%

Water Absorption (Saturation)

0.05%
0.03%
0.1%
0.1%

Refractive Index

1.49
1.49
1.49

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.2 W/m·K0.12 BTU/hr·ft·°F
0.22 W/m·K0.13 BTU/hr·ft·°F
0.2 W/m·K0.12 BTU/hr·ft·°F
0.24 W/m·K0.14 BTU/hr·ft·°F

Thermal Expansion (CTE, 20–100 °C)

110 µm/m·K61.1 µin/in·°F
110 µm/m·K61.1 µin/in·°F
110 µm/m·K61.1 µin/in·°F
150 µm/m·K83.3 µin/in·°F

Max Service Temperature (continuous)

90°C194 °F
100°C212 °F
95°C203 °F
70°C158 °F

Min Service Temperature

-40°C-40 °F
-10°C14 °F
-35°C-31 °F
-10°C14 °F

Heat Deflection Temp. @ 0.45 MPa

75°C167 °F
100°C212 °F
88°C190 °F
80°C176 °F

Heat Deflection Temp. @ 1.8 MPa

45°C113 °F
60°C140 °F
55°C131 °F
52°C126 °F

Vicat Softening Point (B50)

65°C149 °F
90°C194 °F
88°C190 °F
80°C176 °F

Limiting Oxygen Index

18%
18%
18%
18%

Max Service Temperature (short-term)

120°C248 °F
130°C266 °F
120°C248 °F
95°C203 °F

Same in both: Specific Heat Capacity 1,900 J/kg·K0.45 BTU/lb·°F

Electrical

Conductivity and insulation.

Electrical Resistivity

1×10¹⁴ Ω·m3.94×10²¹ µΩ·in
1×10¹⁵ Ω·m3.94×10²² µΩ·in
1×10¹⁴ Ω·m3.94×10²¹ µΩ·in
1×10¹⁴ Ω·m3.94×10²¹ µΩ·in

Dielectric Strength

25 kV/mm635 V/mil
28 kV/mm711 V/mil
25 kV/mm635 V/mil
27 kV/mm686 V/mil

Dielectric Constant (1 MHz)

2.3
2.25
2.25
2.3

Dissipation Factor (1 MHz)

6×10⁻⁴
3×10⁻⁴
4×10⁻⁴
4×10⁻⁴

Volume Resistivity

1×10¹⁶ Ω·cm
1×10¹⁷ Ω·cm
1×10¹⁶ Ω·cm
1×10¹⁶ Ω·cm

Same in both: Surface Resistivity 1×10¹⁵ Ω · Comparative Tracking Index (CTI) 600 V

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

UV / Weathering Resistance

45 / 100
20 / 100
25 / 100
20 / 100

Same in both: Corrosion Resistance 90 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

50 / 100
65 / 100
65 / 100
62 / 100

Weldability

80 / 100
90 / 100
88 / 100
95 / 100

Formability (cold)

80 / 100
65 / 100
60 / 100
70 / 100

Polishability

25 / 100
30 / 100
40 / 100
45 / 100

Mold Shrinkage

1.3%
1.6%
1.5%
1.6%

Melt Flow Rate

10 g/10 min
12 g/10 min
12 g/10 min
0.3 g/10 min

Processing Melt Temperature (typ.)

215°C419 °F
230°C446 °F
230°C446 °F
215°C419 °F

Mold Temperature (typ.)

40°C104 °F
35°C95 °F
40°C104 °F
40°C104 °F

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

82 MJ/kg35,254 BTU/lb
78 MJ/kg33,534 BTU/lb
78 MJ/kg33,534 BTU/lb
78 MJ/kg33,534 BTU/lb

Embodied Carbon (primary production)

2.2 kg CO₂/kg
2 kg CO₂/kg
2 kg CO₂/kg
2 kg CO₂/kg

Embodied Water

110 L/kg13.2 gal/lb
100 L/kg12 gal/lb
90 L/kg10.8 gal/lb
60 L/kg7.2 gal/lb

Typical Recycled Content

10%
3%
5%
0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

17 kN·m/kg
39 kN·m/kg
29 kN·m/kg
29 kN·m/kg

Specific Stiffness (E / density)

0.7 MN·m/kg
1.7 MN·m/kg
1.2 MN·m/kg
0.9 MN·m/kg

Modulus of Resilience

120 kJ/m³
385 kJ/m³
284 kJ/m³
368 kJ/m³

Same in both: Thermal Diffusivity 0.1 mm²/s · Thermal Shock Resistance Index 0

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scalePP-HPP-CPP-RTPO

Manufacturing and finishing

CapabilityTPOPP-HPP-CPP-R
Default condition
Relative cost$$ Standard$ Budget$ Budget$ Budget
Min. machined wall
Best machined surface

Ready to make it?

Upload a CAD file and FabDigit prices the part in TPO and PP-H side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.