Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

0.01 GPa0 Msi
0.01 GPa7.25×10⁻⁴ Msi
0.01 GPa0 Msi
0.01 GPa8.7×10⁻⁴ Msi

Shear Modulus

0 GPa4.35×10⁻⁴ Msi

Bulk Modulus

2 GPa0.29 Msi

Poisson's Ratio

0.48
0.3
0.49
0.5

Tensile Strength (Ultimate)

8 MPa1.1 ksi
1 MPa0.15 ksi
16 MPa2.3 ksi
12 MPa1.7 ksi

Elongation at Break

480%
200%
320%
250%

Compressive Strength

3 MPa0.44 ksi
0.1 MPa0.01 ksi

Flexural Modulus

0.02 GPa0 Msi

Shear Strength

5 MPa0.73 ksi
0.35 MPa0.05 ksi

Hardness, Shore A

65 Shore A
30 Shore A
70 Shore A
70 Shore A

Hardness, Shore D

20 Shore D
22 Shore D
22 Shore D

Tear Strength

25 kN/m143 lbf/in
2 kN/m8.6 lbf/in
30 kN/m171 lbf/in
25 kN/m143 lbf/in

Compression Set (22 h, 70 °C)

30%
15%
30%
28%

Compressive Modulus

0 GPa5.8×10⁻⁴ Msi

Physical

Density and transition temperatures.

Density

0.96 g/cm³0.03 lb/in³
0.06 g/cm³0 lb/in³
1.35 g/cm³0.05 lb/in³
1.36 g/cm³0.05 lb/in³

Melting Temperature (Tm)

165°C329 °F
85°C185 °F

Glass Transition (Tg)

-55°C-67 °F
-30°C-22 °F
-25°C-13 °F
-40°C-40 °F

Water Absorption (24 h)

0.3%
0.5%
0.6%
1.5%

Water Absorption (Saturation)

0.8%
2%
5%

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.2 W/m·K0.12 BTU/hr·ft·°F
0.04 W/m·K0.02 BTU/hr·ft·°F
0.2 W/m·K0.12 BTU/hr·ft·°F
0.22 W/m·K0.13 BTU/hr·ft·°F

Specific Heat Capacity

1,900 J/kg·K0.45 BTU/lb·°F
2,100 J/kg·K0.5 BTU/lb·°F
1,600 J/kg·K0.38 BTU/lb·°F
1,600 J/kg·K0.38 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

200 µm/m·K111 µin/in·°F
180 µm/m·K100 µin/in·°F
180 µm/m·K100 µin/in·°F
180 µm/m·K100 µin/in·°F

Max Service Temperature (continuous)

105°C221 °F
70°C158 °F
125°C257 °F
125°C257 °F

Min Service Temperature

-50°C-58 °F
-50°C-58 °F
-30°C-22 °F
-40°C-40 °F

Heat Deflection Temp. @ 0.45 MPa

55°C131 °F

Vicat Softening Point (B50)

60°C140 °F
55°C131 °F

Limiting Oxygen Index

19%
18%
28%
26%

Max Service Temperature (short-term)

135°C275 °F
90°C194 °F
165°C329 °F
150°C302 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1×10¹³ Ω·m3.94×10²⁰ µΩ·in
1×10¹² Ω·m3.94×10¹⁹ µΩ·in
1×10¹¹ Ω·m3.94×10¹⁸ µΩ·in
1×10⁸ Ω·m3.94×10¹⁵ µΩ·in

Dielectric Strength

20 kV/mm508 V/mil
22 kV/mm559 V/mil
16 kV/mm406 V/mil

Dielectric Constant (1 MHz)

2.6
1.4
7
8

Dissipation Factor (1 MHz)

0.0015
0.05

Volume Resistivity

1×10¹⁵ Ω·cm
1×10¹⁴ Ω·cm
1×10¹⁴ Ω·cm
1×10¹⁰ Ω·cm

Surface Resistivity

1×10¹³ Ω

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

88 / 100
90 / 100
85 / 100
78 / 100

UV / Weathering Resistance

70 / 100
35 / 100
95 / 100
88 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

25 / 100
85 / 100
35 / 100
25 / 100

Weldability

65 / 100
70 / 100
65 / 100
10 / 100

Formability (cold)

90 / 100
90 / 100
85 / 100
85 / 100

Polishability

20 / 100
10 / 100

Mold Shrinkage

1.8%
2.5%
2.5%
2.3%

Melt Flow Rate

20 g/10 min
2.5 g/10 min

Processing Melt Temperature (typ.)

210°C410 °F
160°C320 °F
90°C194 °F

Mold Temperature (typ.)

40°C104 °F
165°C329 °F
160°C320 °F
170°C338 °F

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

95 MJ/kg40,843 BTU/lb
75 MJ/kg32,244 BTU/lb
105 MJ/kg45,142 BTU/lb
115 MJ/kg49,441 BTU/lb

Embodied Carbon (primary production)

3.6 kg CO₂/kg
3.4 kg CO₂/kg
4.5 kg CO₂/kg
4.8 kg CO₂/kg

Embodied Water

130 L/kg15.6 gal/lb
130 L/kg15.6 gal/lb

Typical Recycled Content

5%
15%
0%
0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

8 kN·m/kg
17 kN·m/kg
12 kN·m/kg
9 kN·m/kg

Specific Stiffness (E / density)

0 MN·m/kg
0.1 MN·m/kg
0 MN·m/kg
0 MN·m/kg

Thermal Diffusivity

0.1 mm²/s
0.3 mm²/s
0.1 mm²/s
0.1 mm²/s

Thermal Shock Resistance Index

1
0
3
2

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scaleTPEEVA Foam

Manufacturing and finishing

CapabilityTPEEVA FoamCSMECO
Injection moldingYesYes
Default conditionShore A 30 to Shore A 90Closed Cell
Relative cost$$ Standard$$ Standard$$$ Premium$$$$ High
Min. machined wall
Best machined surface
Chrome Plating (Plastic)YesYes
EMI Shielding CoatingYesYes
Soft Touch CoatingYesYes
Spray PaintingYesYes
UV CoatingYesYes

Ready to make it?

Upload a CAD file and FabDigit prices the part in TPE and EVA Foam side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.