FabDigit

SMC vs UP vs Vinyl Ester vs BMC

Benchmark · 4 materials

Side-by-side benchmark of 4 polymer grades.

SMC vs UP and 2 more: properties

SMCUPVinyl EsterBMC

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

11 GPa1.6 Msi
3.4 GPa0.49 Msi
3.3 GPa0.48 Msi
11 GPa1.6 Msi

Shear Modulus

4.2 GPa0.61 Msi
1.3 GPa0.19 Msi
1.2 GPa0.17 Msi
4.2 GPa0.61 Msi

Poisson's Ratio

0.3
0.35
0.36
0.3

Tensile Strength (Ultimate)

75 MPa10.9 ksi
55 MPa8 ksi
84 MPa12.2 ksi
42 MPa6.1 ksi

Elongation at Break

1.5%
2%
5.5%
0.5%

Compressive Strength

180 MPa26.1 ksi
130 MPa18.9 ksi
115 MPa16.7 ksi
160 MPa23.2 ksi

Compressive Modulus

11 GPa1.6 Msi
3.4 GPa0.49 Msi
3.3 GPa0.48 Msi
10 GPa1.5 Msi

Flexural Strength

180 MPa26.1 ksi
95 MPa13.8 ksi
145 MPa21 ksi
85 MPa12.3 ksi

Flexural Modulus

11 GPa1.6 Msi
3.6 GPa0.52 Msi
3.5 GPa0.51 Msi
10.5 GPa1.5 Msi

Shear Strength

50 MPa7.3 ksi
48 MPa7 ksi
55 MPa8 ksi
45 MPa6.5 ksi

Izod Impact, Notched

550 J/m10.3 ft·lbf/in
16 J/m0.3 ft·lbf/in
30 J/m0.56 ft·lbf/in
75 J/m1.4 ft·lbf/in

Hardness, Rockwell M

100 HRM
98 HRM
105 HRM
100 HRM

Bulk Modulus

4 GPa0.57 Msi
4 GPa0.58 Msi

Fracture Toughness (K_IC)

0.5 MPa·√m0.46 ksi·√in
0.85 MPa·√m0.77 ksi·√in

Hardness, Shore D

85 Shore D
88 Shore D

Physical

Density and transition temperatures.

Density

1.85 g/cm³0.07 lb/in³
1.2 g/cm³0.04 lb/in³
1.13 g/cm³0.04 lb/in³
1.85 g/cm³0.07 lb/in³

Glass Transition (Tg)

115°C239 °F
90°C194 °F
120°C248 °F
120°C248 °F

Water Absorption (24 h)

0.2%
0.25%
0.15%
0.15%

Water Absorption (Saturation)

0.7%
1.2%
0.8%
0.6%

Refractive Index

1.55
1.55

Light Transmission

85%

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.25 W/m·K0.14 BTU/hr·ft·°F
0.19 W/m·K0.11 BTU/hr·ft·°F
0.2 W/m·K0.12 BTU/hr·ft·°F
0.6 W/m·K0.35 BTU/hr·ft·°F

Specific Heat Capacity

1,200 J/kg·K0.29 BTU/lb·°F
1,300 J/kg·K0.31 BTU/lb·°F
1,300 J/kg·K0.31 BTU/lb·°F
1,100 J/kg·K0.26 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

25 µm/m·K13.9 µin/in·°F
100 µm/m·K55.6 µin/in·°F
60 µm/m·K33.3 µin/in·°F
25 µm/m·K13.9 µin/in·°F

Max Service Temperature (continuous)

130°C266 °F
85°C185 °F
95°C203 °F
150°C302 °F

Heat Deflection Temp. @ 0.45 MPa

240°C464 °F
90°C194 °F
120°C248 °F
250°C482 °F

Heat Deflection Temp. @ 1.8 MPa

215°C419 °F
72°C162 °F
105°C221 °F
220°C428 °F

Limiting Oxygen Index

25%
19%
21%
24%

Max Service Temperature (short-term)

180°C356 °F
130°C266 °F
120°C248 °F
200°C392 °F

Same in both: Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1×10¹¹ Ω·m3.94×10¹⁸ µΩ·in
1×10¹² Ω·m3.94×10¹⁹ µΩ·in
1×10¹³ Ω·m3.94×10²⁰ µΩ·in
1×10¹² Ω·m3.94×10¹⁹ µΩ·in

Dielectric Strength

15 kV/mm381 V/mil
17 kV/mm432 V/mil
17 kV/mm432 V/mil
14 kV/mm356 V/mil

Dielectric Constant (1 MHz)

4.8
3.2
3.3
4.6

Volume Resistivity

1×10¹³ Ω·cm
1×10¹⁴ Ω·cm
1×10¹⁵ Ω·cm
1×10¹⁴ Ω·cm

Surface Resistivity

1×10¹³ Ω
1×10¹⁴ Ω
1×10¹⁴ Ω
1×10¹³ Ω

Comparative Tracking Index (CTI)

600 V
600 V
550 V
600 V

Same in both: Dissipation Factor (1 MHz) 0.02

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

70 / 100
50 / 100
85 / 100
70 / 100

UV / Weathering Resistance

55 / 100
40 / 100
45 / 100
60 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

30 / 100
55 / 100
55 / 100
35 / 100

Weldability

5 / 100
5 / 100
5 / 100
3 / 100

Formability (cold)

5 / 100
5 / 100
5 / 100
3 / 100

Polishability

45 / 100
65 / 100
60 / 100
40 / 100

Mold Shrinkage

0.1%
2%
2%
0.15%

Mold Temperature (typ.)

150°C302 °F
25°C77 °F
40°C104 °F
160°C320 °F

Processing Melt Temperature (typ.)

35°C95 °F

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

60 MJ/kg25,795 BTU/lb
70 MJ/kg30,095 BTU/lb
80 MJ/kg34,394 BTU/lb
55 MJ/kg23,646 BTU/lb

Embodied Carbon (primary production)

3.2 kg CO₂/kg
3.4 kg CO₂/kg
5 kg CO₂/kg
3 kg CO₂/kg

Embodied Water

180 L/kg21.6 gal/lb
180 L/kg21.6 gal/lb
200 L/kg24 gal/lb
120 L/kg14.4 gal/lb

Same in both: Typical Recycled Content 0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

41 kN·m/kg
46 kN·m/kg
74 kN·m/kg
23 kN·m/kg

Specific Stiffness (E / density)

5.9 MN·m/kg
2.8 MN·m/kg
2.9 MN·m/kg
5.9 MN·m/kg

Thermal Diffusivity

0.1 mm²/s
0.1 mm²/s
0.1 mm²/s
0.3 mm²/s

Same in both: Thermal Shock Resistance Index 0

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scale

Manufacturing and finishing

CapabilitySMCUPVinyl EsterBMC
Default condition
Relative cost$$ Standard$ Budget$$ Standard$$ Standard
Min. machined wall
Best machined surface