FabDigit

ECO vs TPE and 2 more: properties

ECOTPEEVA FoamCSM

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

0.01 GPa8.7×10⁻⁴ Msi
0.01 GPa0 Msi
0.01 GPa7.25×10⁻⁴ Msi
0.01 GPa0 Msi

Poisson's Ratio

0.5
0.48
0.3
0.49

Tensile Strength (Ultimate)

12 MPa1.7 ksi
8 MPa1.1 ksi
1 MPa0.15 ksi
16 MPa2.3 ksi

Elongation at Break

250%
480%
200%
320%

Hardness, Shore A

70 Shore A
65 Shore A
30 Shore A
70 Shore A

Hardness, Shore D

22 Shore D
20 Shore D
22 Shore D

Tear Strength

25 kN/m143 lbf/in
25 kN/m143 lbf/in
2 kN/m8.6 lbf/in
30 kN/m171 lbf/in

Compression Set (22 h, 70 °C)

28%
30%
15%
30%

Shear Modulus

0 GPa4.35×10⁻⁴ Msi

Bulk Modulus

2 GPa0.29 Msi

Compressive Strength

3 MPa0.44 ksi
0.1 MPa0.01 ksi

Flexural Modulus

0.02 GPa0 Msi

Shear Strength

5 MPa0.73 ksi
0.35 MPa0.05 ksi

Compressive Modulus

0 GPa5.8×10⁻⁴ Msi

Physical

Density and transition temperatures.

Density

1.36 g/cm³0.05 lb/in³
0.96 g/cm³0.03 lb/in³
0.06 g/cm³0 lb/in³
1.35 g/cm³0.05 lb/in³

Glass Transition (Tg)

-40°C-40 °F
-55°C-67 °F
-30°C-22 °F
-25°C-13 °F

Water Absorption (24 h)

1.5%
0.3%
0.5%
0.6%

Water Absorption (Saturation)

5%
0.8%
2%

Melting Temperature (Tm)

165°C329 °F
85°C185 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.22 W/m·K0.13 BTU/hr·ft·°F
0.2 W/m·K0.12 BTU/hr·ft·°F
0.04 W/m·K0.02 BTU/hr·ft·°F
0.2 W/m·K0.12 BTU/hr·ft·°F

Specific Heat Capacity

1,600 J/kg·K0.38 BTU/lb·°F
1,900 J/kg·K0.45 BTU/lb·°F
2,100 J/kg·K0.5 BTU/lb·°F
1,600 J/kg·K0.38 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

180 µm/m·K100 µin/in·°F
200 µm/m·K111 µin/in·°F
180 µm/m·K100 µin/in·°F
180 µm/m·K100 µin/in·°F

Max Service Temperature (continuous)

125°C257 °F
105°C221 °F
70°C158 °F
125°C257 °F

Min Service Temperature

-40°C-40 °F
-50°C-58 °F
-50°C-58 °F
-30°C-22 °F

Limiting Oxygen Index

26%
19%
18%
28%

Max Service Temperature (short-term)

150°C302 °F
135°C275 °F
90°C194 °F
165°C329 °F

Heat Deflection Temp. @ 0.45 MPa

55°C131 °F

Vicat Softening Point (B50)

60°C140 °F
55°C131 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1×10⁸ Ω·m3.94×10¹⁵ µΩ·in
1×10¹³ Ω·m3.94×10²⁰ µΩ·in
1×10¹² Ω·m3.94×10¹⁹ µΩ·in
1×10¹¹ Ω·m3.94×10¹⁸ µΩ·in

Dielectric Strength

16 kV/mm406 V/mil
20 kV/mm508 V/mil
22 kV/mm559 V/mil

Dielectric Constant (1 MHz)

8
2.6
1.4
7

Volume Resistivity

1×10¹⁰ Ω·cm
1×10¹⁵ Ω·cm
1×10¹⁴ Ω·cm
1×10¹⁴ Ω·cm

Dissipation Factor (1 MHz)

0.0015
0.05

Surface Resistivity

1×10¹³ Ω

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

78 / 100
88 / 100
90 / 100
85 / 100

UV / Weathering Resistance

88 / 100
70 / 100
35 / 100
95 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

25 / 100
25 / 100
85 / 100
35 / 100

Weldability

10 / 100
65 / 100
70 / 100
65 / 100

Formability (cold)

85 / 100
90 / 100
90 / 100
85 / 100

Mold Shrinkage

2.3%
1.8%
2.5%
2.5%

Mold Temperature (typ.)

170°C338 °F
40°C104 °F
165°C329 °F
160°C320 °F

Polishability

20 / 100
10 / 100

Melt Flow Rate

20 g/10 min
2.5 g/10 min

Processing Melt Temperature (typ.)

210°C410 °F
160°C320 °F
90°C194 °F

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

115 MJ/kg49,441 BTU/lb
95 MJ/kg40,843 BTU/lb
75 MJ/kg32,244 BTU/lb
105 MJ/kg45,142 BTU/lb

Embodied Carbon (primary production)

4.8 kg CO₂/kg
3.6 kg CO₂/kg
3.4 kg CO₂/kg
4.5 kg CO₂/kg

Typical Recycled Content

0%
5%
15%
0%

Embodied Water

130 L/kg15.6 gal/lb
130 L/kg15.6 gal/lb

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

9 kN·m/kg
8 kN·m/kg
17 kN·m/kg
12 kN·m/kg

Specific Stiffness (E / density)

0 MN·m/kg
0 MN·m/kg
0.1 MN·m/kg
0 MN·m/kg

Thermal Diffusivity

0.1 mm²/s
0.1 mm²/s
0.3 mm²/s
0.1 mm²/s

Thermal Shock Resistance Index

2
1
0
3

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scaleTPEEVA Foam

Manufacturing and finishing

CapabilityECOTPEEVA FoamCSM
Injection moldingYesYes
Default conditionShore A 30 to Shore A 90Closed Cell
Relative cost$$$$ High$$ Standard$$ Standard$$$ Premium
Min. machined wall
Best machined surface
Chrome Plating (Plastic)YesYes
EMI Shielding CoatingYesYes
Soft Touch CoatingYesYes
Spray PaintingYesYes
UV CoatingYesYes

Ready to make it?

Upload a CAD file and FabDigit prices the part in ECO and TPE side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.