FabDigit

CIIR vs IIR and 2 more: properties

CIIRIIRBIIREPDM

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

0 GPa5.8×10⁻⁴ Msi
0.01 GPa7.25×10⁻⁴ Msi
0 GPa5.8×10⁻⁴ Msi
0.01 GPa8.7×10⁻⁴ Msi

Shear Modulus

0 GPa1.89×10⁻⁴ Msi
0 GPa1.89×10⁻⁴ Msi
0 GPa2.9×10⁻⁴ Msi

Bulk Modulus

2 GPa0.29 Msi
2 GPa0.29 Msi
2 GPa0.29 Msi

Poisson's Ratio

0.5
0.49
0.5
0.5

Tensile Strength (Ultimate)

12 MPa1.7 ksi
12 MPa1.7 ksi
11 MPa1.6 ksi
12 MPa1.7 ksi

Elongation at Break

500%
600%
500%
400%

Shear Strength

7 MPa1 ksi
7 MPa0.94 ksi

Hardness, Shore A

60 Shore A
60 Shore A
60 Shore A
70 Shore A

Hardness, Shore D

15 Shore D
15 Shore D
22 Shore D

Tear Strength

30 kN/m171 lbf/in
30 kN/m171 lbf/in
30 kN/m171 lbf/in
25 kN/m143 lbf/in

Compression Set (22 h, 70 °C)

30%
35%
32%
20%

Physical

Density and transition temperatures.

Density

1.18 g/cm³0.04 lb/in³
1.12 g/cm³0.04 lb/in³
1.13 g/cm³0.04 lb/in³
1.15 g/cm³0.04 lb/in³

Glass Transition (Tg)

-60°C-76 °F
-68°C-90 °F
-60°C-76 °F
-55°C-67 °F

Water Absorption (24 h)

0.6%
0.5%
0.5%
0.5%

Refractive Index

1.51

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.22 W/m·K0.13 BTU/hr·ft·°F
0.13 W/m·K0.08 BTU/hr·ft·°F
0.22 W/m·K0.13 BTU/hr·ft·°F
0.3 W/m·K0.17 BTU/hr·ft·°F

Specific Heat Capacity

1,900 J/kg·K0.45 BTU/lb·°F
1,900 J/kg·K0.45 BTU/lb·°F
1,900 J/kg·K0.45 BTU/lb·°F
2,000 J/kg·K0.48 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

170 µm/m·K94.4 µin/in·°F
180 µm/m·K100 µin/in·°F
180 µm/m·K100 µin/in·°F
180 µm/m·K100 µin/in·°F

Max Service Temperature (continuous)

140°C284 °F
125°C257 °F
130°C266 °F
120°C248 °F

Min Service Temperature

-45°C-49 °F
-50°C-58 °F
-45°C-49 °F
-50°C-58 °F

Limiting Oxygen Index

22%
20%
20%
19%

Max Service Temperature (short-term)

175°C347 °F
165°C329 °F
170°C338 °F
160°C320 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1×10¹² Ω·m3.94×10¹⁹ µΩ·in
1×10¹¹ Ω·m3.94×10¹⁸ µΩ·in
1×10¹⁰ Ω·m3.94×10¹⁷ µΩ·in
1×10¹² Ω·m3.94×10¹⁹ µΩ·in

Dielectric Strength

24 kV/mm610 V/mil
25 kV/mm635 V/mil
25 kV/mm635 V/mil
25 kV/mm635 V/mil

Dielectric Constant (1 MHz)

2.6
2.3
2.4
3

Dissipation Factor (1 MHz)

0.006
0.003
0.004
0.007

Volume Resistivity

1×10¹⁴ Ω·cm
1×10¹⁵ Ω·cm
1×10¹⁵ Ω·cm
1×10¹⁴ Ω·cm

Comparative Tracking Index (CTI)

600 V

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

80 / 100
75 / 100
85 / 100
85 / 100

UV / Weathering Resistance

88 / 100
80 / 100
85 / 100
95 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Formability (cold)

85 / 100
80 / 100
88 / 100
90 / 100

Mold Shrinkage

2%
2.5%
2.2%
2.5%

Processing Melt Temperature (typ.)

110°C230 °F
90°C194 °F
100°C212 °F

Mold Temperature (typ.)

175°C347 °F
175°C347 °F
170°C338 °F
175°C347 °F

Weldability

5 / 100
25 / 100
15 / 100

Polishability

20 / 100

Same in both: Machinability 30 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

115 MJ/kg49,441 BTU/lb
105 MJ/kg45,142 BTU/lb
105 MJ/kg45,142 BTU/lb
95 MJ/kg40,843 BTU/lb

Embodied Carbon (primary production)

3.6 kg CO₂/kg
4 kg CO₂/kg
3.6 kg CO₂/kg
4 kg CO₂/kg

Embodied Water

180 L/kg21.6 gal/lb
300 L/kg35.9 gal/lb
180 L/kg21.6 gal/lb
150 L/kg18 gal/lb

Same in both: Typical Recycled Content 5%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

10 kN·m/kg
11 kN·m/kg
10 kN·m/kg
10 kN·m/kg

Thermal Shock Resistance Index

4
2
3
3

Same in both: Specific Stiffness (E / density) 0 MN·m/kg · Thermal Diffusivity 0.1 mm²/s

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scaleEPDM

Manufacturing and finishing

CapabilityCIIRIIRBIIREPDM
Injection moldingYes
Default conditionSolid
Relative cost$$ Standard$$ Standard$$ Standard$$ Standard
Min. machined wall
Best machined surface
Chrome Plating (Plastic)Yes
EMI Shielding CoatingYes
Soft Touch CoatingYes
Spray PaintingYes
UV CoatingYes

Ready to make it?

Upload a CAD file and FabDigit prices the part in CIIR and IIR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.