Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

12 GPa1.7 Msi
69 GPa10 Msi
69 GPa10 Msi
69.5 GPa10.1 Msi

Poisson's Ratio

0.3
0.33
0.33
0.33

Tensile Strength (Ultimate)

20 MPa2.9 ksi
90 MPa13.1 ksi
270 MPa39.2 ksi
275 MPa39.9 ksi

Elongation at Break

1%
22%
11%
11%

Compressive Strength

75 MPa10.9 ksi
235 MPa34.1 ksi

Shear Modulus

26 GPa3.8 Msi
26 GPa3.8 Msi
26 GPa3.8 Msi

Bulk Modulus

70 GPa10.2 Msi
69 GPa10 Msi
69 GPa10 Msi

Yield Strength (0.2% offset)

35 MPa5.1 ksi
245 MPa35.5 ksi
235 MPa34.1 ksi

Shear Strength

60 MPa8.7 ksi
172 MPa24.9 ksi
180 MPa26.1 ksi

Fatigue Strength (Endurance Limit)

35 MPa5.1 ksi
90 MPa13.1 ksi
90 MPa13.1 ksi

Hardness, Brinell

23 HB
85 HB
95 HB

Fracture Toughness (K_IC)

30 MPa·√m27.3 ksi·√in
29 MPa·√m26.4 ksi·√in

Hardness, Vickers

90 HV
100 HV

Charpy V-Notch Impact (RT)

18 J13.3 ft·lbf

Physical

Density and transition temperatures.

Density

2.1 g/cm³0.08 lb/in³
2.71 g/cm³0.1 lb/in³
2.7 g/cm³0.1 lb/in³
2.7 g/cm³0.1 lb/in³

Melting Point (Solidus)

645°C1,193 °F
607°C1,125 °F
607°C1,125 °F

Liquidus Temperature

655°C1,211 °F
654°C1,209 °F
654°C1,209 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

1.6 W/m·K0.92 BTU/hr·ft·°F
210 W/m·K121 BTU/hr·ft·°F
188 W/m·K109 BTU/hr·ft·°F
190 W/m·K110 BTU/hr·ft·°F

Specific Heat Capacity

900 J/kg·K0.21 BTU/lb·°F
900 J/kg·K0.21 BTU/lb·°F
897 J/kg·K0.21 BTU/lb·°F
897 J/kg·K0.21 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

26 µm/m·K14.4 µin/in·°F
23.6 µm/m·K13.1 µin/in·°F
23.4 µm/m·K13 µin/in·°F
23 µm/m·K12.8 µin/in·°F

Max Service Temperature (continuous)

130°C266 °F
120°C248 °F
150°C302 °F
150°C302 °F

Min Service Temperature

-50°C-58 °F
-200°C-328 °F
-196°C-321 °F
-196°C-321 °F

Latent Heat of Fusion

395 J/g170 BTU/lb
397 J/g171 BTU/lb
393 J/g169 BTU/lb

Electrical

Conductivity and insulation.

Electrical Conductivity

55 % IACS
49 % IACS
49 % IACS

Electrical Resistivity

3.1×10⁻⁸ Ω·m1.22 µΩ·in
3.52×10⁻⁸ Ω·m1.39 µΩ·in
3.5×10⁻⁸ Ω·m1.38 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

60 / 100
58 / 100
70 / 100
68 / 100

Galvanic Potential (seawater, vs SCE)

-0.8 V
-0.83 V
-0.78 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

85 / 100
30 / 100
55 / 100
62 / 100

Weldability

0 / 100
70 / 100
80 / 100
85 / 100

Formability (cold)

5 / 100
92 / 100
40 / 100
40 / 100

Polishability

15 / 100
50 / 100
65 / 100
70 / 100

Brazeability / Solderability

65 / 100
50 / 100
45 / 100

Machinability Rating (AISI 1212 = 100 %)

50%
190%

Castability

25 / 100

Sustainability

Primary-production footprint per kilogram.

Typical Recycled Content

0%
30%
30%
30%

Embodied Energy (primary production)

200 MJ/kg85,985 BTU/lb
200 MJ/kg85,985 BTU/lb
200 MJ/kg85,985 BTU/lb

Embodied Carbon (primary production)

12 kg CO₂/kg
12.5 kg CO₂/kg
12.5 kg CO₂/kg

Embodied Water

1,200 L/kg144 gal/lb
1,200 L/kg144 gal/lb
1,200 L/kg144 gal/lb

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

10 kN·m/kg
33 kN·m/kg
100 kN·m/kg
102 kN·m/kg

Specific Stiffness (E / density)

5.7 MN·m/kg
25.5 MN·m/kg
25.6 MN·m/kg
25.7 MN·m/kg

Thermal Diffusivity

0.8 mm²/s
86.1 mm²/s
77.6 mm²/s
78.5 mm²/s

Thermal Shock Resistance Index

0
12
31
33

Strength versus weight

Yield strength against density for every aluminum grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

20501002005002.22.42.62.83Density (g/cm³)Yield strength (MPa) — log scale60056005A8281Metapor

Manufacturing and finishing

CapabilityMetapor828160056005A
CNC machiningYesYesYes
Sheet metalYesYesYes
Default condition
Relative cost$$$$ High$$ Standard$$ Standard$ Budget
Min. machined wall0.5 mm0.5 mm0.5 mm
Best machined surfaceRa 0.8 µmRa 0.8 µmRa 0.8 µm
DLCYesYesYes

They share 15 finishes: Anodizing Type II, Cerakote, Chem Film (Alodine), E-Coating, Electroless Nickel (EN), Electropolishing, Epoxy Coating, Gold Plating, Hard Anodize Type III w/ PTFE, Hard Anodizing Type III, Nickel Plating, PTFE Coating and 3 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Metapor and 8281 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.