Stainless Steel ER309Cb and ER316 are both stainless steel grades. Both yield at about 410 MPa — strength does not separate them. On the shop floor, ER316 sits in a lower cost tier (premium, $$$) than ER309Cb (high, $$$$).

ER316Choose it when cost is the deciding factor.

ER309Cb vs ER316: properties

ER309CbER316

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

196 GPa28.4 Msi
193 GPa28 Msi

Shear Modulus

76 GPa11 Msi
77 GPa11.2 Msi

Bulk Modulus

160 GPa23.2 Msi
140 GPa20.3 Msi

Poisson's Ratio

0.29
0.3

Tensile Strength (Ultimate)

600 MPa87 ksi
590 MPa85.6 ksi

Yield Strength (0.2% offset)

410 MPa59.5 ksi
420 MPa60.9 ksi

Elongation at Break

35%
38%

Compressive Strength

415 MPa60.2 ksi
420 MPa60.9 ksi

Shear Strength

390 MPa56.6 ksi
400 MPa58 ksi

Fatigue Strength (Endurance Limit)

240 MPa34.8 ksi
235 MPa34.1 ksi

Fracture Toughness (K_IC)

150 MPa·√m137 ksi·√in
140 MPa·√m127 ksi·√in

Charpy V-Notch Impact (RT)

60 J44.3 ft·lbf
95 J70.1 ft·lbf

Hardness, Brinell

190 HB
185 HB

Hardness, Rockwell B

90 HRB
89 HRB

Hardness, Vickers

200 HV
195 HV

Same in both: Reduction in Area 45%

Physical

Density and transition temperatures.

Density

7.9 g/cm³0.29 lb/in³
7.98 g/cm³0.29 lb/in³

Melting Point (Solidus)

1,400°C2,552 °F
1,385°C2,525 °F

Liquidus Temperature

1,450°C2,642 °F
1,425°C2,597 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

15 W/m·K8.7 BTU/hr·ft·°F
16.3 W/m·K9.4 BTU/hr·ft·°F

Thermal Expansion (CTE, 20–100 °C)

15.5 µm/m·K8.6 µin/in·°F
16 µm/m·K8.9 µin/in·°F

Max Service Temperature (continuous)

800°C1,472 °F
760°C1,400 °F

Same in both: Specific Heat Capacity 500 J/kg·K0.12 BTU/lb·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Min Service Temperature -100°C-148 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

2.2 % IACS
2.3 % IACS

Electrical Resistivity

7.8×10⁻⁷ Ω·m30.7 µΩ·in
7.5×10⁻⁷ Ω·m29.5 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

68 / 100
70 / 100

Galvanic Potential (seawater, vs SCE)

—
-0.08 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

32 / 100
35 / 100

Machinability Rating (AISI 1212 = 100 %)

35%
32%

Weldability

88 / 100
90 / 100

Brazeability / Solderability

55 / 100
60 / 100

Polishability

60 / 100
70 / 100

Same in both: Formability (cold) 55 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

55 MJ/kg23,646 BTU/lb
75 MJ/kg32,244 BTU/lb

Embodied Carbon (primary production)

4.8 kg CO₂/kg
5.2 kg CO₂/kg

Embodied Water

150 L/kg18 gal/lb
130 L/kg15.6 gal/lb

Same in both: Typical Recycled Content 55%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

76 kN·m/kg
74 kN·m/kg

Specific Stiffness (E / density)

24.8 MN·m/kg
24.2 MN·m/kg

Modulus of Resilience

429 kJ/m³
457 kJ/m³

Thermal Diffusivity

3.8 mm²/s
4.1 mm²/s

Same in both: Thermal Shock Resistance Index 3

Strength versus weight

Yield strength against density for every stainless steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

3005007001,0001,5002,0007.27.47.67.888.2Density (g/cm³)Yield strength (MPa) — log scaleER309CbER316

Manufacturing and finishing

CapabilityER309CbER316
Default condition——
Relative cost$$$$ High$$$ Premium
Min. machined wall——
Best machined surface——

Both take the same 7 finishes: Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Pickling, Plasma Spray, Silver Plating.

ER309Cb vs ER316 — frequently asked

What is the difference between ER309Cb and ER316?

Stainless Steel ER309Cb and ER316 are both stainless steel grades. Both yield at about 410 MPa — strength does not separate them. On the shop floor, ER316 sits in a lower cost tier (premium, $$$) than ER309Cb (high, $$$$).

Which is cheaper, ER309Cb or ER316?

ER316 is the lower-cost material: it sits in the premium tier ($$$) while ER309Cb is high ($$$$). Part price depends far more on geometry, tolerance and quantity than on raw stock — upload a CAD file for a live quote.

When should I choose ER309Cb over ER316?

Pick ER316 when cost is the deciding factor.

Ready to make it?

Upload a CAD file and FabDigit prices the part in ER309Cb and ER316 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.